Damage of single-crystal turbine blades of GTP
Naprienko S.A., Orlov M.R. Damage of single-crystal turbine blades of GTP // Proceedings of VIAM. 2016. No. 2. DOI: 10.18577/2307-6046-2016-0-2-3-3. URL: https://viam-works.ru/en/journal/2016/2/3
Keywords
single-crystal blades, superalloys GS26-VI, GS32-VI, GTP, hydrogen embrittlement.
Abstract
Fractures of single-crystal turbine blades of GTP of alloys GS26-VI and GS32-VI after operating damage were analyzed to identify fracture mechanism. Single-crystal samples of alloy GS32-VI were tested under short-term loading and creep at temperature of 570°С, which corresponded to working conditions of blade tails, to confirm the fracture mechanism.
Reference list
- Kablov E.N., Tolorajya V.N. VIAM – osnovopolozhnik otechestvennoj tehnologii litya monokristallicheskih turbinnyh lopatok GTD i GTU [VIAM – the founder of domestic casting technology of single-crystal turbine blades of GTE and GTU] // Aviacionnye materialy i tehnologii. 2012. №S. S. 105–117.
- Kablov E.N., Bondarenko Yu.A., Echin A.B., Surova V.A. Kablov D.E. Razvitie processa napravlennoj kristllizacii lopatok GTD iz zharoprochnyh i intermetallidnyh splavov s monokristallicheskoj strukturoj [Development of process of the directed kristllizatsiya of blades of GTE from heat resisting and intermetallic alloys with single-crystal structure] // Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 20–25.
- Litye lopatki gazoturbinnyh dvigatelej: splavy, tehnologii, pokrytija. 2-e izd. / pod obshh. red. E.N. Kablova [Cast blades of gas turbine engines: alloys, technologies, coverings. 2nd ed. / under the general editorship of E.N.Kablov]. M.: Nauka, 2006. 632 s.
- Kablov E.N., Bondarenko Yu.A., Kablov D.E. Osobennosti struktury i zharoprochnyh svojstv monokristallov 001> vysokorenievogo nikelevogo zharoprochnogo splava, poluchennogo v usloviyah vysokogradientnoj napravlennoj kristallizacii [Features of structure and heat resisting properties of monocrystals of 001> high-rhenium nickel hot strength alloys received in the conditions of high-gradient directed crystallization] // Aviacionnye materialy i tehnologii. 2011. №4. S. 25–31.
- Chabina E.B., Alekseev A.A., Filonova E.V., Lukina E.A. Primenenie metodov analiticheskoj mikroskopii i rentgenostrukturnogo analiza dlya issledovaniya strukturno-fazovogo sostoyaniya materialov [Application of methods of analytical microscopy and X-ray of the structural analysis for research of structural and phase condition of materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. № 5. St. 06. Available at: http://www.viam-works.ru (accessed: February 10, 2015).
- Nazarkin R.M. Rentgenodifrakcionnye metodiki precizionnogo opredeleniya parametrov kristallicheskih reshetok nikelevyh zharoprochnyh splavov (kratkij obzor) [X-ray diffraction techniques for precise determination of lattice constants in Ni-based superalloys: a brief review] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 41–48.
- Echin A.B., Bondarenko Yu.A. Novaya promyshlennaya vysokogradientnaya ustanovka UVNS-6 dlya polucheniya lopatok i drugih detalej GTD iz litejnyh zharoprochnyh i intermetallidnyh splavov s monokristallicheskoj strukturoj [New industrial high-gradient UVNS-6 for manufacture of GTE blades and other parts from casting heat-resistant and intermetallic alloys with single-crystal structure] // Aviacionnye materialy i tehnologii. 2014. №4. S. 31–36.
- Orlov M.R., Yakimova M.S., Letov A.F. Analiz rabotosposobnosti monokristallicheskih lopatok turbiny vysokogo davleniya v sostave nazemnyh gazoturbinnyh ustanovok [The analysis of operability of single-crystal turbine blades of high pressure as a part of land gas turbine units] //Aviacionnye materialy i tehnologii. 2012. №S. S. 399–407.
- Krylov O.V. Geterogennyj kataliz [Heterogeneous catalysis]. M.: Akademkniga, 2004. 679 s.
- Stepanov A.V. Poluchenie vodoroda i vodorodsoderzhashhih gazov [Receiving hydrogen and vodorodsoderzhashchy gases]. Kiev: Naukova dumka, 1982. 312 s.
- Tolorajya V.N., Kablov E.N., Orehov N.G. Tehnologii litya monokristallicheskih turbinnyh lopatok GTD i GTU [Casting technologies of single-crystal turbine blades of GTE and GTU] // Aviacionnye materialy i tehnologii. 2003. №1. S. 63–79.
- Shalin R.E., Svetlov I.L., Kachanov E.B. Monokristally nikelevyh zharoprochnyh splavov [Monocrystals of nickel hot strength alloys]. M.: Mashinostroenie, 1977, 336 s.
- Ospennikova O.G., Orlov M.R., Avtaev V.V. Anizotropiya uprugoplasticheskih harakteristik zharoprochnyh nikelevyh splavov – osnova konstruirovaniya monokristallicheskih turbinnyh lopatok [Anisotropy of elasto-plastic characteristics of heat resisting nickel alloys – basis of designing of single-crystal turbine blades] // Deformaciya i razrushenie materialov. 2013. №11. S. 12–19.
- Krivko A.I., Epishin A.I., Svetlov I.L., Samojlov A.I. Uprugie svojstva monokristallov nikelevyh splavov [Elastic properties of monocrystals of nickel alloys] // Problemy prochnosti. 1988. №2. C. 68–75.
- Svetlov I.L., Suhanov N.N., Krivko A.I. Temperaturnaja zavisimost' harakteristik kratkovremennoj prochnosti, modulja Junga i kojefficienta linejnogo rasshirenija monokristallov splava ZhS6F[Temperature dependence of characteristics of short-term durability, Ung’s module and factor of linear dilatation of monocrystals of alloy of ZhS6F] // Problemy prochnosti. 1987. №4. C. 51–56.