Estimation of the elastic modulus of refractory oxides based fibers

Zimichev A.M., Varrik N.M., M.A. Dalin
Zimichev A.M., Varrik N.M., M.A. Dalin Estimation of the elastic modulus of refractory oxides based fibers // Proceedings of VIAM. 2014. No. 6. DOI: 10.18577/2307-6046-2014-0-6-5-5. URL: https://viam-works.ru/en/journal/2014/6/5
Keywords
modulus of elasticity
Abstract

The elastic modulus of high temperature fibers based on aluminum oxide are esti-mated. The results of the acoustic testing of refractory oxides based filaments intended for the manufacture of flexible sealing insulation are described.

Reference list
  1. Kablov E.N. Strategicheskie napravlenia razvitia materialov i technologii ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviationnie materiali i tehnologii. 2012. №S. S. 7–17.
  2. Ivahnenko Yu.A., Babashov V.G., Zimichev A.M., Tinyakova E.V. Visokotemperaturnie teploizoljazionnie i teplozachitie materiali na osnove tugoplavkih soedinenii [High-temperature and heat-insulating materials based on refractory compounds] //Aviationnie materiali i tehnologii. 2012. №S. S. 380–386.
  3. Grashchenkov D.V., Tinyakova E.V. Teploizoliazionnii material na osnove mullito-korundobih i kvarzevih volokon [Thermal insulation material on the basis of mullite-corundum and quartz fibers] //Aviationnie materiali i tehnologii. 2012. №3. S. 43–47.
  4. Kablov E.n., Shchetanov B.v., Abuzin Y.a., Ivahnenko Yu.a. Metallicheskie i keramicheskie komposizionnie materiali [Metal and ceramic composite materials] /V sb. materi-alov Mezhdunarodnoi nauch-praktich. konf. «Sovremennie tehnologii – kluchevoe zveno v vozrozhdenii otechestvennogo aviastroenia». T. 1. Kazan'. 2008. S. 181–188.
  5. Kablov E.N., Grashchenkov D.V., Isayeva N.V., Solntsev S.S. Perspectivnie visokotem-peraturnie keramicheskie kompositionnie materiali [Promising high-temperature ceramic composites] //Rossiiskii himicheskii zhurnal. 2010. T. LIV. №1. S. 20–24.
  6. Kablov E.N. Shchetanov B.V., Ivakhnenko Yu.A., Balinova Yu.A. Perspectivnie armirujuchie visokotemperaturnie volokna dlia metallicheskih and keramicheskih kom-positionnie materiali [Prospective reinforcing fiber for high temperature ceramic composites and metal materials] //Trudi VIAM. 2013. №2. St. 05 (viam-works.ru).
  7. Kablov E.N. Tendencii i orientiri innovationnogo razvitia Rossii [Trends and bench-marking innovation development in Russia]: Sb. nauch.-informationnih materialov. M.: VIAM. 2013. 543 s.
  8. Dospehi dlia «Burana». Materiali and tehnologii VIAM for MKS «Energiya-Buran» [Armor for the «Buran». Materials and technologies for VIAM ISS «Energia-Buran»] /Pod obchei. red. E.N. Kablov. M.: Fond «Nauka i zhizn». 2013. 128 s.
  9. Shchetanov B.V., Ivakhnenko Yu.A., Babashov V.G. Teplozachitnie materiali [Heat-proof materials] //Rossiiskii himicheskii zhurnal. 2010. T. LIV. №1. S. 12–20.
  10. Krenkel W., Lamon J. Hight-Temperature Ceramic Materials and Composites /In: 7-th Internatiolal Conference on Ceramic Matrix Composites (HT-CMC 7). 2010. 938 p.
  11. Ceramic Fibers and Coatings. Advanced Materials for the Twenty-First Century Committee on Advanced Fibers for High-Temperature Ceramic Composites. Washington: National Academy Press. 1998. 95 р.
  12. Wilson D.M., Visser L.R. High performance oxide fibers for metal and ceramic composites /In: Processing of fibers & composites. Barga. 2000. 31 p.
  13. Parlier M., Ritti M.-H., Jankowiak A. Potential and Perspectives for Oxide-Oxide Composites //Journal Aerospacelab. 2011. №3. Р. 1–12.
  14. Jessen T., Ustundag E. 24-th Annual Conference on Composites, Advanced Ceramics, Materials, and Structures. B /In: Ceramic Engineering and Science Proceedings. 2000. V. 21. №4. Р. 760.
  15. Bunsell A.R. Oxide fibers for high-temperature reinforcement and insulation //JOM. 2005. V. 57. №2. Р. 48–51.
  16. Kirienko T.A., Solov’eva E.P., Balinova Yu.A. Physical-chemical Properties of Spinning Solutions for Aluminum-Silicate Fibrous Materials //Glass and Ceramics. 2013. V. 70. №7–8. Р. 300–302.
  17. Yavorsky B.M., Detlaf A.A., Lebedev A.K. Spravochnik po fisike [Handbook of Physics]. M.: Oniks 21 vek. 2008. 1056 s.
  18. Dalin M.A., Generalovof A.S., Boychuk A.S., Lozhkova D.S. Osnovnie tendencii of razvitia akusticheskih methodov of neraztushajuchego kontrolia [The main trends in the development of acoustic methods of nondestructive testing] //Aviationnie materiali i tehnologii. 2013. №1. S. 64–68.
  19. Generalovof A.S., Murashov V.V., Dalin M.A., Boychuk A.S. Diagnostika polimernih kompositov ultrazvukovim reverbazionno-skvoznim metodom [Diagnosis polymer composites ultrasonic reverberation-through-method] //Aviationnie materiali i tehnologii. 2012. №1. S. 42–47.
  20. Sposob opredelenia prochnostnih haracteristik polymernih kompositionnih materialov [A method for determining the strength characteristics of polymeric composite materials]: pat. 2461820 Ros. Federatsia; opubl. 20.09.2012. Bull. №26. 14 s.
  21. GOST 28007–88 Gosudarstvennii komitet po standartam.