Anodic oxide coating – protection of titanium alloys against hot salt corrosion

Zakharova L.V.
Zakharova L.V. Anodic oxide coating – protection of titanium alloys against hot salt corrosion // Proceedings of VIAM. 2015. No. 10. DOI: 10.18577/2307-6046-2015-0-10-2-2. URL: https://viam-works.ru/en/journal/2015/10/2
Abstract

Titanium alloys are widely applied in products of aviation engineering operating during long term in all climates including sea climate conditions, where deposition of sea salt on their surface can cause hot salt corrosion at elevated temperatures (≥250°C) accompanied with titanium surface embrittlement. Taking into account the potential danger of hot salt corrosion for high-loaded parts from titanium alloys operating in sea climate conditions at temperatures ≥250°C, the opportunity of identifying of coatings able to protect such parts from the influence of salt deposits seems to be of interest. This paper shows the possibility of protection of the surface of titanium alloys by anodic oxide coating of 10–15 μm in thickness against the impact of NaCl deposits (the main component of sea salt) at temperatures under 500°C, tensile stress and alternating loads.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1. S. 3–33.
  2. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  3. Kablov E.N. Materialy dlja izdelija «Buran» – innovacionnye reshenija formirovanija shestogo tehnologicheskogo uklada [Materials for the product «Buran» – innovative solutions of forming of the sixth technological way] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  4. Horev A.I. Fundamental'nye i prikladnye raboty po titanovym splavam dlja «Burana» i perspektivnye napravlenija ih razvitija [Fundamental and applied works on titanium alloys for «Buran» and the perspective directions of their development] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 10–14.
  5. Kashapov O.S., Novak A.V., Nochovnaja N.A., Pavlova T.V. Sostojanie, problemy i perspektivy sozdanija zharoprochnyh titanovyh splavov dlja detalej GTD [Condition, problems and perspectives of creation of heat resisting titanium alloys for GTD details] //Trudy VIAM. 2013. №3. St. 02 (viam-works.ru).
  6. Horev A.I. Fundamental'nye i prikladnye raboty po konstrukcionnym titanovym splavam i perspektivnye napravlenija ih razvitija [Fundamental and applied works on structural titanium alloys and perspective directions of their development] //Trudy VIAM. 2013. №2. St. 04 (viam-works.ru).
  7. Solonina O.P., Glazunov S.G. Titanovye splavy. Zharoprochnye titanovye splavy [Titanium alloys. Heat resisting titanium alloys]. M.: Metallurgija. 1976. 448 s.
  8. Kolachev B.A., Livanov V.A., Buhanova A.A. Mehanicheskie svojstva titana i ego splavov [Mechanical properties of titanium and its alloys]. M.: Metallurgija. 1974, 543 s.
  9. Gorynin I.V., Ushakov S.S., Hatuncev A.N., Loshakova I.L. Titanovye splavy dlja morskoj tehniki [Titanium alloys for sea equipment]. SPb.: Politehnika. 2007. 387 s.
  10. Sinjavskij S.V. Soprotivlenie titanovyh splavov razlichnym vidam korrozionnogo rastreskivanija [Resistance of titanium alloys to different types of corrosion cracking] //Tehnologija legkih splavov. 2010. №4. S. 80–85.
  11. Li S.Q., Lei J.F., Liu Y.-Y., Yu B.-X., Li Y.-L., Yang R. Fushi Kexue yu Fandhu Jishu. Hot-salt stress corrosion of titanium alloys of Ti811 and TC4 //Corros. Sci. And Prol. Tehnol. 2010. V. 22. №2. P. 79–84.
  12. Xiong Y., Zhu S., Wang F. Synergistic corrosion behavior of coated Ti60 alloys with NaCl deposit in moist air at elevated temperature //Corros. Sci. 2008. V. 50. P. 15–22.
  13. Ulrich Zwicker. Titan und Titanlegierungen. Springer-Verlag Berlin. Heidelberg. New York. 1974. 512 с.
  14. Bacos M.-P., Thomas M., Raviart J.-L., Morel A., Mercier S., Josso P. Influence of an oxidation protective coating upon hot corrosion and mechanical behavior of Ti–48Al–2Cr–2Nb alloy //Intermetallics. 2011. V. 19. №8. P. 1120–1129.
  15. Yingun Hua, Yuchuan Bai, Yunxia Ye, Qing Xue, Haixie Liu, Ruifang Chen, Kangmin Chen. Hot corrosion behavior of TC11 titanium alloy treated by laser shock processing //Applied Surface Science. 2013. V. 283. №15. P. 775–780.
  16. Zaharova L.V. Vlijanie kisloroda vozduha i tolshhiny solevyh otlozhenij na korrozionnoe rastreskivanie titanovyh splavov pri vysokih temperaturah v kontakte s NaCl [Influence of oxygen of air and thickness of salt deposits on corrosion cracking of titanium alloys at high temperatures in contact with NaCl] //Trudy VIAM. 2014. №10. St. 12 (viam-works.ru).