UDC
678.83:620.165.79
DOI
10.18577/2307-6046-2016-0-2-11-11
Article PDF (Russian)
(726.94 KB)
How to cite
Shuldeshova P.M., Deev I.S., Zhelezina G.F. Features of destruction of SVM aramide fibers and structural organoplastics on their basis // Proceedings of VIAM. 2016. No. 2 (38). Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-2-11-11.
Features of destruction of SVM aramide fibers and structural organoplastics on their basis
Abstract
Nature of destruction of SVM aramide fiber and structural organoplastics on its basis is researched. Features of destruction of fiber are to be considered when developing this class of polymercomposites. Nature of fibers destruction is considered at stretching and compression, as well as behavior of SVM fiber at stretching of the organoplastics on its basis.
Keywords
organoplastics, aramide fibers, splitting fibers, fibrils, microplastics, impact resistance.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
- Zhelezina G.F. Konstrukcionnye i funkcionalnye organoplastiki novogo pokoleniya [Constructional and functional organoplastics of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 06. Available at: http://www.viam-works.ru (accessed: September 05, 2014).
- Kablov E.N., Kirillov V.N., Zhirnov A.D., Startsev O.V., Vapirov Yu.M. Centry dlya klimaticheskih ispytanij aviacionnyh PKM [The centers for climatic tests of aviation PCM] // Aviacionnaya promyshlennost. 2009. №4. S. 36–46.
- Zhelezina G.F., Shul'deshova P.M. Konstrukcionnye organoplastiki na osnove plenochnyh kleev [Constructional organoplasty on the basis of film glues] // Klei. Germetiki. Tehnologii. 2014. №2. S. 9–14.
- Nefedov N.I., Kondrashov E.K., Semenova L.V., Lebedeva T.A. Erozionnostojkie pokrytiya dlya zashhity izdelij iz polimernyh kompozicionnyh materialov [Erosion-resistant coatings for protection of articles from polymer composite materials] // Aviacionnye materialy i tehnologii. 2014. №S3. S. 25–27.
- Kraev I.D., Obraztsova E.P., Yurkov G.Yu. Vliyanie morfologii magnitnogo napolnitelya na radiopogloshhayushhie harakteristiki kompozicionnyh materialov [Influence of morphology of magnetic filler on radar-absorbing characteristics of composite materials] // Aviacionnye materialy i tehnologii. 2014. №S2. S. 10–14.
- Sidorenko Yu.N. Konstrukcionnye i funkcionalnye voloknistye kompozicionnye materialy [Constructional and functional fibrous composite materials]. Tomsk: TGU, 2006. 107 s.
- Shuldeshova P.M., Zhelezina G.F. Vliyanie atmosfernyh uslovij i zapylennosti sredy na svojstva konstrukcionnyh organoplastikov [An influence of atmospheric condition and dust loading on properties of structural organic plastics] // Aviacionnye materialy i tehnologii. 2014. №1. S. 64–68.
- Shuldeshova P.M., Zhelezina G.F. Aramidnyj sloisto-tkanyj material dlya zashhity ot ballisticheskih i udarnyh vozdejstvij [The aramid layered and woven material for protection against impact and ballistic influences] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №9. St. 06. Available at: http://www.viam-works.ru (accessed: September 05, 2014). DOI: 10.18577/2307-6046-2014-0-9-6-6.
- Shuldeshov E.M., Lepeshkin V.V., Romanov A.M. Metod nerazrushajushhego kontrolja kompleksnoj dielektricheskoj pronicaemosti vhodnyh slabo napolnennyh sloev gradientnyh radiopogloshhajushhih polimernyh kompozicionnyh materialov [Method of non-destructive testing of complex dielectric permittivity of the entrance poorly filled layers of gradient radio absorbing polymeric composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №10. St. 11. Available at: http://www.viam-works.ru (accessed: September 05, 2014). DOI: 10.18577/2307-6046-2014-0-10-11-11.
- Semenova L.V., Novikova T.A., Nefedov N.I. Klimaticheskaya stojkost i starenie lakokrasochnogo pokrytiya [Climatic resistance and aging of the paintwork coating] // Aviacionnye materialy i tehnologii. 2014. №S3. S. 31–34.
- Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
- Voinov S.I., Zhelezina G.F., Soloveva N.A., Yamshhikova G.A., Timoshina L.N. Vliyanie vneshnej sredy na svojstva ugleplastika, poluchennogo metodom propitki pod davleniem (RTM) [Environmental effects on properties of CFRP manufactured by RTM method] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №2. St. 08. Available at: http://www.viam-works.ru (accessed: September 05, 2014). DOI: 10.18577/2307-6046-2015-0-2-8-8.
- Belyaev A.A., Romanov A.M., Shirokov V.V., Shuldeshov E.M. Izmerenie dielektricheskoj pronicaemosti steklosotoplasta v svobodnom prostranstve [Measurement of honeycomb glass fiber plasticspermittivity in free space] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №5. St. 06. Available at: http://www.viam-works.ru (accessed: September 05, 2014). DOI: 10.18577/2307-6046-2014-0-5-6-6.
- Shuldeshov E.M., Lepeshkin V.V., Romanov A.M. Metod nerazrushayushhego kontrolya koefficienta otrazheniya radiopogloshhayushhih polimernyh kompozicionnyh materialov [Method of non-destructive testing of reflection coefficient of radio absorbing polymeric composite materials] // Kontrol. Diagnostika. 2015. №6. S. 44–48.
- Donetskij K.I., Kogan D.I., Khrulkov A.V. Ispolzovanie principov «zelenoj himii» v perspektivnyh tehnologiyah izgotovlenija izdelij iz PKM [Use of principles of «green chemistry» in perspective manufacturing techniques of products from PCM] // Kompozitnyj mir. 2013. №5. S. 34–38.
- Doneckij K.I., Khrulkov A.V. Principy «zelenoj himii» v perspektivnyh tehnologiyah izgotovleniya izdelij iz PKM [Principles of «green chemistry» in perspective manufacturing technologies of PCM
- articles] // Aviacionnye materialy i tehnologii. 2014. №S2. S. 24–28.
- Doneckij K.I., Khrulkov A.V. Primenenie naturalnyh volokon pri izgotovlenii polimernyh kompozicionnyh materialov [Application of natural fibers for manufacturing of polymer composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №2. St. 10. Available at: http://www.viam-works.ru (accessed: September 05, 2014). DOI: 10.18577/2307-6046-2015-0-2-10-10.
- Deev I.S., Kablov E.N., Kobets L.P., Chursova L.V. Issledovanie metodom skaniruyushhej elektronnoj mikroskopii deformacii mikrofazovoj struktury polimernyh matric pri mehanicheskom nagruzhenii [Research of the scanning electron microscopy method deformation of microphase structure of polymeric matrix at mechanical loading] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №7. St. 06. Available at: http://www.viam-works.ru (accessed: September 05, 2014). DOI: 10.18577/2307-6046-2014-0-7-6-6.
- Deev I.S., Kobec L.P. Issledovanie mikrostruktury i mikropolej deformacij v polimernyh kompozitah metodom rastrovoj elektronnoj mikroskopii [Research of microstructure and microfields of deformations in polymeric composites method of raster electron microscopy] // Zavodskaja laboratorija. Diagnostika materialov. 1999. T. 65. №4. S. 27–34.
- Deev I.S., Kobec L.P. Issledovanie mikrostruktury i osobennostej razrushenija jepoksidnyh polimerov i kompozicionnyh materialov na ih osnove [Research of microstructure and features of destruction of epoxy polymers and composite materials on their basis] // Materialovedenie. 2010. №5. S. 8–16 (nachalo). 2010. №6. S. 13–18.