Determination of gallium, germanium, arsenic and selenium contents in heat-resistant nickel alloys microalloyed by REM using ICP-MS

Yakimovitch P.V., Alekseev A.V.
Yakimovitch P.V., Alekseev A.V. Determination of gallium, germanium, arsenic and selenium contents in heat-resistant nickel alloys microalloyed by REM using ICP-MS // Proceedings of VIAM. 2015. No. 3. DOI: 10.18577/2307-6046-2015-0-3-9-9. URL: https://viam-works.ru/en/journal/2015/3/9
Abstract

Heat-resistant nickel alloys are widely applied in the modern aviation industry and engine building. Some critical components subjected to huge thermal and power loadings are made of them. Thus, an important task is to control chemical composition of nickel-based alloys, in particular the content of trace constituents, which include gallium, germanium, arsenic and selenium. Gallium, germanium, arsenic and selenium content in certified reference samples of nickel alloys microalloyed by REM was determined using mass spectrometry with inductively coupled plasma (ICP-MS). The method of dissolution of a sample and its preparation for analysis was described. Spectral interferences were eliminated using the equations of mathematical correction. The detection limits (% mass.) were as follows: Ga – 0,000002, Ge – 0,000002, Se – 0,00003, As – 0,00004. The range of the defined concentrations was 0,000009–0,0023% mass., the relative standard deviation of not higher than 0,05.

Reference list
  1. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of current and future high-tech] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  2. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokolenija [Casting nickel superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36–52.
  4. Kablov E.N., Petrushin N.V., Vasilenok L.B., Morozova G.I. Renij v zharoprochnyh nikelevyh splavah dlja lopatok gazovyh turbin (prodolzhenie) [Rhenium in nickel superalloys for gas turbine blades (continued)] //Materialovedenie. 2000. №3. S. 38–43.
  5. Kablov E.N., Logunov A.V., Sidorov V.V. Mikrolegirovanie RZM – sovremennaja tehnologija povyshenija svojstv litejnyh zharoprochnyh nikelevyh splavov [Microalloying REM - modern technology improve the properties of heat-resistant nickel alloys casting] //Perspektivnye materialy. 2001. №1. S. 23–34.
  6. Kablov E.N. Fiziko-mehanicheskie i tehnologicheskie osobennosti sozdanija zharoprochnyh splavov, soderzhashhih renij [Physical, mechanical and technological features of the creation of high-temperature alloys containing rhenium] //Vestnik Moskovskogo universiteta. Ser. 2. Himija. 2005. T. 46. №3. S. 155–167.
  7. Kablov E.N., Buntushkin V.P., Povarova K.B., Bazyleva O.A., Morozova G.I., Kazanskaja N.K. Malolegirovannye legkie zharoprochnye vysokotemperaturnye materialy na osnove intermetallida Ni3Al [Low-alloy high-temperature heat-resistant lightweight materials based on the intermetallic compound Ni3Al] //Metally. 1999. №1. S. 58–65.
  8. Lomberg B.S., Ovsepjan S.V., Bakradze M.M. Osobennosti legirovanija i termicheskoj obrabotki zharoprochnyh nikelevyh splavov dlja diskov gazoturbinnyh dvigatelej novogo pokolenija [Features alloying and heat treatment of heat-resistant nickel alloys for disks of gas turbine engines of the new generation] //Aviacionnye materialy i tehnologii. 2010. №2. S. 3‒8.
  9. Sidorov V.V., Timofeeva O.B., Kalicev V.A., Gorjunov A.V. Vlijanie mikrolegirovanija RZM na svojstva i strukturno-fazovye prevrashhenija v intermetallidnom splave VKNA-25-VI [Effect of microalloying REM on the properties and structural phase transformations in intermetallic alloys VKNA-25-VI] //Aviacionnye materialy i tehnologii. 2012. №4. S. 8‒13.
  10. Min P.G., Sidorov V.V. Rafinirovanie othodov zharoprochnogo nikelevogo splava ZhS32-VI ot primesi kremnija v uslovijah vakuumnoj indukcionnoj plavki [Refining of nickel superalloys ZHS32-VI of silicon impurities in a vacuum induction melting] //Trudy VIAM. 2014. №9. St. 01 (viam-works.ru).
  11. GOST 11739.26–90. Splavy aljuminievye litejnye i deformiruemye. Metody opredelenija gallija [Aluminum casting alloys and wrought. Methods for determination of gallium].
  12. Mirzoyan F.V., Tarayan V.M., Hairyan E.K. Sensitive spectrophotometric determination of germanium as methylene blue 12-molybdogermanate //Analytica Chimica Acta. 1981. V. 124. P. 185–192.
  13. GOST 6689.13–92. Nikel', splavy nikelevye i medno-nikelevye. Metody opredelenija mysh'jaka [Nickel, nickel and copper-nickel. Methods for determination of arsenic].
  14. GOST 13047.25–2002. Nikel'. Kobal't. Metody opredelenija selena v nikele [Nickel. Cobalt. Methods for determination of selenium in nickel].
  15. Hu J., Wang H. Determination of Trace Elements in Super Alloy by ICP-MS //Mikrochim. Acta. 2001. V. 137. P. 149–155.
  16. Pupyshev A.A., Jepova E.N. Spektral'nye pomehi poliatomnyh ionov v metode mass-spektrometrii s induktivno-svjazannoj plazmoj [Spectral interference polyatomic ions in mass spectrometry with inductively coupled plasma] //Analitika i kontrol'. 2001. T. 5. №4. S. 335–369.
  17. Lejkin A.Ju., Jakimovich P.V. Sistemy podavlenija spektral'nyh interferencij v mass-spektrometrii s induktivno-svjazannoj plazmoj [Spectral interferences suppression system in mass-spectrometry with inductively coupled plasma] //Zhurnal analiticheskoj himii. 2012. T. 67. №8. S. 752–762.
  18. Gao Y., Liu R. at al. Application of chemical vapor generation in ICP-MS: A review //Chin Sci Bull. 2013. V. 58. P. 1980–1991.
  19. Nie X., Liang Y. Determination of trace elements in high purity nickel by high resolution inductively coupled plasma mass spectrometry //J. Cent. South Univ. 2012. V. 19. P. 2416−2420.
  20. Jakubenko E.V., Vojtkova Z.A., Chernikova I.I., Ermolaeva T.N. Mikrovolnovaja probopodgotovka dlja opredelenija Si, P, V, Cr, Mn, Ni, Cu, W metodom AJeS-ISP v konstrukcionnyh staljah [Microwave sample preparation for determination of Si, P, V, Cr, Mn, Ni, Cu, W ICP-AES method for structural steels] //Zavodskaja laboratorija. Diagnostika materialov. 2014. T. 80. №1. S. 12–15.
  21. Dvoreckov R.M., Karachevcev F.N., Zagvozdkina T.N., Mehanik E.A. Opredelenie legirujushhih jelementov nikelevyh splavov aviacionnogo naznachenija metodom AJeS-ISP v sochetanii s mikrovolnovoj probopodgotovkoj [Determination of alloying elements nickel alloys aviation applications by ICP-AES combined with microwave sample preparation] //Zavodskaja laboratorija. Diagnostika materialov. 2013. T. 79. №9. S. 6–9.
  22. MI 1.2.052–2013. Metodika izmerenij massovoj doli primesej R, Mn, Fe, Cu, Zn, Ga, As, Se, Ag, Cd, Sn, Sb, Te, Tl, Pb, Bi v nikelevyh splavah metodom mass-spektrometrii s induktivno svjazannoj plazmoj [Method for determination of mass fraction of impurities P, Mn, Fe, Cu, Zn, Ga, As, Se, Ag, Cd, Sn, Sb, Te, Tl, Pb, Bi in nickel alloys by mass spectrometry with inductively coupled plasma]. M.: VIAM. 2013.