The obtaining and testing of the fine-dispersed metal powder of the high-chromium alloy on nickel-base for laser metal deposition

Evgenov A.G., Nerush S.V., Vasilenko S.A.
Evgenov A.G., Nerush S.V., Vasilenko S.A. The obtaining and testing of the fine-dispersed metal powder of the high-chromium alloy on nickel-base for laser metal deposition // Proceedings of VIAM. 2014. No. 5. DOI: 10.18577/2307-6046-2014-0-5-4-4. URL: https://viam-works.ru/en/journal/2014/5/4
Abstract

Fine-dispersed metal powders of the heat resisting alloy brand EP648-VI for laser metal deposition (LMD), obtained by method of atomization at a facility HERMI-GA10/100 VI are investigated. It is shown, that the obtained fine-dispersed powders when spraying by cold and hot gas have low oxygen content, the spherical form, the expressed dendritic structure in all range of the granulometric distribution. Adaptive laser metal deposition with application metal powder of the heat resisting alloy EP648-VI of the granulometric distribution 40–80 microns on working off technology of recovery of geometry extreme combs on the bandage shelf of working blades of the second step guarantees high quality of welding material (availability of defects of typemicrocracks, lack of penetrations is not revealed).

Reference list
  1. Shmotin Ju.N., Starkov R.Ju., Danilov D.V., Ospennikova O.G., Lomberg B.S. Novye materialy dlja perspektivnogo dvigatelja OAO «NPO „Saturn”» [New materials for ad-vanced engine JSC «NPO „Saturn”»] //Aviacionnye materialy i tehnologii. 2012. №2. S. 6–8.
  2. Gerasimov D.E., Razuvaev E.V. Proizvodstvo deformirovannyh polufabrikatov iz sov-remennyh i perspektivnyh zharoprochnyh nikelevyh splavov [Production of semi-finished deformed modern and advanced heat-resistant nickel alloys] /V sb. Avi-acionnye materialy i tehnologii. Vyp. «Tehnologija proizvodstva aviacionnyh metalli-cheskih materialov». M.: VIAM. 2002. S. 125–132.
  3. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharoprochnye nikelevye splavy dlja detalej gazoturbinnyh dvigatelej [High-temperature heat-resistant nickel alloys for turbine engine parts] //Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
  4. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jele-menty – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements - materials of current and future high-tech] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  5. Nerush S.V., Evgenov A.G. Proizvodstvo poroshkov pripoev i gotovyh polufabri-katov na ih osnove, a takzhe poroshkov zharoprochnyh splavov i stalej dlja addi-tivnyh tehnologij [Manufacture of solder powder and semi-finished on their basis, as well as powders heat-resistant alloys and steels for additive technologies] /V sb. dokl. nauch.-tehnich. kongressa po dvigatelestroeniju (NTKD-2012). 2012. S. 344–347.
  6. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technolo-gies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  7. Lykov P.A., Safonov E.V., Bromer K.A., Shul'c A.O. Poluchenie metallicheskih mikro-poroshkov gazodinamicheskim raspyleniem [Preparation of metal spray micropowders gasdynamic] //Vestnik Juzhno-Ural'skogo gosudarstvennogo universiteta. Ser. «Mashi-nostroenie». 2012. Vyp. 33. S. 107–112.
  8. Evgenov A.G., Nerush S.V. Tehnologija poluchenija poroshkov i polufabrikatov pripoev, issledovanie melkodispersnyh poroshkov pripoev dlja diffuzionnoj vakuumnoj pajki, poluchennyh metodom atomizacii rasplava [Technology for producing powders and semi solders study of fine powders of alloys, diffusion vacuum brazing, obtained by atomization of the melt] /V sb. materialov V Vserossijskoj nauchno-tehnicheskoj kon-ferencii molodyh specialistov. Ufa: UMPO. 2011. S. 159–162.
  9. Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Gorjunov A.V. Sovremennye tehnologii poluchenija prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokolenija [Modern technologies for bar stock of casting superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 97−105.
  10. Lykov P.A., Bromer K.A., Roshhin V.E., Bryndin S.A. Opredelenie tehnologicheskih parametrov poluchenija metallicheskih ul'tradispersnyh poroshkov [Determination of process parameters for producing a metallic ultrafine powders] //Vestnik Juzhno-Ural'skogo gosudarstvennogo universiteta. Ser. «Metallurgija». 2011. Vyp. 14. S. 17–19.
  11. Kablov E.N., Evgenov A.G., Ryl'nikov V.S., Afanas'ev-Hodykin A.N. Issledovanie melkodispersnyh poroshkov pripoev dlja diffuzionnoj vakuumnoj pajki, poluchennyh metodom avtomizacii rasplava [Investigation of fine powders of alloys, diffusion vacu-um brazing obtained by melt avtomizatsii] //Vestnik MGTU im. N.Je. Baumana. Ser «Mashinostroenie». 2011. №SP2. S. 79–87.
  12. Ospennikova O.G., Evgenov A.G., Nerush S.V., Afanas'ev-Hodykin A.N. Issledovanie melkodispersnyh poroshkov pripoev na nikelevoj osnove primenitel'no k polucheniju vysokotehnologichnogo polufabrikata v vide samoklejushhejsja lenty na organicheskom svjazujushhem [Investigation of fine solder powder nickel-based high-tech applied to obtain a semi-adhesive tape on the organic binder] //Vestnik UGATU. 2012. №5 (50). S. 137–144.
  13. Ospennikova O.G. Strategija razvitija zharoprochnyh splavov i stalej special'nogo naznachenija, zashhitnyh i tehnologicheskih pokrytij [The development strategy of sup-eralloys and special steel, protective coatings and technological] //Aviacionnye materialy i tehnologii. 2012. №S. S. 19–36.
  14. Lykov P.A., Roshhin V.E., Vorob'ev E.I. Vlijanie tehnologicheskih parametrov raspyl-enija metallicheskih rasplavov na granulometricheskij sostav poroshka i formu chastic poroshka [Effect of process parameters on the melt spraying of metal powder particle size distribution and shape of the powder particles] //Izvestija vuzov. Ser. «Chernaja metallurgija». 2012. №6. S. 21–23.
  15. Bersenev A.G., Logunov A.V., Logacheva A.I. Problemy povyshenija kachestva zharoprochnyh splavov, poluchaemyh metodom metallurgii granul [Problems of im-proving the quality of high-temperature alloys, obtained by granule metallurgy] //Vestnik MAI. 2008. T. 15. №3. S. 83–89.
  16. Safronov V.P., Rytov N.N., Jeskin G.I., Solujanov Ju.F. Sovershenstvovanie tehnologii gazostrujnogo raspylenija rasplava [Improving technology gas-jet spray melt] /V sb. statej «Metallurgija granul». Vyp. 1. M.: VILS. 1983. S. 59–63.
  17. Anuchin P.S., Shherbakov A.I., Kalicev V.A. i dr. Osobennosti proizvodstva zharo-prochnyh poroshkovyh pripoev [Features production of heat-resistant powder solders] /V sb. statej «Metallurgija granul». Vyp. 1. M.: VILS. 1983. S. 154–159.
  18. Kablov E.N., Petrushin N.V., Bronfin M.B., Alekseev A.A. Osobennosti mono-kristallicheskih zharoprochnyh nikelevyh splavov, legirovannyh reniem [Features single-crystal high-temperature nickel alloys alloyed with rhenium] //Metally. 2006. №5. S. 47–57.
  19. Kablov E.N., Svetlov I.L., Petrushin N.V. Nikelevye zharoprochnye splavy dlja lit'ja lopatok s napravlennoj i monokristallicheskoj strukturoj [Nickel superalloys for blades casting with directional and single-crystal structure]. Ch. II //Materialovedenie. 1997. №5. S. 14–16.