The applicability of the sulfate-ammonium cadmium plating solution with additive TsKN-04 for the aviation industry

Nikiforov A.A., Smirnov K.N., Kravchenko D.V., Arhipov E.A., Zakirova L.I., Vinogradov S.S.
Nikiforov A.A., Smirnov K.N., Kravchenko D.V., Arhipov E.A., Zakirova L.I., Vinogradov S.S. The applicability of the sulfate-ammonium cadmium plating solution with additive TsKN-04 for the aviation industry // Proceedings of VIAM. 2016. No. 12. DOI: 10.18577/2307-6046-2016-0-12-12-12. URL: https://viam-works.ru/en/journal/2016/12/12
Keywords
cadmium plating, sulfate-ammonium electrolyte, additive TsKN-04, current efficiency, scattering power, covering power
Abstract

In sulfate-ammonium cadmium plating solution with additive TsКN-04 the concentration ranges of the components of the electrolyte are identified to allow obtaining light compact cadmium coatings on complex geometry parts. The electrolyte has a high scattering (50–94%) and covering (92–95%) power that are comparable and sometimes exceeding the same parameters from cyanide electrolytes. With carrying out preventive corrections the electrolyte shows high operational stability and it can be applied in mass production. Mechanical tests show that the technology of deposition of cadmium coating in the sulfate-ammonium bath with the additive TsKN-04 does not influence on mechanical properties of medium strength steels 30kHGSА. The work is executed within the implementation of the complex scientific direction 17.2. «Slip, gas-dynamic and combined coatings for details from carbon steels, including high-strength steels» («The strategic directions of development of materials and technologies of th

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Materialy dlya izdeliya «Buran» – innovacionnye resheniya formirovaniya shestogo tehnologicheskogo uklada [Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  3. Markova E.S., Pokrovskaya N.G., Shalkevich A.B., Gromov V.I. Martensitostareyushhie stali – novye perspektivnye materialy dlya valov GTD // Aviacionnye materialy i tehnologii. 2012. №S. S. 81–84.
  4. 4 Ivanov E.V. Sozdanie iznosostojkih i antifrikcionnyh materialov i pokrytij dlja kosmicheskogo korablja «Buran» [Creation of wearproof and antifriction materials and coverings for the «Buran» spacecraft] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 142–151.
  5. Kablov E.N., Kirillov V.N., Zhirnov A.D., Starcev O.V., Vapirov Yu.M. Centry dlya klimaticheskih ispytanij aviacionnyh PKM [The centers for climatic tests of aviation PCM] // Aviacionnaya promyshlennost. 2009. №4. S. 36–46.
  6. Kablov E.N., Starcev O.V., Medvedev I.M., Panin S.V. Korrozionnaya agressivnost primorskoj atmosfery. Ch. 1. Faktory vliyaniya (Obzor) [Corrosion aggression of the seaside atmosphere. P.1. Factors of influence (Overview)] // Korroziya: materialy, zashhita. 2013. №12. S. 6–18.
  7. Kablov E.N., Startsev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [Review of international experience on corrosion and corrosion protection] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87
  8. Vinogradov S.S. Ekologicheski bezopasnoe galvanicheskoe proizvodstvo. 2-e izd., pererab. i dop. [Ecologically safe galvanic production. 2nd ed., rev. and add.] . M.: Globus, 2002. 352 s.
  9. Vyacheslavov P.M. Elektroliticheskoe osazhdenie splavov [Electrolytic deposition of alloys]. L.: Mashinostroenie, 1986. 112 s.
  10. Taranceva K.R., Nikolotov A.D. Elektroosazhdenie splava olovo-cink iz stabilizirovannogo pirofosfatnogo elektrolita kak alternativa kadmievomu pokrytiyu [Alloy electrosedimentation tin-zinc from the stabilized pirofosfatny electrolit as alternative to cadmic covering] // Korroziya: materialy, zashhita. 2014. №3. S. 27–30.
  11. Celujkin V.N., Koreshkova A.A. O korrozionnyh svojstvah kompozicionnyh pokrytij cink–uglerodnye nanotrubki [About corrosion properties of composition coverings zinc – carbon nanotubes] // Korroziya: materialy, zashhita. 2014. №3. S. 31–34.
  12. Vinogradov S.S., Gubenkova O.A., Mamontova N.N., Nikiforov A.A., Balahonov S.V. Svojstva modificirovannogo cinkovogo pokrytiya [Properties of the modified zinc coating] // Korroziya: materialy, zashhita. 2015. №3.
  13. S. 24–30.
  14. Karimova S.A., Pavlovskaya T.G. Razrabotka sposobov zashhity ot korrozii konstrukcij, rabotajushhih v usloviyah kosmosa [Development of ways of corrosion protection of the designs working in the conditions of space] // Trudy VIAM: electron. nauch.-tehnich. zhurn. 2013. №4. St. 02. Available at: http://www.viam-works.ru (accessed: May 16, 2016).
  15. S.S. Vinogradov, A.A. Nikiforov, S.V. Balakhonov Zamena kadmija. Etap 1. Povyshenie zashhitnoj sposobnosti cinkovyh pokrytij: termoimmersionnoe i modificirovannoe pokrytija
  16. [Cadmium replacement. Part 1. Improving of protective property of zinc coatings: thermo-immersed and modified coatings] // Aviacionnye materialy i tehnologii. 2015. №4. S. 53–60. DOI: 10.18577/2071-9140-2015-0-4-53-60.
  17. Vajner Ya.V., Dasoyan M.A. Tehnologiya elektrohimicheskih pokrytij [Technology of electrochemical coatings]. M.: Mashgiz, 1962. 468 s.
  18. Maksimchuk V.N., Polovnikov S.P. Vodorodnoe rastreskivanie vysokoprochnyh stalej posle naneseniya galvanohimicheskih pokrytii [Hydrogen assisted cracking high-strength steel after drawing galvanic chemical covering]. M.: Energoatomizdat, 2002. 320 s.
  19. Beloglazov S.M. Navodorozhivanie stali pri elektrohimicheskih processah [Steel hydrogen saturation at electrochemical processes]. L.: Izd-vo LGU, 1975. 412 s.
  20. Maksimchuk V.N., Maksimchuk E.V. Proniknovenie vodoroda cherez stal pri kadmirovanii s podsloyami [Hydrogen penetration through steel at cadmium plating with intermediate layers] // Elektrohimiya. 1977. T. XIII. Vyp. II. S. 1646–1652.
  21. Kudryavcev N.T. Elektrohimicheskie pokrytiya metallami [Electrochemical coatings metals]. M.: Himiya, 1979. 352 s.
  22. Smirnov K.N., Arhipov E.A., Kravchenko D.V. K voprosu o kroyushhej sposobnosti elektrolitov [To question of covering ability of electrolits] // Galvanotehnika i obrabotka poverhnosti. 2015. T. 23. №3. S. 30–34.
  23. Smirnov K.N., Kravchenko D.V., Arhipov E.A. Kroyushhaya sposobnost elektrolitov kadmirovaniya [Covering ability of electrolits of cadmium plating] // Galvanotehnika i obrabotka poverhnosti. 2013. T. 21. №4. S. 30–32.
  24. Azhogin F.F. Korrozionnoe rastreskivanie i zashhita vysokoprochnyh stalej [Corrosion cracking and protection high-strength staly]. M.: Metallurgiya, 1974. 245 s.
  25. Korrozionnoe rastreskivanie metallov / pod obshh. red. V.V. Romanova [Corrosion cracking of metals / gen. ed. by V.V. Romanov]. M.: Mashgiz, 1960. 186 s.