Investigation of the potential application of polyesterurethane compound to protect the materials of aviation hardware parts

Karimova S.A., Avdushkina L.I., Efimova E.A., Nizamov Т.I., Aliyev A.A.
Karimova S.A., Avdushkina L.I., Efimova E.A., Nizamov Т.I., Aliyev A.A. Investigation of the potential application of polyesterurethane compound to protect the materials of aviation hardware parts // Proceedings of VIAM. 2015. No. 4. DOI: 10.18577/2307-6046-2015-0-4-10-10. URL: https://viam-works.ru/en/journal/2015/4/10
Abstract

In this work the anti-corrosion properties of polyesterurethane compound in conditions of high humidity (WKL-100) and the salt spray chamber (KCT-35) on samples of 30KhGSA steel and D16-T, 1163-AT and 1163-T aluminum alloys were determined. The results were compared with properties of well-known Cor Ban 35, PINS AT (TU38.401-58-120–95) and Dinitrol AV-40 protecting compounds. The fulfilled tests have shown high protective properties of pilot batch of PEUK compound for application in technological processes for enhanced parts and units protection in aviation hardware.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period till 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  3. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. II. Relaksacija ishodnoj strukturnoj neravnovesnosti i gradient svojstv po tolshhine [Climatic aging of composite materials of aviation assignment. II. Relaxation of initial structural non-equilibrium and gradient of properties on thickness] //Deformacija i razrushenie materialov. 2012. №6. S. 17–19.
  4. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. I. Mehanizmy starenija [Climatic aging of composite materials of aviation assignment. I. Aging mechanisms] //Deformacija i razrushenie materialov. 2010. №11. S. 19–27.
  5. Kablov E.N., Petrova A.P., Narskij A.R. G.V. Akimov – sozdatel' otechestvennoj nauki o kor-rozii [G.V. Akimov – the creator of domestic science about corrosion] //Istorija nauki i tehniki. 2009. №11. S. 12–15.
  6. Kirillov V.N., Starcev O.V., Efimov V.A. Klimaticheskaja stojkost' i povrezhdaemost' polimernyh kompozicionnyh materialov, problemy i puti reshenija [Climatic firmness and damageability of polymeric composite materials, problems and solutions] //Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.
  7. Kirillov V.N., Efimov V.A., Shvedkova A.K., Nikolaev E.V. Issledovanie vlijanija klimaticheskih faktorov i mehanicheskogo nagruzhenija na strukturu i mehanicheskie svojstva PKM [Research of influence of climatic factors and mechanical loading on structure and the PKM mechanical properties] //Aviacionnye materialy i tehnologii. 2011. №4. S. 41–45.
  8. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. III. Znachimye faktory starenija [Climatic aging of composite materials of aviation assignment. III. Significant factors of aging] //Deformacija i razrushenie materialov. 2011. №1. S. 34–40.
  9. Semenova L.V., Nefedov N.I. Pokrytija dlja zashhity gidroagregatov [Coverings for protection of hydraulic units] //Trudy VIAM. 2014. №2. St. 05. (viam-works.ru).
  10. Karimova S.A., Pavlovskaja T.G. Razrabotka sposobov zashhity ot korrozii konstrukcij, rabotajushhih v uslovijah kosmosa [Development of ways of corrosion protection of the designs working in the conditions of space] //Trudy VIAM. 2013. №4. St. 02. (viam-works.ru).
  11. Gui F., Furrow K., Williams J., Cooper K., Kelly R.G. Laboratory evaluations of corrosion prevention compounds for aircraft. Department of Materials Science and Engineering, University of Virginia. 2002.
  12. Craig B.D., Lane R.A., Rose D.H. Corrosion Prevention and Control: A Program Man-agement Guide for Selecting Materials //Advanced Materials, Manufacturing and Testing Information Analysis Center. 2006. P. 75–82.
  13. Zalivochnyj kompaund [Filling compound]: pat. №2006022 Ros. Federacija; opubl. 05.01.2004.
  14. Nizamov T.I. Osobennosti proektirovanija antenny gidrolokatora dlja morskogo monitoringa [Features of design of the aerial of the sonar for sea monitoring] //Izvestija NAN Azerbajdzhana. Ser. «Fiziko-matematicheskie i tehnicheskie nauki». 2003. №5(II). S. 184–190.
  15. Topliva, smazochnye materialy, tehnicheskie zhidkosti. Assortiment. Primenenie [Fuels, lubricants, technical liquids. Range. Application]: Spravochnik /Pod red. V.M. Shkol'nikova. 2-e izd. M.: Tehinform. 1999. S. 384, 386.
  16. GOST 9.054–80 Edinaja sistema zashhity ot korrozii i starenija. Materialy konservacion-nye. Masla, smazki i neftjanye ingibirovannye tonkoplenochnye pokrytija. Metody uskorennyh ispytanij zashhitnyh svojstv [Uniform system of corrosion protection and aging. Materials konservatsionny. Oils, lubricant and oil inhibited thin-film coverings. Methods of accelerated tests of protective properties].
  17. Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Aljuminievye deformiruemye splavy [Aluminum deformable alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 167–182.
  18. Zhilikov V.P., Karimova S.A., Leshko S.S., Chesnokov D.V. Issledovanie dinamiki korrozii aljuminievyh splavov pri ispytanii v kamere solevogo tumana (KST) [Research of dynamics of corrosion of aluminum alloys when testing in the salt spray chamber (KST)] //Aviacionnye materialy i tehnologii. 2012. №4. S. 18–22.
  19. Kurs M.G., Karimova S.A. Naturno-uskorennye ispytanija: osobennosti metodiki i sposoby ocenki korrozionnyh harakteristik aljuminievyh splavov [Natural accelerated tests: features of technique and ways of assessment of corrosion characteristics of aluminum alloys] //Aviacionnye materialy i tehnologii. 2014. №1. S. 51–57.