A device for machining of foamed polymer materials

Stolyankov Yu.V., Beider E.Ya., Platonov M.M., Petrova G.N.
Stolyankov Yu.V., Beider E.Ya., Platonov M.M., Petrova G.N. A device for machining of foamed polymer materials // Proceedings of VIAM. 2015. No. 5. DOI: 10.18577/2307-6046-2015-0-5-8-8. URL: https://viam-works.ru/en/journal/2015/5/8
Abstract

Some features of foamed polymer materials based on structure-purposed polyimides are considered in the article. Comparison of domestic foamed materials with their foreign analogues is also provided in the article to illustrate the possibility of their usage in the resource- and energy saving technology for production of three-layer sandwich panels. Existing processes for machining of the foamed material materials are described in the article in comparison with the offered device. Description of its structure and main advantages at machining of foamed polymers is given as well.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2013 goda [The strategic directions of development of materials and technologies of their processing for the period till 2013] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  3. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry in aviation materials science] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  4. Kablov E.N. Razrabotki VIAM dlja gazoturbinnyh dvigatelej i ustanovok [Development of VIAM for gas turbine engines and installations] //Kryl'ja Rodiny. 2010. №4. S. 31–33.
  5. Kablov E.N., Solntsev S.S., Rozenenkova V.A., Mironova N.A. Composite glass-metal coatings for protecting beryllium at high temperatures //Glass and Ceramics. 2012. P. 1–4.
  6. Fizicheskie i himicheskie processy pri pererabotke polimerov [Physical and chemical processes when processing polymers]. SPb: Nauchnye osnovy i tehnologii. 2013. 314 s.
  7. Bejder Je.Ja., Petrova G.N., Izotova T.F., Barbot'ko S.L. Stekloplastiki na termoplastichnoj matrice [Fibreglasses on thermoflexible matrix] //Trudy VIAM. 2013. №7. St. 03 (viam-works.ru).
  8. Doroshenko N.I., Chursova L.V. Jevoljucija materialov dlja lopastej vertoletov [Evolution of materials for blades of helicopters] //Aviacionnye materialy i tehnologii. 2012. №2. S. 16–18.
  9. Bejder Je.Ja., Gureeva E.V., Petrova G.N. Penopoliimidy [Penopoliimida] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №6. S. 2–8.
  10. Bejder Je.Ja., Petrova G.N., Izotova T.F., Gureeva E.V. Kompozicionnye termoplastichnye materialy i penopoliimidy [Composite thermoflexible materials and penopoliimidy] //Trudy VIAM. 2013. №11. St. 01 (viam-works.ru).
  11. Bejder Je.Ja., Petrova G.N., Malyshenok S.V. Kompozicionnye termoplastichnye materialy – svojstva i sposoby pererabotki [Composite thermoflexible materials – properties and ways of processing] //Plasticheskie massy. 2013. №7. S. 56–60.
  12. Petrova G.N., Bejder Je.Ja., Izotova T.F., Malyshenok S.V. Kompozicionnye termoplastichnye materialy – sposoby poluchenija i pererabotki [Composite thermoflexible materials – ways of receiving and processing] //Vse materialy. Jenciklopedi-cheskij spravochnik. 2013. №10. S. 10–17.
  13. Petrova G.N., Rumjanceva T.V., Bejder Je.Ja. Vlijanie modificirujushhih dobavok na pozharobezopasnye svojstva i tehnologichnost' polikarbonata [Influence of modifying additives on fireproof properties and technological effectiveness of polycarbonate] //Trudy VIAM. 2013. №6. St. 06 (viam-works.ru).
  14. Antjufeeva N.V., Aleksashin V.M., Stoljankov Ju.V. Sovremennoe metodicheskoe obespechenie termoanaliticheskih issledovanij polimernyh kompozitov i prepergov [Modern methodical ensuring thermoanalytical researches of polymeric composites and prepergov] //Kompozity i nanostruktury. 2014. T. 6. №3. S. 176–184.
  15. Stoljankov Ju.V., Ishodzhanova I.V., Antjufeeva N.V. K voprosu o defektah obrazcov dlja ispytanij ugleplastikov [To question of defects of test pieces ugleplastikov] //Trudy VIAM. 2014. №10. St. 10 (viam-works.ru).
  16. Ustrojstvo dlja mehanicheskoj obrabotki vspenennyh polimernyh materialovm [The device for machining of frothed polymeric materials]: pat. №145916 Ros. Federacija; opubl. 27.09.2014.