Application of model solutions for ICP-AES procedures

Zagvozdkina T.N., Karachevtsev F.N., Dvoretskov R.M.
Zagvozdkina T.N., Karachevtsev F.N., Dvoretskov R.M. Application of model solutions for ICP-AES procedures // Proceedings of VIAM. 2015. No. 3. DOI: 10.18577/2307-6046-2015-0-3-10-10. URL: https://viam-works.ru/en/journal/2015/3/10
Abstract

Narrowing of the alloying limits is a current trend in the development of new alloys. In order to determine the exact chemical composition of the alloys under development, it is necessary to use an analyzing procedure, which provides the relative error at least three times lower than the alloying limits. The error value is within 1,5 to 2,5% (rel.) range for the majority of alloying elements. Application of model solutions for atomic absorption analysis to reduce measurement errors of alloying elements and impurities was described in the paper. The use of model solutions as reference samples allowed to reduce the error of measurement techniques down to 1% (rel.).

Reference list
  1. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokolenija [Casting nickel superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36–52.
  2. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharoprochnye nikelevye splavy dlja detalej gazoturbinnyh dvigatelej [High-temperature heat-resistant nickel alloys for turbine engines parts] //Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
  3. Lomberg B.S., Ovsepjan S.V., Bakradze M.M. Osobennosti legirovanija i termicheskoj obrabotki zharoprochnyh nikelevyh splavov dlja diskov gazoturbinnyh dvigatelej novogo pokolenija [Features alloying and heat treatment of heat-resistant nickel alloys for disks of gas turbine engines of the new generation] //Aviacionnye materialy i tehnologii. 2010. №2. S. 3–8.
  4. Lomberg B.S., Ovsepjan S.V., Bakradze M.M. Novyj zharoprochnyj nikelevyj splav dlja diskov gazoturbinnyh dvigatelej (GTD) i gazoturbinnyh ustanovok (GTU) [New heat-resistant nickel alloy disks of gas turbine engines (GTE) and gas turbines (GT)] //Materialovedenie. 2010. №7. S. 24–28.
  5. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Litejnye zharoprochnye nikelevye splavy dlja perspektivnyh aviacionnyh GTD [Casting nickel superalloys for advanced gas turbine engines] //Tehnologija legkih splavov. 2007. №2. S. 6–16.
  6. Lomberg B.S., Bakradze M.M., Chabina E.B., Filonova E.V. Vzaimosvjaz' struktury i svojstv vysokozharoprochnyh nikelevyh splavov dlja diskov gazoturbinnyh dvigatelej [Relationship between structure and properties of nickel-base superalloys for gas turbine engine disks] //Aviacionnye materialy i tehnologii. 2011. №2. S. 25–30.
  7. Chabina E.B., Filonova E.V., Lomberg B.S., Bakradze M.M. Struktura sovremennyh deformiruemyh nikelevyh splavov [The structure of modern wrought nickel alloys] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №6. S. 22–27.
  8. Petrushin N.V., Eljutin E.S., Chabina E.B., Timofeeva O.B. O fazovyh i strukturnyh prevrashhenijah v zharoprochnyh renijsoderzhashhih splavah monokristallicheskogo stroenija [Phase and structural transformations in the heat-resistant alloys rhenium single crystal structure] //Litejnoe proizvodstvo. 2008. №7. S. 1–7.
  9. Petrushin N.V., Svetlov I.L., Samojlov A.P. i dr. Vysokotemperaturnye fazovye i strukturnye prevrashhenija v monokristallah zharoprochnogo nikelevogo splava, soderzhashhego renij i rutenij [High-temperature phase and structural transformations in single heat-resistant nickel alloy containing rhenium and ruthenium] //Materialovedenie. 2008. №11. S. 26–31.
  10. Pupyshev A.A. Atomno-absorbcionnyj spektral'nyj analiz [Atomic absorption spectral analysis]. M.: Tehnosfera. 2009. 784 s.
  11. Tormysheva E.A., Smirnova E.V., Ermolaeva T.N. Mikrovolnovaja probopodgotovka naplavochnyh materialov dlja analiza metodom atomno-jemissionnoj spektroskopii s induktivno svjazannoj plazmoj [Microwave Sample Preparation surfacing materials for analysis by atomic emission spectroscopy with inductively coupled plasma] //Zavodskaja laboratorija. Diagnostika materialov. 2010. T. 76. №10. S. 10–13.
  12. Kablov E.N., Morozov G.A., Krutikov V.N., Muravskaja N.P. Attestacija standartnyh obrazcov sostava slozhnolegirovannyh splavov s primeneniem jetalona [Certification of standard samples of complex alloys using standard] //Aviacionnye materialy i tehnologii. 2012. №2. S. 9–11.
  13. Letov A.F., Karachevcev F.N., Gundobin N.V., Titov V.I. Razrabotka standartnyh obrazcov sostava splavov aviacionnogo naznachenija [Development of standard samples of alloys aviation applications] //Aviacionnye materialy i tehnologii. 2012. №S. S. 393–398.