Ceramic composite materials with high oxidation resistance for the novel aircrafts (review)

Sorokin O.Ju., Grachshencov D.V., Solncev S.St., Evdokimov S.A.
Sorokin O.Ju., Grachshencov D.V., Solncev S.St., Evdokimov S.A. Ceramic composite materials with high oxidation resistance for the novel aircrafts (review) // Proceedings of VIAM. 2014. No. 6. DOI: 10.18577/2307-6046-2014-0-6-8-8. URL: https://viam-works.ru/en/journal/2014/6/8
Abstract

Future prospect of novel oxidation-resistant materials for aviation purposes was highlighted. The key methods of their processing with ultra-high temperature ceramic matrix (UHTC) were discussed.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Jastin J.F., Jankowiak A. Ultra high temperature ceramics: densification, properties and thermal stability //Aerospace Lab. 2011. №3. P. 1–11.
  3. Matovic B., Yano T. Silicon Carbide and other carbides: from stars to the advanced ceramics /In: Handbook of advanced Ceramics. Chapter 3.1. 2013. P. 225–244.
  4. Dospehi dlja «Burana». Materialy i tehnologii VIAM dlja MKS «Jenergija–Buran» [Armor for the «Buran». Materials and technologies for VIAM ISS «Energia-Buran»] /Pod. red. E.N. Kablova. M.: Fond «Nauka i zhizn'». 2013. 128 s.
  5. Grashhenkov D.V., Chursova L.V. Strategija razvitija kompozicionnyh i funkcional'nyh materialov [Development Strategy composite and functional materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  6. Opeka M.M., Talmy I.G., Zaykoski J.A. Oxidation-based materials selection for 2000°C+hypersonic aerosurfaces: Theoretical considerations and historical experience //J. Mater. Sci. 2004. V. 39. P. 5887–5904.
  7. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Promising high-temperature ce-ramic composites] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 20–24.
  8. Lebedeva Ju.E., Popovich N.V., Orlova L.A. Zashhitnye vysokotemperaturnye pokrytija dlja kompozicionnyh materialov na osnove SiC [Protective coatings for high-temperature composite materials based on SiC] //Trudy VIAM. 2013. №2. St. 06 (viam-works.ru).
  9. Solncev S.S., Rozenenkova V.A., Mironova N.A., Gavrilov S.V. Keramicheskie pokrytija dlja zashhity vysokoprochnoj stali pri termicheskoj obrabotke [The ceramic coating to protect the high-strength steel during heat treatment] //Aviacionnye materialy i tehnologii. 2011. №4. S. 3–8.
  10. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S., Sevast'janov V.G. Vysokotemperaturnye konstrukcionnye kompozicionnye materialy na osnove stekla i keramiki dlja perspektivnyh izdelij aviacionnoj tehniki [High-temperature structural composite materials based on glass and ceramic products for advanced aircraft] //Steklo i keramika. 2012. №4. S. 7–11.
  11. Simonenko E.P., Simonenko N.P., Sevast'janov V.G., Grashhenkov D.V., Kuznecov N.T., Kablov E.N. Funkcional'no gradientnyj kompozicionnyj material SiC/(ZrO2–HfO2–Y2O3), poluchennyj s primeneniem zol'-gel' metoda [Functionally gradient com-posite material SiC/(ZrO2–HfO2–Y2O3), prepared using a sol-gel method] //Kompozity i nanostruktury. 2011. T. 4. S. 52–64.
  12. Zhu Y., Wang S., Chen H. Effect of copper on microstructure and mechanical properties of Sf/ZrC composites fabricated by low-temperature liquid metal infiltration //Cer. Int. 2014. V. 40. P. 2793–2798.
  13. Bongiorno A., Först C.J., Kalia R.K. A Perspective on Modeling Materials in Extreme Environments: Oxidation of Ultrahigh-Temperature Ceramics //MRS Bulletin. 2006. V. 31. P. 410–418.
  14. Gasch M., Ellerby D., Beckman S. Processing, properties and arc jet oxidation of hafnium diboride/silicon carbide ultrahigh temperature ceramics //J. Mater. Sci. 2004. V. 39. P. 5925–5937.
  15. Eakins E., Jayaseelan D.D., Lee W.E. Toward Oxidation-Resistant ZrB2–SiC Ultra High Temperature Ceramics //Metal. Mater. Trans. A. 2011. V. 42A. P. 878–887.
  16. Ermolenko I.N., Ul'janova T.M., Vitjaz' P.A. Voloknistye vysokotemperaturnye keramicheskie materialy [High temperature ceramic fiber material]. M.: Nauka i tehnika. 1991. 255 s.
  17. Monteverde F., Alfano D., Savino R. Effects of LaB6 addition on arc-jet convectively heated SiC-containing ZrB2-based ultra-high temperature ceramics in high enthalpy supersonic airflows //Corrosion Science. 2013. V. 75. P. 443–453.
  18. Williams P.A., Sakidia R., Perepezko J.H. Oxidation of ZrB2–SiC ultra-high tempera-ture composites over a wide range of SiC content //J. Eur. Cer. Soc. 2012. V. 32. P. 3875–3883.
  19. Magnani G., Antolini F., Beaulardi L. Sintering, high temperature strength and oxidation resistance of liquid-phase-pressureless-sintered SiC–AlN ceramics with addition of rare-earth oxides //J. Eur. Cer. Soc. 2009. V. 29. P. 2411–2417.
  20. Lojanová Š., Dusza J., Šajgalík P. Characterization of rare-earth doped Si3N4/SiC mi-cro/nanocomposites //Proc. and Appl. Of Cer. 2010. V. 4. №1. P. 25–32.
  21. Paul A., Jayaseelan D.D., Venugopal S. UHTC composites for hypersonic applications //Am. Cer. Soc. Bul. 2012. V. 91. №1. P. 22–29.
  22. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of current and future high-tech] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  23. Stackpoole M., Rom G., Whitt J. UHTC composites with nanotube-reinforcement for advanced TPS applications /In: 3-rd Int. Planetary Probe Workshop. Anavyssos, Attiki. 2005.
  24. Gunjaev G.M., Kablov E.N., Aleksashin V.M. Modificirovanie konstrukcionnyh ugleplastikov uglerodnymi nanochasticami [Modification of structural carbon fiber with carbon nanoparticles] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 5–19.
  25. Yadhukulakrishnan G.B., Karumuri S., Rahman A. Spark plasma sintering of graphene reinforced zirconium diboride ultra-high temperature ceramic composites //Cer. Int. 2013. №39. P. 6637–6646.