Modern technologies of hotmelt polymer composite materials processing
Timoshkov P.N., Khrulkov A.V. Modern technologies of hotmelt polymer composite materials processing // Proceedings of VIAM. 2014. No. 8. DOI: 10.18577/2307-6046-2014-0-8-4-4. URL: https://viam-works.ru/en/journal/2014/8/4
Abstract
At present time polymer composite materials (PCM) based on hotmelt binder have become increasingly popular displacing traditional solvent-based PCM. This fact make possible the emergence of perspective new ways of PCM processing and allows to sim-plify and reduce the cost of PCM-based constructions and products forming process. To make it real new technological processes and new types of industrial equipment having different characteristics compared with previously known, and a number of associated auxiliary equipment have been developed.
Reference list
- Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih perera-botki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. III. Znachimye faktory starenija [Climatic aging of composite materials for aircraft industry. III. Significant factors of aging] //Deformacija i razrushenie materialov. 2011. №1. S. 34–40.
- Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace Materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
- Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svjazujushhie dlja perspektivnyh metodov izgotovlenija konstrukcionnyh voloknistyh PKM [New polymeric binders for advanced manufacturing techniques of structural fibrous RMB] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
- Sokolov I.I., Raskutin A.E. Ugleplastiki i stekloplastiki novogo pokolenija [Carbon and fiberglass new generation] //Trudy VIAM. 2013. №4 (viam-works.ru).
- Babin A.N. Svjazujushhie dlja polimernyh kompozicionnyh materialov novogo pokolenija [Binders for polymer composite materials of new generation ] //Trudy VIAM. 2013. №4 (viam-works.ru).
- Dushin M.I., Hrul'kov A.V., Kogan D.I., Muhametov R.R., Karavaev R.Ju. Ugleplastiki, polu-chenye metodom infuzii rasplava svjazujushhego [Carbon composites, obtained by infusion melt binder] //Kompozity i nanostruktury. 2013. №2 (18). S. 42–50.
- Zwehen C. Assessment of the Science Base for Composite Materials //Advanced Materials by Design. 2011. №3. Р. 73–93.
- Bejder Je.Ja., Petrova G.N., Izotova T.F., Barbot'ko S.L. Stekloplastiki na termoplastichnoj matrice [Glass-reinforced on thermoplastic matrix] //Trudy VIAM. 2013. №7. St. 03 (viam-works.ru).
- Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svjazujushhie dlja perspektivnyh metodov izgotovlenija PKM novogo pokolenija [Melt binders promising methods of manufacturing a new generation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
- McClain M., Goering J. Overview of Recent Developments in 3D Structures /ICCM-17, 3D Textiles & Composites. Edinburgh. 2009.
- Grigor'ev M.M., Kogan D.I., Tverdaja O.N., Panina N.N. Osobennosti izgotovlenija PKM metodom RFI [Features manufacturing method RMB RFI] //Trudy VIAM. 2013. №4. St. 03 (viam-works.ru).
- http://cavitec-ch.site-preview.net/en/, http://www.centurydesign.com/, http://www.calitzler.com/, http://www.coatema.de/, http://www.mikrosam.com/
- Kablov E.N., Starcev O.V., Deev I.S., Nikishin E.F. Svojstva polimernyh kompozicionnyh materialov posle vozdejstvija otkrytogo kosmosa na okolozemnyh orbitah [Properties of polymeric composite materials after exposure to open space in earth orbit] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №10. S. 2–3.
- Dushin M.I., Hrul'kov A.V., Raskutin A.E. K voprosu udalenija izlishkov svjazujushhego pri avtoklavnom formovanii izdelij iz polimernyh kompozicionnyh materialov [On the question of removing excess binder in an autoclave molding products from polymeric composite materials] //Trudy VIAM. 2013. №1. St. 03 (viam-works.ru).
- Dushin M.I., Kogan D.I., Hrul'kov A.V., Gusev Ju.A. Prichiny obrazovanija poristosti v izdelijah iz polimernyh kompozicionnyh materialov [Reasons for the formation of porosity in the products of polymeric composite materials] //Kompozity i nanostruktury. 2013. №3 (19). S. 60–71.
- Dushin M.I., Chursova L.V., Hrul'kov A.V., Kogan D.I. Osobennosti izgotovlenija polimernyh kompozicionnyh materialov metodom vakuumnoj infuzii [Features manufacture of polymer composite materials using vacuum infusion] //Voprosy materialovedenija. 2013. №3 (75). S. 33–40.