Aluminium casting alloys (on the 100th anniversary of the birth of M.B. Altman)

Goncharenko E.S., Trapeznikov A.V., Ogorodov D.V.
Goncharenko E.S., Trapeznikov A.V., Ogorodov D.V. Aluminium casting alloys (on the 100th anniversary of the birth of M.B. Altman) // Proceedings of VIAM. 2014. No. 4. DOI: 10.18577/2307-6046-2014-0-4-2-2. URL: https://viam-works.ru/en/journal/2014/4/2
Abstract

The article describes the main methods of refining and modification of cast aluminum alloys proposed by M.B. Altman. The basic theoretical and scientific-technical provisions are quoted, systematized M.B. Altman. The classification of casting aluminium alloys on purpose were considered, dynamics of their development were shown. Modern casting aluminium alloys with high manufacturability and improved me-chanical properties were presented, as well as perspective directions of development of foundry of aluminium alloys in the coming years.

Reference list
  1. Kolobnev I.F., Al'tman M.B. Gazovaja poristost' i metody bor'by s nej v aljuminievyh otlivkah [Gas porosity and methods of combating it in aluminum castings]. M.: ITJeIN. 1948. 48 s.
  2. Al'tman M.B., Lebedev A.A., Chuhrov M.V. Plavka i lit'e legkih splavov [Melting and casting of light alloys]. M.: Metallurgija. 1969. 680 s.
  3. Al'tman M.B., Stromskaja N.P. Povyshenie svojstv standartnyh litejnyh aljuminievyh splavov [Raising the standard properties of cast aluminum alloys]. M.: Metallurgija. 1984. 128 s.
  4. Jeskin G.I. Ul'trazvukovaja obrabotka rasplavlennogo aljuminija [Ultrasonic treatment of molten aluminum]. M.: Metallurgija. 1965. 224 s.
  5. Al'tman M.B. Nemetallicheskie vkljuchenija v aljuminievyh splavah [Non-metallic in-clusions in aluminum alloys]. M.: Metallurgija. 1965. 127 s.
  6. Al'tman M.B. Metallurgija litejnyh aljuminievyh splavov [Metallurgy of cast aluminum alloys]. M.: Metallurgija. 1972. 153 s.
  7. Branchukov D.N., Panfilov A.V. Rafinirovanie aljuminievyh splavov novymi kombinirovannymi fljusami [Refining aluminum alloys combined with new fluxes] //Vse materialy. Jenciklopedicheskij spravochnik. 2009. №3. S. 10–15.
  8. Kolobnev I.F. Termicheskaja obrabotka aljuminievyh splavov [Heat treatment of alumi-num alloys]. M.: Metallurgija. 1966. 394 s.
  9. Kolobnev I.F. Zharoprochnost' litejnyh aljuminievyh splavov [Heat resistance of cast aluminum alloys]. M.: Metallurgija. 1973. 320 s.
  10. Lebedev V.M., Mel'nikov A.V., Postnikov N.S., Cherkasov V.V. Vysokojeffektivnye litejnye aljuminievye splavy [High-performance aluminum casting alloys] /V sb.: Aviacionnye materialy na rubezhe XX–XXI vekov. M.: VIAM. 1994. S. 101–105.
  11. Aristova N.A., Kolobnev I.F. Termicheskaja obrabotka litejnyh aljuminievyh splavov [Heat treatment of cast aluminum alloys]. M.: Metallurgija. 1977. 144 s.
  12. Goncharenko E.S., Kornysheva I.S. Litejnyj aljuminievyj splav AL4MS dlja agregatnogo lit'ja [Foundry aluminum alloy casting for an aggregate AL4MS] //Tehnologija legkih splavov. 2009. №3. S. 99–101.
  13. Goncharenko E.S., Kornysheva I.S. Aviacionnye otlivki, poluchennye lit'em po gazificiruemym modeljam [Aviation casting obtained by casting on gasified models] //Litejnoe proizvodstvo. 2011. №6. S. 21–23.
  14. Gao Chengksun i dr. Lit'e po gazificiruemym modeljam otlivok iz aljuminievyh splavov [Lost foam casting of aluminum alloy castings] //Lit'e i cvetnye splavy. 2010. T. 30. №8. S. 746–747.
  15. Goncharenko E.S., Kornysheva I.S. Perspektivy primenenija otlivok iz aljuminievyh splavov [Prospects of application of aluminum alloy castings] //Litejnoe proizvodstvo. 2012. №1. S. 21–23.
  16. Goncharenko E.S., Kornysheva I.S. Otlivki iz aljuminievyh splavov. Issledovanija, materialy, tehnologii [Casting of aluminum alloys. Research, materials, technology] //Litejnoe proizvodstvo. 2013. №2. S. 2–4.
  17. Dujunova V.A., Goncharenko E.S., Muhina I.Ju., Uridija Z.P., Volkova E.F. Nauchnoe nasledie akademika I.N. Fridljandera. Sovremennye issledovanija magnievyh i litejnyh aljuminievyh splavov [Scientific Heritage of Academician I.N. Friedlander. Modern studies of magnesium and aluminum alloy casting] //Cvetnye metally. 2013. №9. S. 71–78.
  18. Stepanov A.V., Kosarina E.I., Savvina N.A., Usachev V.E. Makro- i mikroporistost' v splavah na osnove aljuminija i nikelja, obnaruzhenie ee rentgenoskopicheskimi metodami nerazrushajushhego kontrolja [Macro- and micro-porosity in alloys based on aluminum and nickel, her discovery of X-ray non-destructive testing] //Aviacionnye materialy i tehnologii. 2012. №S. S. 423–430.
  19. Chirkov E.F. Temp razuprochnenija pri nagrevah – kriterij ocenki zharoprochnosti konstrukcionnyh splavov sistem Al–Cu–Mg i Al–Cu [Temp softening when heated – evaluation criterion resistance of building systems alloys Al–Cu–Mg and Al–Cu] //Aviacionnye materialy i tehnologii. 2013. №S2. S. 11–19.
  20. Kablov E.N. Osnovnye itogi i napravlenija razvitija materialov dlja perspektivnoj aviacionnoj tehniki [Main outcomes and directions of development of materials for advanced aircraft] /V sb. 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: Jubilejnyj nauch.-tehnich. sb. M. VIAM. 2007. S. 20–26.
  21. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  22. Kornysheva I.S., Volkova E.F., Goncharenko E.S., Muhina I.Ju. Perspektivy primenen-ija magnievyh i litejnyh aljuminievyh splavov [Prospects of application of magnesium and aluminum alloy casting] //Aviacionnye materialy i tehnologii. 2012. №S. S. 212–222.
  23. Antipov V.V. Strategija razvitija titanovyh, magnievyh, berillievyh i aljuminievyh splavov [The development strategy of titanium, magnesium, beryllium and aluminum alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
  24. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i vysokih tehnologij budushhego [Rare metals and rare earth elements – modern materials and high-tech future] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  25. Semenov B.I., Kushtarov K.M. Proizvodstvo izdelij iz metalla v tverdozhidkom sostojanii [Manufacture of metal in the solid-liquid state]. M.: Izd-vo MGTU im. N.Je. Baumana. 2010. 223 s.