The investigation of the properties and technological parameters producing metallic fibers for abradable sealing materials of aircraft GTE

Farafonov D.P., Degovets M.L., Serov M.M.
Farafonov D.P., Degovets M.L., Serov M.M. The investigation of the properties and technological parameters producing metallic fibers for abradable sealing materials of aircraft GTE // Proceedings of VIAM. 2014. No. 7. DOI: 10.18577/2307-6046-2014-0-7-2-2. URL: https://viam-works.ru/en/journal/2014/7/2
Abstract

In order to increase the operating temperature of abradable seal materials the prop-erties and technological parameters for obtaining metallic fibers by method of extraction melt hanging drops from a variety of heat-resistant alloys based on nickel, iron and intermetallic compounds Ni3Al and NiAl was investigate. The possibility of creating high-effective sealing materials with operating temperatures above 1000°C for use in the flow path of the turbine GTE are shown.

Reference list
  1. Migunov V.P. Materialy dlja uplotnenij protochnoj chasti GTD [Sealants flowing part of GTE] /V sb.: Voprosy aviacionnoj nauki i tehniki. Ser. Aviacionnye materialy. Vyp. Uplotnitel'nye materialy dlja protochnoj chasti GTD. M.: VIAM. 1993. S. 5–8.
  2. Kuznecov E.G., Majler D.P., Pochuev V.P. Primenenie istiraemyh uplotnenij v protochnoj chasti GTD [Application abradable seals in the running part of GTE] /V sb.: Voprosy aviacionnoj nauki i tehniki. Ser. Aviacionnye materialy. Vyp. Uplotnitel'nye materialy dlja protochnoj chasti GTD. M.: VIAM. 1993. S. 8–13.
  3. Egan O.M., Sapronov T.G., Maksimova R.Z., Mokina G.P., Kachanovskaja L.T. Metodiki issledovanij materialov dlja uplotnenij protochnogo trakta [Research methodology materials for sealing the flow path] /V sb.: Voprosy aviacionnoj nauki i tehniki. Ser. Aviacionnye materialy. Vyp. Uplotnitel'nye materialy dlja protochnoj chasti GTD. M.: VIAM. 1993. S. 17–21.
  4. Inozemcev A.A., Sandrackij V.L. Gazoturbinnye dvigateli [Gas turbine engines]. Perm': OAO «Aviadvigatel'». 2006. S. 278–280.
  5. Migunov V.P. Uplotnitel'nye materialy [Sealants] /V sb. Aviacionnye materialy na rubezhe HH–HHI vekov. M.: VIAM. 1994. S. 344–346.
  6. Migunov V.P., Lomberg B.S. Poristovoloknistye metallicheskie materialy dlja zvukopogloshhajushhih i uplotnitel'nyh konstrukcij [Porous and fibrous metallic materials for sound and sealing structures] /V sb.: 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: Jubilejnyj nauch.-tehnich. sb. M.: VIAM. 2007. S. 270–275.
  7. Migunov V.P., Farafonov D.P., Degovec M.L., Stupina T.I. Uplotnitel'nye materialy dlja protochnogo trakta GTD [Sealing materials for the flow path GTE] //Aviacionnye materialy i tehnologii. 2012. №S. S. 94–97.
  8. Migunov V.P., Farafonov D.P. Issledovanie osnovnyh jekspluatacionnyh svojstv novogo klassa uplotnitel'nyh materialov dlja protochnogo trakta GTD [Investigation of the basic operational properties of a new class of materials for sealing the flow path GTE] //Aviacionnye materialy i tehnologii. 2011. №3. S. 15–20.
  9. Sporer D., Wilson S., Giovannetti I., Refke A., Giannozzi M. On the potential of metal and ceramic based abradables in turbine seal applications /Proceedings of the thirty-sixth turbomachinery symposium. Texas A & M University. 2007. P. 79–86.
  10. Potter D.J., Chai Y.W., Tatlock G.J. Improvements in honeycomb abradable seals //Materials at High Temperatures. 2009. V. 26. №2. P. 127–135.
  11. Zheng N.X., Däubler M.A., Schweitzer K.K., Hensle W., Schlegel H. Development of air seal system for modern jet engines. Munich: MTU Aero Engines GmbH. 2003.
  12. Sporer D., Wilson S., Dorfman M. Ceramics for abradable shroud seal applications //Advanced ceramic coatings and interfaces. 2009. V. 30. №4. P. 39–53.
  13. Serov M.M., Borisov B.V. Poluchenie metallicheskih volokon i poristyh materialov iz nih metodom jekstrakcii visjashhej kapli rasplava [Preparation of metallic fibers and porous material of which the hanging drop method of extraction of the melt] //Tehnologija legkih splavov. 2007. №3. S. 62–65.
  14. Serov M.M. Mikrokristallicheskie i amorfnye splavy, poluchennye metodom vysokoskorostnogo zatverdevanija rasplava [Microcrystalline and amorphous alloys obtained by high-speed melt solidification] //Tehnologija legkih splavov. 2008. №4.
  15. S. 34–40.
  16. Borisov B.V., Serov M.M. Formirovanie poristyh voloknovyh materialov metodom jekstrakcii visjashhej kapli rasplava [Formation of porous materials by extraction of fiber hanging melt drops] //Izvestija vuzov. Poroshkovaja metallurgija i funkcional'nye pokrytija. 2013. №1. S. 55–58.
  17. Anciferov V.N., Serov M.M., Lezhnin V.P., Smetkin A.A. O poluchenii, svojstvah i primenenii bystroohlazhdennyh volokon волокон [On receipt, properties and applications of rapidly cooled fibers] //Izvestija vuzov. Poroshkovaja metallurgija i funkcion-al'nye pokrytija. 2011. №4. S. 36–40.
  18. Solncev S.S., Rozenenkova V.A., Mironova N.A., Gavrilov S.V. Vysokotemperaturnye tonkoplenochnye pokrytija dlja uplotnitel'nyh materialov iz metallicheskih volokon [High-temperature thin-film coatings for sealing materials of metal fibers] //Aviacionnye materialy i tehnologii. 2012. №1. S. 30–36.
  19. Solncev S.S., Rozenenkova V.A., Mironova N.A., Gavrilov S.V. Vysokotemperaturnye pokrytija SiC–Si3N4–SiO2 dlja uplotnitel'nyh materialov iz metallicheskih volokon [High temperature coating SiC–Si3N4–SiO2 for sealing materials of metal fibers] //Steklo i keramika. 2011. №6. S. 27–30.
  20. Solntsev S.S., Rozenenkova V.A., Mironova N.A., Gavrilov S.V. SiC–Si3N4–SiO2 high-temperature coatings for metal fiber sealing materials //Glass and Ceramics. 2011. V. 68. №5–6. P. 194–195.
  21. Bazyleva O.A., Arginbaeva Je.G., Turenko E.Ju. Vysokotemperaturnye intermetallidnye splavy dlja detalej GTD [High-temperature intermetallic alloys for GTE parts] //Aviacionnye materialy i tehnologii. 2013. №3. S. 26–31.
  22. Bazyleva O.A., Arginbaeva Je.G., Turenko E.Ju. Zharoprochnye litejnye intermetallidnye splavy [Heat-resistant casting intermetallic alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 57–60.
  23. Splav na osnove intermetallida Ni3Al [Alloy based on Ni3Al intermetallic]: pat. 2434067 Ros. Federacija; opubl. 01.07.2010.
  24. Splav na osnove intermetallida Ni3Al [Alloy based on Ni3Al intermetallic]: pat. 2434068 Ros. Federacija; opubl. 05.10.2010.
  25. Sposob poluchenija poristogo istiraemogo materiala iz metallicheskih volokon [A method for producing a porous abradable material of metal fibers]: pat. 2382828 Ros.Federacija; opubl. 28.04.2008.
  26. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.