Morozova G.I. The importance of physicochemical phase analysis technique in the development of aviation metallic material science and creation of Ni-based superalloys. (Dedicated to the 125th anniversary of the N.I. Blok’s birth) // Proceedings of VIAM. 2016. No. 1 (37). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-1-50-55.

The importance of physicochemical phase analysis technique in the development of aviation metallic material science and creation of Ni-based superalloys. (Dedicated to the 125th anniversary of the N.I. Blok’s birth)

Morozova G.I.
Abstract

In this paper the historical aspect of foundation and development of physicochemical phase analysis technique for investigation of aviation alloys with different basic metals was considered. This work is dedicated to the memory of Natalia I. Blok in connection with the 125th anniversary of her birth. In fairness, it must be said that N.I. Blok and her research team discovered the γ'-phase in Nickel superalloy EI437B and founded the role of aluminum in γ'-phase formation, which was done for the first time in the world. This discovery contributed to the accelerated development of new superalloys for hot sections of gas turbine engines. The discovery of the fine dispersed γ'-phase formed the basis of the theory of heterophase superalloys strengthening, this theory was advocated by the academician S.T.Kishkin. The main achievements in the field of research of nickel alloys chemistry by the physicochemical phase analysis applicable in selection of new alloy compositions, in study of phase t

Reference list
  1. Kishkin S.T., Lashko N.F., Popova N.M., Zaslavskaja L.V., Rybina M.F., Platonova A.F. Primenenie differencialnogo karbidnogo analiza dlya izucheniya prirody vtorichnoj tverdosti stali [Application of the differential carbide analysis for studying of the nature of secondary hardness of steel] / V sb. nauch. tr. VIAM. M. : Oborongiz, 1957. Vyp. 6. S. 88–95.
  2. Popova N.M. Karbidnyj analiz stali [Carbide steel analysis]. M.: Oborongiz, 1956. 100 s.
  3. Lashko N.F., Zaslavskaya L.V., Kozlova M.N., Morozova G.I., Sorokina K.P., Yakovleva E.F. Fiziko-himicheskij fazovyj analiz stalej i splavov [Physical and chemical phase analysis staly and alloys]. M.: Metallurgiya, 1978. 336 s.
  4. Kishkin S.T., Kablov E.N. Litejnye zharoprochnye splavy dlya turbinnyh lopatok [Foundry hot strength alloys for turbine blades] / V sb.: Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002 : yubilejnyj nauch.-tehnich. sb. / pod red. E.N. Kablova. M.: VIAM, 2002. S. 48–58.
  5. Kablov E.N., Kishkin S.T. Perspektivy primenenija litejnyh zharoprochnyh splavov dlja proizvodstva turbinnyh lopatok GTD [Perspectives of application of foundry hot strength alloys for production of turbine blades of GTE] // Gazoturbinnye tehnologii. 2002. №1. S. 34–37
  6. Kishkin S.T., Logunov A.V., Petrushin N.V., Glezer G.M., Kuleshova E.A., Morozova S.G. Nauchnye osnovy legirovaniya zharoprochnyh nikelevyh splavov [Scientific bases of alloying of heat resisting nickel alloys] / V sb.: Voprosy aviacionnoj nauki i tehniki : nauch.-tehnich. sb. Ser. «Aviacionnye materialy». M.: VIAM, 1987. S. 6–18.
  7. Lomberg B.S., Ovsepjan S.V., Bakradze M.M. Osobennosti legirovaniya i termicheskoj obrabotki zharoprochnyh nikelevyh splavov dlya diskov gazoturbinnyh dvigatelej no-vogo pokoleniya [Features of alloying and thermal processing of heat resisting nickel alloys for disks of gas turbine engines of new generation] // Aviacionnye materialy i tehnologii. 2010. №2. S. 3–8.
  8. Kishkin S.T., Morozova G.I., Belyaev M.S., Gnevsheva A.I., Sorokina L.P. Fazovye prevrashheniya v zharoprochnom nikelevom splave ZhS6U, ispytannom na ustalost [Phase transformations in the heat resisting ZhS6U nickel alloy tested for fatigue] // Fizika metallov i metallovedenie. 1984. T. 58. Vyp. 6. S. 1171–1178.
  9. Morozova G.I. Fenomen γ-fazy [Phenomenon γ'-phases] // Doklady AN SSSR. 1992. T. 325. № 6. S. 1193–1198.
  10. Kablov E.N., Buntushkin V.P., Morozova G.I., Bazyleva O.A. Osnovnye principy legirovaniya intermetallida Ni3Al pri sozdanii vysokotemperaturnyh splavov [The basic principles of alloying of Ni3Al intermetallic compound at creation of high-temperature alloys] // Materialovedenie. 1998. №7. S. 13–17.
  11. Kishkin S.T., Morozova G.I. Osobennosti metoda fiziko-himicheskogo fazovogo analiza sovremennyh zharoprochnyh nikelevyh splavov [Features of method of the physical and chemical phase analysis of modern heat resisting nickel alloys] // Voprosy aviacionnoj nauki i tehniki : nauch.-tehnich. sb. Ser. «Aviacionnye materialy». M.: VIAM, 1987. S. 86–93.
  12. Morozova G.I. Zakonomernost formirovaniya himicheskogo sostava /-matricy mnogokomponentnyh nikelevyh splavov [Pattern of forming of chemical composition of /-matrix of multicomponent nickel alloys] // Doklady AN SSSR. 1991. T. 320. №6. S. 1413–1416.
  13. Morozova G.I. Kompensaciya disbalansa legirovaniya zharoprochnyh nikelevyh splavov [Compensation of imbalance of alloying of heat resisting nickel alloys] // MiTOM. 2012. №12. S. 52–56.
  14. Kablov E.N., Petrushin N.I. Kompyuternyj metod konstruirovaniya litejnyh zharoprochnyh nikelevyh splavov [Computer method of designing of cast heat resisting nickel alloys] / V sb.: Litejnye zharoprochnye splavy. Effekt Kishkina. M.: Nauka, 2006. S. 56–78.
  15. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  16. Belov N.A. Ekonomnolegirovannye zharoprochnye alyuminievye splavy: principy optimizacii fazovogo sostava [Economically alloyed heat resisting aluminum alloys: principles of optimization of phase structure] // Aviacionnye materialy i tehnologii. 2011. №2. S. 6–11.
  17. Karachevtsev F.N., Zagvozdkina T.N., Orlov G.V. Razrabotka i issledovanie metrologicheskih harakteristik ekspress-metodiki analiza zharoprochnyh nikelevyh splavov [Development and research of metrological characteristics of express-analysis of heat-resistant nickel alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №11. St. 09. Available at: http://www.viam-works.ru (accessed: October14, 2015). DOI: 10.18577/2307-6046-2015-0-11-9-9.