Phosphorus and sulfur segregation in model heat resisting nickel alloy

Chabina E.B.
Chabina E.B. Phosphorus and sulfur segregation in model heat resisting nickel alloy // Proceedings of VIAM. 2015. No. 9. DOI: 10.18577/2307-6046-2015-0-9-2-2. URL: https://viam-works.ru/en/journal/2015/9/2
Abstract

Harmful impurity (sulfur and phosphorus) and microalloying additives (boron and lanthanum) competition at model heat resisting nickel alloy of Ni–Co–Cr–Al–Ti–W–Mo–Nb system inner interfaces segregations formation was investigated. It was shown that sulfur and phosphorus form segregation on grain boundaries and interphase interfaces «inclusion – matrix». Boron and lanthanum force out sulfur and phosphorus from interfaces, and these microalloying additives action mechanisms are different: boron refines and strengthens grain boundaries, and the lanthanum connects sulfur and phos-phorus in favorable morphology inclusions

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period to 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlja aviacionnogo dvigatelestroenija [Creation of modern heat resisting materials and technologies of their production for aviation engine building] //Kryl'ja Rodiny. 2012. №3–4. S. 34–38.
  3. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharoprochnye nikelevye splavy dlja detalej gazoturbinnyh dvigatelej [High-temperature heat resisting nickel alloys for details of gas turbine engines] //Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
  4. Lomberg B.S., Bakradze M.M., Chabina E.B., Filonova E.V. Vlijanie mikrolegirujushhih jelementov na strukturno-fazovuju stabil'nost' i svojstva zharoprochnogo deformiruemogo splava (pri dlitel'nyh narabotkah) [Influence of microdoping elements on structural and phase stability and property of heat resisting deformable alloy (at long practices)] //Metallurg. 2013. №9. S. 93–97.
  5. Lomberg B.S., Ovsepjan S.V., Bakradze M.M. Osobennosti legirovanija i termicheskoj obrabotki zharoprochnyh nikelevyh splavov dlja diskov gazoturbinnyh dvigatelej novogo pokolenija [Features of alloying and thermal processing of heat resisting nickel alloys for disks of gas turbine engines of new generation] //Aviacionnye materialy i tehnologii. 2010. №2. S. 3–8.
  6. Artjushov V.N., Kudrin A.A., Kirpichnikov M.S., Ponomareva L.L. Vlijanie mikrolegirovanija na tehnologicheskuju plastichnost' zharoprochnogo splava HN62MBKTJu (JeP742) [Influence of microalloying on technological plasticity of HN62MBKTYU hot strength alloy (ЭП742)] //Metallurg. 2011. №8. S. 69–72.
  7. Chabina E.B., Filonova E.V., Lomberg B.S., Zajcev D.V. Osobennosti formirovanija struktury vysokozharoprochnogo nikelevogo splava pri kompleksnom mikrolegirovanii lantanoidami [Features of forming of structure of high-heat resisting nickel alloy at complex microalloying lanthanoids] //Metally. 2014. №6. S. 62–69.
  8. Kozlov Je.V., Nikonenko E.L., Popova N.A., Koneva N.A. Vlijanie legirovanija lantanom na fazovyj sostav supersplava na osnove Ni–Al–Cr [Alloying influence by lanthanum on phase structure of superalloy on the basis of Ni–Al–Cr] //Vestnik TGU. 2013. T. 18. №4. S. 1527–1528.
  9. Supersplavy [Superalloys]. T. II /Pod red. Ch.T. Simsa, N.S. Stoloffa, U.K. Hagelja. M.: Metallurgija. 1995. Kn. 1. 384 s.
  10. Ohrupchivanie konstrukcionnyh stalej i splavov [Okhrupchivaniye constructional staly and alloys] /Pod red. K.L. Brajenta, S.K. Bener-dzhi. M.: Metallurgija. 1988. 551 s.
  11. Gibbons T.B. Some effects of trace elements in reducing creep performance in high-strength superalloys //Materials Science and Technology. 1985. №1. P. 1033–1039.
  12. Guttmann M. The influence of interfacial segregation in embrittlement phenomena //Adv. Mech. and Phys. Surfaces. 1981. V. 1. P. 1–109.
  13. McLean M., Strang A. Effects of trace elements on mechanical properties of superalloys //Metals Technology. 1984. V. 11. №10. P. 454–465.
  14. Meetham G.W. Trace elements in superalloys (review) //Metals technology. 1984. V. 11. №10. P. 414–418.
  15. Fizicheskoe metallovedenie. T. 1. Atomnoe stroenie metallov i splavov [Physical metallurgical science. V. 1. Nuclear structure of metals and alloys] /Pod red. R.U. Kana, P. Haazena. M.: Metallurgija. 1987. 639 s.
  16. Guttmann M. Temper embrittlement and ternary equilibrium segregation //Material Science and Engineering. 1980. V. 42. P. 227–232.
  17. Mak Lin D. Granicy zeren v metallah [Borders of grains in metals]. M.: Metallurgizdat. 1960. 322 s.
  18. Zhuanggi H., Hongwei S., Shouren G. Role of P, S and B on creep behavior of alloy 718 //Jour-nal of Material Science and Technology. 2001. V. 17. №4. P. 399–402.
  19. Bokshtejn S.Z., Vasilenok L.B., Kishkin S.T., Radin I.V., Shpunt K.Ja. Izotopnoe issledovanie mikrolegirovanija granic zeren v nikelevyh splavah [Isotope research of microalloying of borders of grains in nickel alloys] //Poverhnost'. Fizika. Himija. Mehanika. 1987. №3. S. 117–122.
  20. Bruemmer S.M., Jones R.H., Thomas M.T., Baer D.R. //Metallurgical Transaction. 1983. V. 14A. №2. P. 223.
  21. Mulford R.A. Grain Boundary Embrittlement of Ni and Ni Alloys //Treatise on materials sci-ence and technology. 1983. V. 25. P. 1–18.
  22. Swindeman R.W., Sikko V.H., Kluch R.L. //Metallurgical Transaction. 1983. V. 14A. №4. P. 584.
  23. Loier C., Boos J.Y. The influence of grain boundary sulfur concentration on the intergranular brittleness of nickel of different purities //Metallurgical Transaction. 1981. V. 12A. №7. P. 1223–1233.
  24. Guttmann M. Grain boundary segregation, two dimensional compound formation and precip-ita-tion //Metal Transaction. 1977. V. A8. №9. P. 1383–1403.
  25. Orehov N.G., Cherkasova E.R., Chabina E.B., Sidorenko V.I. Izuchenie poverhnostej razrushenija sovremennyh nikelevyh splavov metodom Ozhe-jelektronnoj spektroskopii [Studying of surfaces of destruction of modern nickel alloys by method Ozhe-elektronnoy of spectroscopy] /V sb. Voprosy aviacionnoj nauki i tehniki. Ser. «Aviacionnye materialy». Vyp. Metody issledovanija konstrukcionnyh materialov. M.: VIAM. 1987. S. 150–156.
  26. Kablov E.N., Bronfin M.B. Jeffekt S.T. Kishkina, ili pochemu struktura zharoprochnyh nikelevyh splavov dolzhna byt' geterofaznoj [Kishkin's effect or why the structure of heat resisting nickel alloys has to be heterophase] /V kn. Litejnye zharoprochnye splavy. Jeffekt S.T. Kishkina: nauchn.-tehn. sb.; Pod. red. E.N. Kablova. M.: Nauka. 2006. S. 7–14.
  27. Lomberg B.S., Bakradze M.M., Chabina E.B., Filonova E.V. Vzaimosvjaz' struktury i svojstv vysokozharoprochnyh nikelevyh splavov dlja diskov gazoturbinnyh dvigatelej [Interrelation of structure and properties of high-heat resisting nickel alloys for disks of gas turbine engines] //Aviacionnye materialy i tehnologii. 2011. №2. S. 25–30.
  28. Chabina E.B., Filonova E.V., Lomberg B.S., Morozova G.I. Jevoljucija struktury i fazovogo sostava deformiruemyh zharoprochnyh nikelevyh splavov dlja diskov GTD s uslozhneniem ih legirovanija [Evolution of structure and phase composition of deformable heat resisting nickel alloys for disks GTD with complication of their alloying] //MiТОМ. 2015. №3 (717). S. 8–12.
  29. Chabina E.B., Filonova E.V., Lomberg B.S., Bakradze M.M. Struktura sovremennyh deformiruemyh nikelevyh splavov [Structure of modern deformable nickel alloys] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №6. S. 22–27.
  30. Bokshtejn S.Z., Kishkin S.T., Shalin R.E. Strukturnaja stabil'nost' konstrukcionnyh materialov [Structure of modern deformable nickel alloys] /V sb. Aviacionnye materialy na rubezhe XX–XXI vekov. M.: VIAM. 1994. S. 547–553.
  31. Chabina E.B., Alekseev A.A., Filonova E.V., Lukina E.A. Primenenie metodov analiticheskoj mikroskopii i rentgenostrukturnogo analiza dlja issledovanija strukturno-fazovogo sostojanija materialov [Application of methods of analytical microscopy and the rentgenostrukturny analysis for research of structural and phase condition of materials] //Trudy VIAM. 2013. №5. St. 06 (viam-works.ru).
  32. Metody analiza poverhnosti [Methods of the analysis of surface] /Pod red. A. Zanderny. M.: Mir. 1979. 582 s.
  33. Edwards B.C., Byre B.L., Gage G. //Acta Metallurgica. 1980. V. 28. R. 335–356.
  34. Babikova Ju.F., Gusakov A.A., Rjabova T.T. Avtoradiografija po mgnovennomu izlucheniju [Autoradiography on prompt radiation]: Uchebnoe posobie. M.: MIFI. 1980. 52 s.
  35. Was G.S., Martin J.R. The influence of grain boundary precipitation on the measurement of chromium redistribution and phosphorous segregation in Ni–16Cr–9Fe //Metallurgical Trans-action. 1985. V. 16A. №3. P. 349–359.
  36. Guttmann M., Dumoulin P., Tan-Tai N., Fontaine P. An Auger Electron Spectroscopic study of phosphorus segregation in the grain boundaries of nickel base alloy 600 //Corrosion NACE. 1981. V. 37. №7. P. 416–425.
  37. Briant C.L. Grain boundary segregation in Ni-base alloy 182 //Metallurgical Transaction. 1988. V. 19A. №1. P. 137–143.