The design characteristic of metallic materials taking into account the humidity

Grinevich A.V., Lutsenko A.N., Karimova S.A.
Grinevich A.V., Lutsenko A.N., Karimova S.A. The design characteristic of metallic materials taking into account the humidity // Proceedings of VIAM. 2014. No. 7. DOI: 10.18577/2307-6046-2014-0-7-10-10. URL: https://viam-works.ru/en/journal/2014/7/10
Abstract

The problem of determining the design characteristics of structural metallic materials in connection with the new edition of Aviation Rules is considered. It is shown that the requirements for accounting for the influence of corrosion environments are included in the section laying down the requirements for the design values of strength properties. The criterion of damage to corrosion, which allows to realize the effect of «compression» of time, which provides the basis for the determination of the calculated values of the fatigue life when exposed to corrosive environment, is proposed. A list of the strength characteristics for which it is advisable to determine the estimated value of the strength characteristics of the humidity is established.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Ospennikova O.G. Strategija razvitija zharoprochnyh splavov i stalej special'nogo naznachenija, zashhitnyh i teplozashhitnyh pokrytij [The development strategy of superalloys and special steel, protective and thermal barrier coatings] //Aviacionnye materialy i tehnologii. 2012. №S. S. 19–36.
  3. Fejgenbaum Ju.M., Dubinskij S.V. Vlijanie sluchajnyh jekspluatacionnyh povrezhde-nij na prochnost' i resurs konstrukcii vozdushnyh sudov [The effect of random damage to operational strength and resource aircraft design] //Nauchnyj vestnik Moskovskogo gosudarstvennogo tehnicheskogo universiteta grazhdanskoj aviacii. 2013. №187. S. 83–91.
  4. Aviacionnye pravila. Chast' 25. Normy letnoj godnosti samoletov transportnoj kategorii [Aviation Regulations. Part 25. Airworthiness standards transport category airplanes]. MAK: OAO «Aviaizdat». 2009. 267 s.
  5. Serensen S.V., Kogaev V.P., Shnejderovich R.M. Nesushhaja sposobnost' i raschet detalej mashin na prochnost' [Bearing capacity and settlement of machine parts for durability]: Rukovodstvo i sprav. posob. M.: Mashinostroenie. 1975. 488 s.
  6. Kogaev V.P., Mahutov N.A., Gusenkov A.P. Raschety detalej mashin i konstrukcij na prochnost' i dolgovechnost' [Calculations of machine parts and structures for strength and durability]: Spravochnik. M.: Mashinostroenie. 1985. 224 s.
  7. Akimov G.V. Teorija i metody issledovanija korrozii metallov [Theory and Methods of metal corrosion]. M.-L.: Izd-vo AN SSSR. 1945. 414 s.
  8. Krenig V.O. Korrozija metallov [Metal corrosion]. M.-L.: ONTI NKTP SSSR. 1936. 304 s.
  9. Korrozionnaja ustalost' metallov [Corrosion fatigue of metals] /Pod red. akademika Ja.M. Kolotyrkina. Kiev: Naukova Dumka. 1982. 371 s.
  10. Ulig G.G., Revi R.U. Korrozija i bor'ba s nej [Corrosion and combating]. L.: Himija. 1989. 455 s.
  11. Kablov E.N. Korrozija ili zhizn' [Corrosion or life] //Nauka i zhizn'. 2012. №11. S. 16–21.
  12. EUROCORR 2010: The European Corrosion Congress 2010 /In: European Federation of Corrosion Event. 2010. №324. 684 p.
  13. Grinevich A.V., Zhirnov A.D., Karimova S.A. Prognozirovanie ustalostnoj dolgovechnosti metallicheskih materialov pri korrozionnom vozdejstvii [Prediction of fatigue life of metallic materials under corrosion attack] /V sb. dokladov konf. «Gelendzhik-2010». M.: ONTI CAGI. 2010. S. 199–205.
  14. Zhilikov V.P., Karimova S.A., Leshko S.S., Chesnokov D.V. Issledovanie dinamiki korrozii aljuminievyh splavov pri ispytanii v kamere solevogo tumana (KST) [Study of the dynamics of corrosion of aluminum alloys when tested in the salt spray chamber (SSC] //Aviacionnye materialy i tehnologii. 2012. №4. S. 18–22.
  15. Hohlatova L.B., Kolobnev N.I., Antipov V.V., Karimova S.A., Rudakov A.G., Oglodkov M.S. Vlijanie korrozionnoj sredy na skorost' rosta treshhiny ustalosti v aljuminievyh splavah [Effect of environment on corrosion fatigue crack growth rate in aluminum alloys] //Aviacionnye materialy i tehnologii. 2011. №1. S. 16–20.
  16. Karimova S.A., Pavlovskaja T.G. Razrabotka sposobov zashhity ot korrozii konstrukcij, rabotajushhih v uslovijah kosmosa [Development of methods of corrosion protection structures operating in space] //Trudy VIAM. 2013. №4. St. 02 (viam-works.ru).
  17. Starcev O.V., Medvedev I.M., Kurs M.G. Tverdost' kak indikator korrozii aljuminievyh splavov v morskih uslovijah [Hardness as an indicator of corrosion of aluminum alloys in marine environments] //Aviacionnye materialy i tehnologii. 2012. №3. S. 16–19.
  18. Mahsidov V.V., Kolobnev N.I., Karimova S.A., Sbitneva S.V. Vzaimosvjaz' struktury i korrozionnoj stojkosti v splave 1370 sistemy Al–Mg–Si–Cu–Zn [Relationships between structure and corrosion resistance of the alloy system 1370 Al–Mg–Si–Cu–Zn] //Aviacionnye materialy i tehnologii. 2012. №1. S. 8–13.
  19. Lucenko A.N., Grinevich A.V., Karimova S.A. Prochnostnye harakteristiki materialov planera samoletov v uslovijah vlazhnosti [Strength characteristics of materials glider aircraft in wet conditions] //Voprosy materialovedenija. 2013. №1. S. 212–219.
  20. Grinevich A.V., Lucenko A.N., Karimova S.A. Dolgovechnost' izdelij i korrozionnaja ustalost' konstrukcionnyh materialov [Durability of products and corrosion fatigue of structural materials] //Voprosy materialovedenija. 2013. №1. S. 220–229.
  21. Grinevich A.V., Lucenko A.N., Karimova S.A. Issledovanie ostatochnoj ustalostnoj dolgovechnosti aljuminievogo splava V95p.ch.-T1 posle jekspozicii v razlichnyh uslovijah [Investigation of the residual fatigue life of aluminum alloy V95p.ch.-T1 after exposure to different conditions] //Voprosy materialovedenija. 2013. №2. S. 118–122.
  22. Erasov V.S., Grinevich A.V., Senik V.Ja., Konovalov V.V., Trunin Ju.P., Nesterenko G.I. Raschetnye znachenija harakteristik prochnosti aviacionnyh materialov [Calculated values of the strength characteristics of aircraft materials] //Aviacionnye materialy i tehnologii. 2012. №2. S. 14–16.