Abradable sealing material made of fibers from copper alloys

Migunov V.P., Farafonov D.P., Degovets M.L.
Migunov V.P., Farafonov D.P., Degovets M.L. Abradable sealing material made of fibers from copper alloys // Proceedings of VIAM. 2014. No. 9. DOI: 10.18577/2307-6046-2014-0-9-4-4. URL: https://viam-works.ru/en/journal/2014/9/4
Abstract

Possibility of creation of abradable sealing material from metal fibers with high op-erational properties, workable in GTE compressor with blades and stator parts made of titanium alloys was investigated. Usage of discrete fibers from copper alloys as an initial material for abradable seals of radial gap in compressor has been offered.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Vinogradov A.S., Badykov R.R., Shpakov I.D. Issledovanie germetichnosti radial'no-torcevogo kontaktnogo uplotnenija opory kompressora aviacionnogo dvigatelja na razlichnyh rezhimah raboty [Investigation tightness radial mechanical contact seal support aircraft engine compressor at different operating modes] //Vestnik SGAU. 2012. №3. S. 260–264.
  3. Inozemcev A.A., Sandrackij V.L. Gazoturbinnye dvigateli [Gas turbine engines]. Perm': OAO «Aviadvigatel'». 2006. S. 278–280.
  4. Migunov V.P., Farafonov D.P., Degovec M.L., Stupina T.I. Uplotnitel'nye materialy dlja protochnogo trakta GTD [Sealing materials for GTD flow path] //Aviacionnye materialy i tehnologii. 2012. №S. S. 94–97.
  5. Rozenenkova V.A., Solncev St.S., Mironova N.A. Tonkoplenochnye pokrytija dlja uplotnitel'nyh istiraemyh materialov na osnove diskretnyh volokon dlja protochnogo trakta GTD [Thin-film coating for sealing abrasive materials on the basis of discrete fibers to the flow path of GTD] //Trudy VIAM. 2013. №5. St. 04 (viam-works.ru).
  6. Sporer D., Wilson S., Giovannetti I., Refke A., Giannozzi M. On the potential of metal and ceramic based abradables in turbine seal applications /Proceedings of the 36-th turbomachinery symposium. Texas A&M University, Turbomachinery Laboratory. 2007. P. 79–86.
  7. Potter D.J., Chai Y.W., Tatlock G.J. Improvements in honeycomb abradable seals //Materials at High Temperatures. 2009. V. 26. №2. P. 127–135.
  8. Il'in A.A., Kolachev B.A., Pol'kin I.S. Titanovye splavy. Sostav, struktura, svojstva [Titanium alloys. The composition, structure and properties]. Spravochnik. M.: VILS–MATI. 2009. 520 s.
  9. Kashapov O.S., Pavlova T.V., Nochovnaja N.A. Vlijanie rezhimov termicheskoj obrabotki na strukturu i svojstva zharoprochnogo titanovogo splava dlja lopatok KVD [Effect of heat treatment on the structure and properties of heat-resistant titanium alloy blades for HPC] //Aviacionnye materialy i tehnologii. 2010. №2. S. 8–14.
  10. Antashev V.G., Nochovnaja N.A. Sovremennoe sostojanie i tendencii razvitija issledovanij v oblasti titanovyh splavov [Current status and trends of research in the field of titanium alloys] /V sb.75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: Jubilejnyj nauch.-tehnich. sb. M.: VIAM. 2007. S. 70–74.
  11. Zheng N.X., Däubler M.A., Schweitzer K.K., Hensle W., Schlegel H. Development of air seal system for modern jet engines. Munich: MTU Aero Engines GmbH. 2003.
  12. P. 1‒9.
  13. Nochovnaja N.A., Alekseev E.B., Izotova A.Ju., Novak A.V. Pozharobezopasnye titanovye splavy i osobennosti ih primenenija [Fireproof titanium alloys and features of their application] //Titan. 2012. №4. S. 42–46.
  14. Sporer D., Wilson S., Dorfman M. Ceramics for abradable shroud seal applications //Advanced ceramic coatings and interfaces. 2009. V. 30. P. 39–53.
  15. Migunov V.P., Farafonov D.P. Issledovanie osnovnyh jekspluatacionnyh svojstv novogo klassa uplotnitel'nyh materialov dlja protochnogo trakta GTD [Investigation of the basic operational properties of a new class of materials for sealing the flow path GTD] //Aviacionnye materialy i tehnologii. 2011. №3. S. 15–20.
  16. Migunov V.P., Farafonov D.P., Degovec M.L. Poristovoloknistyj material sverhnizkoj plotnosti na osnove metallicheskih volokon [Porous and fibrous material, ultra low density on the basis of metal fibers] //Aviacionnye materialy i tehnologii. 2012. №4. S. 38–41.
  17. Borisov B.V. Razrabotka tehnologii poluchenija volokon i poristyh materialov iz zharostojkih splavov metodom jekstrakcii visjashhej kapli rasplava [Development of technology for the manufacture of fibers and porous materials of the heat-resistant alloys by hanging drop melt extraction]: Avtoref. diss. k.t.n. M.: MATI–RGTU im. K.Je. Ciolkovskogo. 2011. 19 s.
  18. Serov M.M., Borisov B.V. Poluchenie metallicheskih volokon i poristyh materialov iz nih metodom jekstrakcii visjashhej kapli rasplava [Preparation of metallic fibers and porous materials, including extraction method hanging molten droplet] //Tehnologija legkih splavov. 2007. №3. S. 62–65.
  19. Migunov V.P. Uplotnitel'nye materialy [Sealing materials] /V sb. Aviacionnye materialy na rubezhe XX–XXI vekov: Nauch.-tehnich. sb. M.: VIAM. 1994. S. 344–346.
  20. Sposob poluchenija poristogo istiraemogo materiala iz metallicheskih volokon [A method for producing a porous abradable material of metal fibers]: pat. 2382828 Ros. Federacija; opubl. 28.04.2008.
  21. Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Prioritetnye napravlenija razvitija tehnologij proizvodstva zharoprochnyh materialov dlja aviacionnogo dvigatelestroenija [Priorities for the development of production technologies, high temperature materials for aircraft engine] //Problemy chernoj metallurgii i materialovedenija. 2013. №3. S. 47–54.