Peculiarities of high-strength aluminum-lithium alloys laser weldin

Lukin V.I., Ioda E.N., Panteleev M.D., Skupov A.A.
Lukin V.I., Ioda E.N., Panteleev M.D., Skupov A.A. Peculiarities of high-strength aluminum-lithium alloys laser weldin // Proceedings of VIAM. 2016. No. 10. DOI: 10.18577/2307-6046-2016-0-10-7-7. URL: https://viam-works.ru/en/journal/2016/10/7
Keywords
laser welding, aluminum-lithium alloys welding, mechanical properties, heat treatment, fractographic research, metallographic research.
Abstract

The structure formation features and mechanical properties of laser welded joints of Al–Li alloys V-1461, V-1469 are studied. It is found that the use of Al–Cu (Al–6Cu and Al–10Cu) filler materials improves the welded seam formation and mechanical properties of welded joint, reduces probability of defects formation such as porosity and incomplete fusion. For the welding joints done by laser welding with or without filler materials Sv-1201 and Sv-1217 there is no tendency to exfoliation and intergranular corrosion of laser welded joints. Postweld heat treatment slightly reduces the corrosion resistance. The work is executed within the frames of the complex scientific direction 10.8. «Fusion welding technologies of new structural materials» («The strategic direction of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Lukin V.I., Ospennikova O.G. Perspektivnye alyuminievye splavy i tehnologii ih soedineniya dlya izdelij aviakosmicheskoj tehniki [Perspective aluminum alloys and technologies of their connection for products of aerospace equipment] // Tez. dokl. 2-j Mezhdunar. konf. i vyst. «Alyuminij–21. Svarka i pajka». 2012. S. 8.
  3. Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanium, magnesium, beryllium and aluminum alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
  4. Grushko O.E., Ovsyannikov B.V., Ovchinnikov V.V. Alyuminievo-litievye splavy: metallurgiya, svarka, metallovedenie [Aluminum-lithium alloys: metallurgy, welding, metallurgical science]. M.: Nauka, 2014. 296 s.
  5. Kablov E.N., Lukin V.I., Zhegina I.P. i dr. Osobennosti i perspektivy svarki alyuminij-litievyh splavov [Features and welding perspectives aluminum-lithium alloys] // Aviacionnye materialy i tehnologii. M.: VIAM, 2002. Vyp.: Tehnologiya proizvodstva aviacionnyh metallicheskih materialov. S. 3–12.
  6. Kablov E.N., Lukin V.I., Ospennikova O.G. Svarka i pajka v aviakosmicheskoj promyshlennosti [Welding and the soldering in the aerospace industry] // Svarka i bezopasnost: Mater. Vseros. nauch.-praktich. konf. 2012. T. 1. S. 21–30.
  7. Lukin V.I., Ospennikova O.G., Ioda E.N., Panteleev M.D. Svarka alyuminievyh splavov v aviakosmicheskoj promyshlennosti [Welding of aluminum alloys in the aerospace industry] // Svarka i diagnostika. 2013. №2. S. 47–52.
  8. Shiganov I.N., Holopov A.A., Trushnikov A.V. i dr. Lazernaya svarka vysokoprochnyh alyuminij-litievyh splavov s prisadochnoj provolokoj [Laser bonding high-strength aluminum-lithium alloys with filler wire] // Svarochnoe proizvodstvo. 2016. №6. S. 44–50.
  9. Lukin V.I., Shalin R.E., Efremov I.S., Yarovinskii Yu.U. Design and fabrication of large structures of aluminium-lithium alloys for aerospace technology // Welding International. 1997. V. 11. №5. P. 387–392.
  10. Shiganov I.N., Shahov S.V., Holopov A.A. Lazernaya svarka alyuminievyh splavov aviacionnogo naznacheniya [Laser bonding of aluminum alloys of aviation assignment] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2012. №5. S. 34–50.
  11. Hohlatova L.B., Blinkov V.V., Kondratyuk D.I., Ryabova E.N., Kolesenkova O.K. Struktura i svojstva svarnyh soedinenij listov iz splavov 1424 i V-1461, izgotovlennyh lazernoj svarkoj [Structure and properties of welded joints of sheets from 1424 and V-1461 alloys made by laser welding] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 9–13. DOI: 10.18577/2071-9140-2015-0-4-9-13.
  12. Milewski J.O., Lewis O.K., Wittig J.E. Microstructural Evaluation of Low and High Duty Cycle Nd:YAG Laser Beam Welds in 2024-T3 aluminum // Welding Journal. 1993. V. 72. №7. P. 341–346.
  13. Lukin V.I., Ioda E.N., Panteleev M.D., Skupov A.A. Vliyanie termicheskoj obrabotki na harakteristiki svarnyh soedinenij vysokoprochnyh alyuminijlitievyh splavov [Heat treatment influence on characteristics of welding joints of high-strength aluminum-lithium alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №4. St. 06. Available at: http://www.viam-works.ru (accessed: July 07, 2016). DOI: 10.18577/2307-6046-2015-0-4-6-6.
  14. Annin B.D., Fomin V.M., Antipov V.V., Ioda E.N., Karpov E.V., Malikov A.G., Orishich A.M., Cherepanov A.N. Issledovanie tehnologii lazernoj svarki alyuminievogo splava 1424 [Research of technology of laser bonding of aluminum alloy 1424] // Doklady Akademii nauk, 2015. T. 465. №4. S. 1–6.
  15. Morozova L.V., Ishodzhanova I.V. Issledovanie zakonomernostej izmeneniya relefa poverhnosti obrazcov iz alyuminij-litievyh splavov metodom lazernoj mikroskopii [Research of patterns of change of a relief of a surface of samples from aluminumlithium alloys a method of laser microscopy] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №10. St. 08. Available at: http://www.viam-works.ru (accessed: July 07, 2016). DOI: 10.18577/2307-6046-2014-0-10-8-8.