Detection of defects in multilayer constructions by ultrasonic resonance method
UDC
620.179.1:678.061
DOI
10.18577/2307-6046-2016-0-11-12-12
Article PDF (Russian)
(590.32 KB)
How to cite
Murashov V.V., Slyusarev M.V. Detection of defects in multilayer constructions by ultrasonic resonance method // Proceedings of VIAM. 2016. No. 11. DOI: 10.18577/2307-6046-2016-0-11-12-12. URL: https://viam-works.ru/en/journal/2016/11/12
Keywords
non-destructive testing, ultrasonic resonance method, multilayer constructions, defects of glued joints, material stratifications, coupling medium.
Abstract
Research results of operation capabilities of ultrasonic resonance method during multilayer constructions control are given. It is shown that the resonance method can be used for detection of glued joints defects and stratifications in constructions from metal and non-metallic materials. Recommendations about application of contact environment on water basis for acoustic contact between piezoelectric invertor of the defectoscope and controlled product are made.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Kontrol kachestva materialov – garantiya bezopasnosti ekspluatatsii aviatsionnoy tekhniki [Quality control of materials – security accreditation of operation of aviation engineering] // Aviacionnye materialy i tehnologii. M.: VIAM, 2001. Vyp. «Metody ispytaniy i kontrolya kachestva metallicheskikh i nemetallicheskikh materialov». S. 3–8.
- Lukina N.F., Dementeva L.A., Petrova A.P., Serezhenkov A.A. Konstrukcionnye i termostojkie klei [Constructional and heat-resistant glues] // Aviacionnye materialy i tehnologii. 2012. №S. S. 328–335.
- Kablov E.N., Minakov V.T., Anikhovskaya L.I. Klei i materialy na ikh osnove dlya remonta konstruktsiy aviatsionnoy tekhniki [Glues and materials on their basis for repair of designs of aviation engineering] // Aviacionnye materialy i tehnologii. 2002. №1.
- S. 61–65.
- Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Entsiklopedicheskiy spravochnik. 2008. №3. S. 2–14.
- Nerazrushayushchiy kontrol: spravochnik / pod obshch. red. V.V. Klyueva [Non-destructive testing: directory / gen. ed. by V. V. Klyuyev]. M.: Mashinostroenie, 2006. T. 3. Ultrazvukovoy kontrol / I.N. Ermolov, Yu.V. Lange. 864 s.
- Murashov V.V. Kontrol kleenykh konstruktsiy [Control of glued designs] // Klei. Germetiki. Tekhnologii. 2005. №1. S. 21–27.
- Kablov E.N., Sivakov D.V., Gulyaev I.N., Sorokin K.V., Fedotov M.Yu., Goncharov V.A. Metody issledovaniya konstrukcionnyh kompozicionnyh materialov s integrirovannoj elektromehanicheskoj sistemoj [Methods of research of constructional composite materials with the integrated electromechanical system] //Aviacionnye materialy i tehnologii. 2010. №4. S. 17–20.
- Murashov V.V. Nerazrushayushchiy kontrol kleevykh soedineniy [Non-destructive testing of glued joints] // Klei. Germetiki. Tekhnologii. 2008. №7. S. 21–28.
- Murashov V.V. Nondestructive Testing of Glued Joints // Polymer Science. Series D. Glues and Sealing Materials. 2009. V. 2. №1. Р. 58–63.
- Murashov V.V., Rumyantsev A.F. Defekty monolitnykh detaley i mnogosloynykh konstruktsiy iz polimernykh kompozitsionnykh materialov i metody ikh vyyavleniya. Chast 1. Defekty monolitnykh detaley i mnogosloynykh konstruktsiy iz polimernykh kompozitsionnykh materialov [Defects of monolithic details and multi-layer designs from polymeric composite materials and methods of their identification. Part 1. Defects of monolithic details and multi-layer designs from polymeric composite materials] // Kontrol. Diagnostika. 2007. №4. S. 23–32.
- Kablov E., Murashov V., Rumyantsev A. Diagnostics of Polymer Composites by Acoustic Methods // Ultrasound. Kaunas: Tecnologija. 2006. №2. Р. 7–10.
- Murashov V.V. Opredelenie fiziko-mehanicheskih harakteristik i sostava polimernyh kompozicionnyh materialov akusticheskimi metodami [Definition of physicomechanical characteristics and composition of polymeric composite materials acoustic methods] // Aviacionnye materialy i tehnologii. 2012. №S. S. 465–475.
- Murashov V.V., Rumyantsev A.F., Ivanova G.A., Fayzrakhmanov N.G. Diagnostika struktury, sostava i svoystv polimernykh kompozitsionnykh materialov [Diagnostics of structure, structure and properties of polymeric composite materials] // Aviacionnye materialy i tehnologii. 2008. №1. S. 17–24.
- Karabutov A.A., Murashov V.V., Podymova N.B. Diagnostika sloistykh kompozitov s pomoshch'yu lazernogo optiko-akusticheskogo preobrazovatelya [Diagnostics of layered composites by means of the laser optics-acoustic converter] // Mekhanika kompozitnykh materialov. Riga. 1999. T. 35. №1. S. 125–134.
- Karabutov A.A., Murashov V.V., Podymova N.B., Oraevsky A.A. Nondestructive characterization of layered composite materials with a laser optoacoustic sensor // Proceedings of SPIE – The International Society for Optical Engineering Nondestructive Evaluation of Materials and Composites II. San Antonio. TX. 1998. P. 103–111.
- Murashov V.V., Rumyantsev A.F. Diagnostika sostava i svoystv polimernykh kompozitov v detalyakh i konstruktsiyakh [Diagnostics of structure and properties of polymeric composites in details and designs] // Kontrol. Diagnostika. 2008. №8. S. 13–17.
- Mishurov K.S., Murashov V.V. Determination of the Composition and Density of Polymer Composite Materials in Details and Constructions by Nondestructive Methods // Polymer Science. Series D. 2016. V. 9. №2. P. 176–180.
- Murashov V.V. Kontrol kleenykh konstruktsiy akusticheskim impedansnym metodom [Control of glued designs by acoustic impedance method] // Klei. Germetiki. Tekhnologii. 2010. №3. S. 13–20.
- Murashov V.V. Kontrol monolitnykh i kleenykh konstruktsiy iz polimernykh kompozitsionnykh materialov akusticheskim impedansnym metodom [Control of monolithic and glued designs from polymeric composite materials acoustic impedance method] // Aviacionnaya promyshlennost. 2009. №3. C. 43–48.
- Murashov V.V. Identification of Areas of Absence of Adhesive Bonding between Layers in Multilayer Structures // Polymer Science. Series D. Glues and Sealing Materials. 2014. V. 7. №1. Р. 46–48.
- Murashov V.V. Nerazrushayushchie metody kontrolya kachestva kleevykh soedineniy [Non-destructive methods of quality control of glued joints] // Vse materialy. Entsiklopedicheskiy spravochnik. 2008. №9. S. 20–26.
- Murashov V.V. Attestation of Glued Articles by Acoustic Impedance Method // Polymer Science. Series D: Glues and Sealing Materials. 2010. V. 3. №4. Р. 267–273.
- Murashov V.V. Control of Glued Structures by the Electromagnetic Acoustic Variant of the Impedance Method // Polymer Science. Series D. Glues and Sealing Materials. 2014. V. 7. №2. Р. 136–139.
- Murashov V.V. Control of Multilayer Constructions by Spectral Acoustic-Impedance Defectoscopy // Polymer Science. Series D: Glues and Sealing Materials. 2014. V. 7. №2. Р. 133–135.
- Murashov V.V., Generalov A.S. Kontrol mnogoslojnyh kleenyh konstrukcij nizkochastotnymi akusticheskimi metodami [Control of multilayer adhesive structures operating in severe climatic condition] // Aviacionnye materialy i tehnologii. 2014. №2. S. 59–67.
- Bakunov A.S., Murashov V.V., Sysoev A.M. Kontrol lopastey vozdushnogo vinta sredstvami nizkochastotnoy akustiki [Control of blades of air screw by means of low-frequency acoustics] // Kontrol. Diagnostika. 2012. №6. S. 72–74.
- Murashov V.V. Kontrol kleenykh konstruktsiy akusticheskim metodom svobodnykh kolebaniy [Control of glued designs by acoustic method of free fluctuations] // Klei. Germetiki. Tekhnologii. 2012. №4. S. 40–44.
- Murashov V.V. Kontrol kleenykh konstruktsiy iz raznorodnykh materialov ultrazvukovym reverberatsionnym metodom [Control of glued designs from diverse materials ultrasonic reverberatsionny method] // Klei. Germetiki. Tekhnologii. 2015. №12. S. 18–22.
- Murashov V.V., Trifonova S.I. Kontrol kachestva polimernyh kompozicionnyh materialov ultrazvukovym vremennym sposobom velosimetricheskogo metoda [Quality control of polymer composite materials using ultrasonic time-of-flight velocimetric technique] // Aviacionnye materialy i tehnologii. 2015. №4. S. 86–90.
- Murashov V.V., Trifonova S.I. Kontrol kleevykh soedineniy v konstruktsiyakh i izdeliyakh iz PKM ultrazvukovym tenevym metodom [Control of glued joints in designs and products from PKM ultrasonic shadow method] // Klei. Germetiki. Tekhnologii. 2015. №5. S. 15–23.
- Murashov V.V. Kontrol kleenykh konstruktsiy akustiko-topograficheskim metodom [Control of glued designs by acoustic-topographical method] // Klei. Germetiki. Tekhnologii. 2016. №3. S. 21–27.
- Murashov V.V. Glued Joint Strength Diagnostics // Polymer Science. Series D: Glues and Sealing Materials. 2009. V. 2. №1. Р. 64–70.
- Lange Yu.V. Akusticheskie nizkochastotnye metody i sredstva nerazrushayushchego kontrolya mnogosloynykh konstruktsiy [Acoustic low-frequency methods and means of non-destructive testing of multi-layer designs]. M.: Mashinostroenie, 1991. 272 s.
- Murashov V.V., Laptev A.S. Kontaktnye zhidkosti dlya sozdaniya akusticheskogo kontakta pri ul'trazvukovom kontrole mnogoslojnyh konstrukcij iz PKM [Contact liquids for creation of an acoustic contact at ultrasonic control of multi-layer structures from PCM] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2015. №8. St. 10. Available at: http://www.viam-works.ru (accessed: May 17, 2016). DOI: 10.18577/2307-6046-2015-0-8-10-10.