The method for adhesion strength determining of silver coating to the silicon substrate by glue applying
Lukin V.I., Rylnikov V.S., Afanasiev-Khodykin A.N., Kutsevich K.E., Nischev K.N. The method for adhesion strength determining of silver coating to the silicon substrate by glue applying // Proceedings of VIAM. 2015. No. 4. DOI: 10.18577/2307-6046-2015-0-4-12-12. URL: https://viam-works.ru/en/journal/2015/4/12
Abstract
The method of determining the adhesion strength of silver coating to the silicon substrate was developed for defining the quality of contact connections in semiconductor elements. It is shown hereby that the best option is to use high-adhesive membranous glue VK-51 and a special tooling with molybdenum heat compensators.
Reference list
- Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
- Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period till 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Petrova A.P., Lukina N.F. Klei dlja mnogorazovoj kosmicheskoj sistemy [Glues for reusable space system] //Trudy VIAM. 2013. №4. St. 04 (viam-works.ru).
- Petrova A.P., Donskoj A.A., Chalyh A.E., Shherbina A.A. Klejashhie materialy. Germetiki [Gluing materials. Hermetics]: Spravochnik. SPb.: Professional. 2008. 592 s.
- Petrova A.P. Klejashhie materialy [Gluing materials]: Spravochnik. M.: ZAO Redakcija zhurnala «Kauchuk i rezi-na». 2002. 196 s.
- Lukina N.F., Dement'eva L.A., Petrova A.P., Serezhenkov A.A. Konstrukcionnye i termostojkie klei [Constructional and heat-resistant glues] //Aviacionnye materialy i tehnologii. 2012. №S. S. 328–335.
- Kucevich K.E., Dement'eva L.A., Lukina N.F., Chursova L.V. Svojstva i naznachenie kleja VK-36RM dlja aviacionnoj tehniki [Properties and glue assignment R of aviation engineering] //Klei. Germetiki. Tehnologii. 2013. №8. S. 5–6.
- Dement'eva L.A., Lukina N.F., Serezhenkov A.A., Kucevich K.E. Osnovnye svojstva i nazna-chenie PKM na osnove kleevyh prepregov [The main properties and PKM assignment on the basis of glue prepregs] /V sb. tez. dokl. XIX Mezhdunarodnoj nauch.-tehn. konf. «Konstrukcii i tehnologii poluchenija izdelij iz nemetallicheskih materialov». Obninsk. 2010. S. 11–12.
- Dement'eva L.A., Serezhenkov A.A., Lukina N.F., Kucevich K.E. Kleevye prepregi i sloistye materialy na ih osnove [Glue prepregs and layered materials on their basis] //Aviacionnye materialy i tehnologii. 2013. №2. S. 19–21.
- Lukina N.F., Dement’eva L.A., Serezhenkov A.A. et al. Adhesive prepregs and composite matirials on their bases //Russian J. of General Chemistry. 2011. V. 81. №5. P. 1022–1024.
- Lukina N.F., Dement'eva L.A., Serezhenkov A.A. i dr. Kleevye prepregi i kompozicionnye materialy na ih osnove [Glue prepregs and composite materials on their basis] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 53–56.
- Dement'eva L.A., Serezhenkov A.A., Bocharova L.I. i dr. Svojstva kompozicionnyh materialov na osnove kleevyh prepregov [Properties of composite materials on the basis of glue prepregs] //Klei. Germetiki. Tehnologii. 2012. №6. S. 19–24.
- Kablov E.N., Antipov V.V., Senatorova O.G., Lukina N.F. Novyj klass sloistyh aljumostekloplastikov na osnove aljuminij-litievogo splava 1441 s ponizhennoj plotnost'ju [New class layered alyumostekloplastikov on basis aluminum-lithium alloy 1441 with lowered density] //Vestnik MGTU im. N.Je. Baumana. 2011. №SP2. S. 174–184.
- Kleevaja kompozicija [Glue composition]: pat. 2471842 Ros. Federacija; opubl. 11.05.2011.
- Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry in aviation materials science] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
- Antipov V.V., Senatorova O.G., Lukina N.F., Sidel'nikov V.V., Shestov V.V. Sloistye metallopolimernye kompozicionnye materialy [Layered metalpolymeric composite materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 226–230.
- Sharova I.A., Petrova A.P. Obzor po materialam Mezhdunarodnoj konferencii po klejam i germetikam (WAC-2012, Francija) [The overview on materials of the International conference on glues and hermetics (WAC-2012, France)] //Trudy VIAM. 2013. №8. St. 06 (viam-works.ru).
- Zhang Zhiye (Zach), Lu Guo-Quan. Pressure-Assisted Low-Temperatuze Sintering of Silver Paste as an Alternative Die-Attach Solution to Soldez Reflow //Trans. Jnd. Applicat. 2002. V. 25. №4. Р. 279–283.