Technological plasticity, structure and phase composition of a pilot titanium ortho alloy with 13 wt. рct. aluminum

Alexeev E.B., Nochovnaya N.A., Panin P.V., Novak A.V.
Alexeev E.B., Nochovnaya N.A., Panin P.V., Novak A.V. Technological plasticity, structure and phase composition of a pilot titanium ortho alloy with 13 wt. рct. aluminum // Proceedings of VIAM. 2015. No. 12. DOI: 10.18577/2307-6046-2015-0-12-8-8. URL: https://viam-works.ru/en/journal/2015/12/8
Keywords
high-temperature titanium ortho alloy, isothermal deformation, acceptable limit of deformation amount, hot pressure treatment, phase transformations, phase composition, ordered phases, microstructure.
Abstract

The article presents research results on technological parameters of deformation, structure and phase composition of a pilot intermetallic ortho alloy Ti–13Al–40Nb–5(Zr+V+Mo+W)–0,5(Si+C) determination. It has been resolved that no strain strengthening effect throughout hot working process is observed at a temperature of 1000°С. Temperature intervals of the following phase areas have been determined for the pilot alloy: (О+βA2)→(О+β(A2+В2)+α2)→(β(A2+В2)+α2)→β(A2+В2). Also it has been shown that technological plasticity (degree of strain) decrease at deformation temperatures lower than 1000°С and prolonged duration is caused by phase transformations: in these conditions decomposition of β-phase takes place together with the ordered intermetallic O- and α2-phases precipitation.

Reference list
  1. Nochovnaya N.A., Antashev V.G., Shiryaev A.A., Alekseev E.B. Issledovanie vliyaniya rezhimov izotermicheskogo deformirovaniya i termicheskoj obrabotki na strukturu i mehanicheskie svojstva opytnogo zharoprochnogo Ti-splava [Research of influence of modes of isothermal deformation and thermal processing on structure and mechanical properties of pilot heat resisting Ti-alloy] //Tehnologija legkih splavov. 2012. №4. S. 92–98.
  2. Nochovnaya N.A., Shiryaev A.A., Alekseev E.B., Antashev V.G. Optimizaciya rezhimov termicheskoj obrabotki dlya lopatochnyh zagotovok iz opytnogo zharoprochnogo titanovogo splava [Optimization of modes of thermal processing for scapular preparations from experimental heat resisting titanium alloy] //MiTOM. 2014. №12 (714). S. 22–26.
  3. Nochovnaya N.A., Alekseev E.B., Izotova A.Yu., Novak A.V. Pozharobezopasnye titanovye splavy i osobennosti ih primeneniya [Fireproof titanium alloys and features of their application] //Titan. 2012. №4 (38). S. 42–46.
  4. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  5. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  6. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] //Nauka i zhizn. 2010. №4. S. 2–7.
  7. Tarasov Yu.M., Antipov V.V. Novye materialy VIAM – dlya perspektivnoj aviacionnoj tehkniki proizvodstva OAO «OAK» [The VIAM new materials – for perspective aviation engineering of production of JSC «OAK»] //Aviacionnye materialy i tehnologii. 2012. №2. S. 5–6.
  8. Kashapov O.S., Novak A.V., Nochovnaya N.A., Pavlova T.V. Sostoyanie, problemy i perspektivy sozdaniya zharoprochnyh titanovyh splavov dlya detalej GTD [Condition, problems and perspectives of creation of heat resisting titanium alloys for GTE details] //Trudy VIAM. 2013. №3. St. 02 (viam-works.ru).
  9. Nochovnaya N.A., Ivanov V.I., Alekseev E.B., Kochetkov A.S. Puti optimizacii ekspluatacionnyh svojstv splavov na osnove intermetallidov titana [Ways of optimization of operational properties of alloys on the basis of titanium intermetallic compound] //Aviacionnye materialy i tehnologii. 2012. №S. S. 196–206.
  10. Nochovnaya N.A., Panin P.V., Kochetkov A.S., Bokov K.A. Sovremennye zharoprochnye splavy na osnove gamma-alyuminida titana: perspektivy razrabotki i primeneniya [Modern hot strength alloys on the basis of titanium gamma aluminide: development and application perspectives] //MiTOM. 2014. №7. S. 23–27.
  11. Nochovnaya N.A., Skvortsova S.V., Anishchuk D.S., Alekseev E.B., Panin P.V., Umarova O.Z. Otrabotka tehnologii opytnogo zharoprochnogo splava na osnove intermetallida Ti2AlNb [Working off of technology of pilot hot strength alloy on the basis of Ti2AlNb intermetallic compound] //Titan. 2013. №4 (42). S. 33–38.
  12. Nochovnaya N.A., Alekseev E.B., Yasinskij K.K., Kochetkov A.S. Specifika plavki i sposoby polucheniya slitkov intermetallidnyh titanovyh splavov s povyshennym soderzhaniem niobiya [Specifics of melting and ways of receiving ingots of intermetallic titanium alloys with the raised content of niobium] //Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. №SP2. C. 53–59.
  13. Kablov D.E., Panin P.V., Shiryaev A.A., Nochovnaya N.A. Opyt ispolzovaniya vakuumno-dugovoj pechi ALD VAR L200 dlya vyplavki slitkov zharoprochnyh splavov na osnove aljuminidov titana [The use of ADL VAR L200 vacuum-arc furnace for ingots fabrication of high-temperature titanium aluminides base alloys] //Aviacionnye materialy i tehnologii. 2014. №2. S. 27–33.
  14. Alekseev E.B., Nochovnaja N.A., Skvorcova S.V., Grushin I.A., Agarkova E.O. Vliyanie termicheskoj obrabotki na strukturno-fazovyj sostav i mehanicheskie svojstva titanovogo splava na osnove orto-fazy [Influence of thermal processing on structural and phase structure and mechanical properties of titanium alloy on the basis of orto-phase] //Titan. 2014. №4 (46). S. 45–49.
  15. Nochovnaya N., Ivanov V., Alexeev E., Izotova A. Opportunities of increase of mechanical properties of the deformed semi-finished products from Ti–Al–Nb system alloys /Proc. 12-th World Conf. on Titanium (Ti–2011). Beijing. 2011. V. 2. P. 1383–1386.
  16. Panin P., Nochovnaya N., Alexeev E., Kablov D. On the problem of low-temperature ductility improvement of Ti–Al and Ti–Al–Nb based alloys /Proc. Int. Symposium on Gamma TiAl Alloys (ISGTA’14). San Diego. 2014 (CD).
  17. Alekseev E.B., Nochovnaya N.A., Panin P.V. Issledovanie struktury i fazovogo sostava opytnogo zharoprochnogo splava na osnove intermetallida Ti2AlNb v deformirovannom sostoyanii [Research of structure and phase composition of pilot hot strength alloy on the basis of Ti2AlNb intermetallic compound in the deformed condition] //Titan. 2014. №4 (46). S. 12–17.
  18. Alekseev E.B., Nochovnaya N.A., Ivanov V.I., Panin P.V., Novak A.V. Issledovanie vliyaniya alyuminiya na fazovyj sostav i svojstva deformirovannyh polufabrikatov iz intermetallidnogo titanovogo splava VTI-4 [Research of influence of aluminum on phase structure and properties of the deformed semi-finished products from intermetallic VTI-4 titanium alloy] //Tehnologiya legkih splavov. 2015. №1. S. 57–61.
  19. Alekseev E.B., Nochovnaja N.A., Skvortsova S.V., Panin P.V., Umarova O.Z. Opredelenie tehnologicheskih parametrov deformacii opytnogo zharoprochnogo splava na osnove intermetallida Ti2AlNb [Determination of technological parameters of deformation of pilot hot strength alloy on the basis of Ti2AlNb intermetallic compound] //Titan. 2014. №2 (44). S. 36–41.
  20. Splav na osnove titana i izdelie, vypolnennoe iz nego [Titanium-based alloy and the product which has been executed of it]: pat. 2210612 Ros. Federatsiya; opubl. 20.08.2003.
  21. Kazantseva N.V., Lepihin S.V. Issledovanie diagrammy sostoyaniya Ti–Al–Nb [Research of the chart of condition of Ti–Al–Nb] //Fizika metallov i metallovedenie. 2006. T. 102. №2. S. 184–195.
  22. Demakov S.L., Stepanov L.S., Popov A.A. Fazovye prevrashheniya v super-α2-titanovom splave. I. Vliyanie temperatury i vremeni vyderzhki pod zakalku na fazovyj sostav i strukturu splava [Phase transformations in super-α2-titanium alloy. I. Temperature and hold time influence under tempering on phase structure and alloy structure] //Fizika metallov i metallovedenie. 1998. T. 86. №5. S. 115–122.