Research of oil resistance from basis butadien–nitrile rubbers made using emulsifiers of different types

Chaykun A.М., Venediktova M.A., Еliseev O.A., Naumov I.S.
Chaykun A.М., Venediktova M.A., Еliseev O.A., Naumov I.S. Research of oil resistance from basis butadien–nitrile rubbers made using emulsifiers of different types // Proceedings of VIAM. 2014. No. 8. DOI: 10.18577/2307-6046-2014-0-8-9-9. URL: https://viam-works.ru/en/journal/2014/8/9
Abstract

In article features of oil resistance rubber compounds are presented on basis bu-tadiyen-nitrile rubbers (BNK) which have been synthesized with use of emulsifiers of different types. Properties butadiyen-nitrile rubbers will be defined not only the content of acrylenitrile links of rubber, but also features of its polymerization. Recently in connection with toughening of ecological requirements, along with traditional emulsifier – nekaly, are used easily washed away alkylsulfonates. In the article the wide complex of properties oil resistance butadiyen-nitrile the rubbers made of BNK with use of emulsifiers of different types is investigated. In the carried-out research the factors influencing oil resistance of rubbers, made of rubbers with different emulsifiers are defined. The dependences revealed in work allow to predict in the maximum degree properties bu-tadiyen-nitrile rubbers made on the basis of rubbers with use of emulsifiers of different types.

Reference list
  1. Bol'shoj spravochnik rezinshhika [Great Compendium rezinschikov]. V 2 ch. M.: Tehinform. 2012. 1385 s.
  2. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki do 2030 goda [Strategic directions of development of materials and technologies to process them until 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Eliseev O.A., Krasnov L.L., Zajceva E.I., Savenkova A.V. Razrabotka i modificirovanie jelastomernyh materialov dlja primenenija vo vseklimaticheskih uslovijah [Development and modification of elastomeric materials for use in all climate conditions] //Aviacionnye materialy i tehnologii. 2012. №S. S. 309–314.
  4. Mahlis F.A., Fedjukin D.L. Terminologicheskij spravochnik po rezine [Terminological reference for rubber]. M.: Himija. 1989. 400 s.
  5. Tehnologija reziny: Recepturostroenie i ispytanija [Rubber Technology: Retsepturostroenie and testing]: Per. s angl. /Pod red. Dzh.S. Dika. SPb.: Nauchnye osnovy i tehnologii. 2010. 620 s.
  6. Shvejcer F.A. Korrozija plastmass i rezin [Corrosion of plastics and rubber]. SPb.: Nauchnye osnovy i tehnologii. 2010. 637 s.
  7. Martin Dzh. M., Smit U.K. Proizvodstvo i primenenie rezinotehnicheskih izdelij [Production and use of rubber products]: Per. s angl. /Pod red. S.Ch. Bhati. SPb.: Professija. 2006. 480 s.
  8. Chajkun A.M., Eliseev O.A., Naumov I.S., Venediktova M.A. Osobennosti morozostojkih rezin na osnove razlichnyh kauchukov [Features frost rubbers based on different rubbers] //Trudy VIAM. 2013. №12. St. 04 (viam-works.ru).
  9. Erasov V.S., Kotova E.A. Jerozionnaja stojkost' aviacionnyh materialov k vozdejstviju teverdyh (pylevyh) chastic [Erosion resistance to the effects of aircraft materials teverdyh (dust) particles] //Aviacionnye materialy i tehnologii. 2011. №3. S. 30–36.
  10. Ushmarin N.F., Petrova N.P., Kol'cov N.I. Issledovanie maslobenzostojkih rezin s primeneniem kompozicionnyh stabilizatorov na osnove kovantoksa 8 PFDA [Maslobenzostojky study of composite rubber-based stabilizers kovantoksa 8 PFDA] //Vestnik Kazanskogo tehnologicheskogo instituta. 2011. №2. S. 67–76.
  11. Sokolova L.V., Matuhina E.V. Fazovoe sostojanie stearata kal'cija v kauchukah BNKS [Phase state of calcium stearate in rubbers BNKS] //Kauchuk i rezina. 2012. №1. S. 14–17.
  12. Kovaleva L.A., Livanova N.M., Ovsjannikov N.Ja. Issledovanie nabuhanija rezin iz butadien-nitril'nyh kauchukov v nepoljarnom rastvoritele n-geptane [Study of swelling rubber butadiene-nitrile rubbers in a nonpolar solvent n-heptane] /V sb. trudov XVIII Mezhdunarodnoj nauch.-praktich. konf. «Rezinovaja promyshlennost'. Syr'e. Materialy. Tehnologii». 2012. S. 63–66.
  13. Maskuljuinate O.E., Morozov Ju.L., Suhinin N.S. i dr. Vlijanie sposoba vvedenija plastifikatora na svojstva parafinatnyh kauchukov BNKS i standartnye reziny na ih osnove [Influence of the route of administration of the plasticizer on the properties of rubber parafinatnyh BNKS and standard rubber based on them] //Kauchuk i rezina. 2006. №3. S. 14–17.
  14. Anisimov B.Ju., Dybman A.S., Imjanitov L.S., Poljakov S.A. Gidrirovanie butadien-nitril'nyh kauchukov [Hydrogenation of butadiene-nitrile rubbers] //Kauchuk i rezina. 2007. №2. S. 32–38.
  15. Shuvaeva A.V. Rezino-tkanevye membrannye materialy na osnove gidrirovannyh butadien-nitril'nyh kauchukov [Rubber-fabric membrane materials based on hydrogenated nitrile rubbers]: Avtoref. dis. k.t.n. M. 2011. 23 s.
  16. Kotova S.V., Mihajlov S.I., Fomina A.A. Osobennosti sovremennogo rynka butadien-nitril'nyh kauchukov [Features modern market NBR] //Kauchuk i rezina. 2012. №6.
  17. S. 33–35.
  18. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  19. Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies for aircraft] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  20. Chajkun A.M., Eliseev O.A., Naumov I.S., Venediktova M.A. Osobennosti postroenija receptur dlja morozostojkih rezin [Features recipes for constructing frost rubbers] //Aviacionnye materialy i tehnologii. 2013. №3. S. 53–55.
  21. Aviacionnye pravila. Gl. 25. Normy letnoj godnosti samoletov transportnoj kategorii [Aviation Regulations. Chap. 25. Standards of airworthiness of transport category]. 3-e izd. OAO Aviaizdat. 2009. 274 s.
  22. Efimov V.A., Shvedkova A.K., Koren'kova T.G., Kirillov V.N. Issledovanie polimernyh konstrukcionnyh materialov pri vozdejstvii klimaticheskih faktorov i nagruzok v laboratornyh i naturnyh uslovijah [Investigation of polymeric structural materials under the influence of climatic factors and stress in laboratory and field conditions] //Trudy VIAM. 2013. №1. St. 05 (viam-works.ru).