Study of microstructure of magnesium-zirconium master alloy and heat-resistant magnesium alloy ML10

Uridiya Z.P., Mukhina I.Y., Frolov A.V., Leonov A.A.
Uridiya Z.P., Mukhina I.Y., Frolov A.V., Leonov A.A. Study of microstructure of magnesium-zirconium master alloy and heat-resistant magnesium alloy ML10 // Proceedings of VIAM. 2015. No. 10. DOI: 10.18577/2307-6046-2015-0-10-6-6. URL: https://viam-works.ru/en/journal/2015/10/6
Abstract

This article presents the research of microstructure of magnesium-zirconium and ML10 alloys. It is hard to alloy magnesium with elements for which the fusing temperature is higher than that of magnesium’s. The impurity doping of magnesium alloy with zirconium is processed through the magnesium-zirconium alloy, for which the fusing temperature is lower than the fusing temperature for zirconium. The impurity doping of light materials with zirconium is problematic not only because of the high fusing temperature of zirconium, but also because of its active liaison with other elements such as hydrogen, oxygen, nitrogen, aluminum, ferrum, silicon, carbon and other elements. The quality of alloy has been examined and the reasons of lower drawing of zirconium in the process of making ML10 magnesium alloy had been defined: it is linked with the fact that there are non-soluble intermetallides in the alloy such as zirconium and hafnium with silicon, ferrum and aluminum, and zirconium with oxygen

Reference list
  1. Kornysheva I.S., Volkova E.F., Goncharenko E.S., Muhina I.Ju. Perspektivy primenenija magnievyh i litejnyh aljuminievyh splavov [Perspectives of application of magnesium and cast aluminum alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 212–222.
  2. Kablov E.N. Osnovnye itogi i napravlenija razvitija materialov dlja perspektivnoj aviacionnoj tehniki [The main results and the directions of development of materials for perspective aviation engineering] /V sb. 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: Jubilejnyj nauch.-tehnich. sb. M.: VIAM. 2007. S. 20–26.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  4. Kablov E.N. VIAM: prodolzhenie puti [VIAM: way continuation] //Nauka v Rossii. 2012. №3. S. 36–44.
  5. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  6. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry in aviation materials science] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  7. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  8. Korchagina V.A. Radi kachestva magnievyh otlivok [For the sake of quality of magnesian otlivka] //Inzhenernaja gazeta. 2006. №33–34. S. 5.
  9. Sadkov V.V., Laponov Ju.L., Ageev A.P. i dr. Perspektivy i uslovija primenenija magnievyh splavov v samoletah OAO «Tupolev» [Perspectives and conditions of application of magnesium alloys in JSC Tupolev airplanes] //Metallurgija mashinostroenija. 2007. №4. S. 19–23.
  10. Antipov V.V., Vahromov R.O., Dujunova V.A., Nochovnaja N.A. Materialy s vysokoj udel'noj prochnost'ju na osnove aljuminija, magnija, titana i tehnologii ih pererabotki [Materials with high specific strength on the basis of aluminum, magnesium, titanium and technology of their processing] //Boepripasy i spechimija. 2013. №3. S. 51–55.
  11. Muhina I.Ju., Uridija Z.P. Magnij – osnova sverhlegkih materialov [Magnesium – basis of extralight materials] //Metallurgija mashinostroenija. 2005. №6. S. 29–31.
  12. Dujunova V.A. Metody zashhity magnievyh splavov v otechestvennom litejnom proizvodstve s 1930-h gg. do nastojashhego vremeni [Methods of protection of magnesium alloys in domestic foundry production since the 1930th so far] //Litejshhik Rossii. 2010. №10. S. 35–37.
  13. Dujunova V.A., Muhina I.Ju., Uridija Z.P. Novye protivoprigarnye prisadochnye materialy dlja litejnyh form magnievyh otlivok [New protivoprigarny prisadochny materials for casting molds of magnesian otlivka] //Litejnoe proizvodstvo. 2009. №9. S. 18–21.
  14. Muhina I.Ju., Dujunova V.A., Uridija Z.P. Perspektivnye litejnye magnievye splavy [Perspective cast magnesium alloys] //Litejnoe proizvodstvo. 2013. №5. S. 2–5.
  15. Dujunova V.A., Goncharenko N.S., Muhina I.Ju., Uridija Z.P., Volkova E.F. Nauchnoe nasledie akademika I.N. Fridljandera. Sovremennye issledovanija magnievyh i litejnyh aljuminievyh splavov v VIAM [Scientific heritage of academician I.N. Fridlyandera. Modern researches of magnesium and cast aluminum alloys in VIAM] //Cvetnye metally. 2013. №9. S. 71–78.
  16. Frolov A.V., Muhina I.Ju., Dujunova V.A., Uridija Z.P. Vlijanie tehnologicheskih parametrov plavki na strukturu i svojstva novyh magnievyh splavov [Influence of technological parameters of melting on structure and property of new magnesium alloys] //Metallurgija mashinostroenija. 2014. №2. S. 26–29.
  17. Muhina I.Ju. Litejnye splavy i tehprocessy pri proizvodstve magnievyh otlivok [Cast alloys and technical processes by production of magnesian otlivka] //Litejnoe proizvodstvo. 2003. №4. S. 18–19.
  18. Goncharenko E.S., Trapeznikov A.V., Ogorodov D.V. Litejnye aljuminievye splavy (k 100-letiju so dnja rozhdenija M.B. Al'tmana) [Cast aluminum alloys (to the 100 anniversary since the birth of M. B. Altman)] //Trudy VIAM. 2014. №4. St. 02 (viam-works.ru).
  19. Al'tman M.B. i dr. Magnievye splavy. Spravochnik [Magnesium alloys. Directory]. M.: Metallurgija. 1978. T. 2. 147 s.
  20. Uridija Z.P., Muhina I.Ju., Dujunova V.A., Kosarina E.I. Kontrol' kachestva lit'ja iz magnievyh splavov i sposoby vosstanovlenija germetichnosti otlivok [Molding quality control from magnesium alloys and ways of recovery of tightness of otlivka] //Trudy VIAM. 2014. №12. St. 04 (viam-works.ru).
  21. Leonov A.A., Dujunova V.A., Stupak E.V., Trofimov N.V. Lit'e magnievyh splavov v razovye formy, poluchennye novymi metodami [Molding of magnesium alloys in the one-time forms received by new methods] //Trudy VIAM. 2014. №12. St. 01 (viam-works.ru).
  22. Shishkareva L.M., Kuz'mina N.A. Obzor metodik opredelenija kachestva struktury monokristallicheskih otlivok zharoprochnyh splavov [Review of techniques of determination of quality of structure of single-crystal otlivka of hot strength alloys] //Trudy VIAM. 2014. №1. St. 06 (viam-works.ru).
  23. Postnov V.I., Burhan O.L., Rahmatullin A.Je., Kachura S.M. Nerazrushajushhie metody kontrolja soderzhanija svjazujushhih v prepregah i PKM (obzor) [Nondestructive control methods of the contents binding in prepregs and PKM (review)] //Trudy VIAM. 2013. №12. St. 06 (viam-works.ru).
  24. Murashov V.V. Nerazrushajushhij kontrol' zagotovok i detalej iz uglerod-uglerodnogo kompozicionnogo materiala dlja mnogorazovogo kosmicheskogo korablja «Buran» [Non-destructive testing of preparations and details from carbon-carbon composite material for the reusable «Buran» spacecraft] //Trudy VIAM. 2013. №4. St. 06 (viam-works.ru).
  25. OST1 90427–94. Kachestvo produkcii. Nerazrushajushhij kontrol' lityh detalej i polufabrikatov aviacionnoj tehniki iz aljuminievyh i magnievyh splavov radiograficheskim metodom. Obshhie polozhenija [Quality of products. Non-destructive testing of cast details and semi-finished products of aviation engineering from aluminum and magnesium alloys radiographic method. General provisions].
  26. PI1.2.226–2008. Nerazrushajushhij kontrol' (NK) metallicheskih izdelij rentgenovskimi metodami [Non-destructive testing (Tax Code) of metal products by x-ray methods].
  27. OST1 90121–90. Magnievye litejnye splavy. Rezhimy termicheskoj obrabotki [Magnesium cast alloys. Modes of thermal processing].
  28. OST1 90248–77. Otlivki fasonnye iz magnievyh splavov. Obshhie tehnicheskie trebovanija [Casting shaped from magnesium alloys. General technical requirements].