Sidorov V.V., Rigin V.E., Filonova E.V., Timofeeva O.B. The structure investigations and properties of VGM4-VI and VGM5-VI single crystal alloys with increased phosphorus quantity // Proceedings of VIAM. 2014. No. 3. DOI: 10.18577/2307-6046-2014-0-3-2-2. URL: https://viam-works.ru/en/journal/2014/3/2
Keywords
phosphorus, lanthanum, structure, st
Abstract

The effect of phosphorus impurity on structure transformation and stress rupture properties of VGM4-VI and VGM5-VI single crystal alloys was investigated. It was es-tablished that a phosphorus at increased content (above 0,01%) reduces the stress rup-ture properties. Using the scanning electron microscope method it was established that a phosphorus at increased content (above 0,01%) increases a quantity of microcracks near rupture place, favours more intensive proceeding the process of hardenable γ'-phase coagulation, enriches the areas near eutectic γ'-phase and favours melt of the structure components at heat treamtent. For neutralization of harmful phosphorus influence in alloys the rear earth metal – lanthanum application is effective.

Reference list
  1. Kablov E.N., Sidorov V.V., Rigin V.E., Gorjunov A.V. Sovremennye tehnologii poluchenija prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokolenija [Modern technologies for bar stock of casting superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. C. 97–105.
  2. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokolenija [Casting nickel superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36–51.
  3. Kablov D.E., Sidorov V.V., Min P.G. Vlijanie primesi azota na strukturu monokristallov zharoprochnogo nikelevogo splava ZhS30-VI i razrabotka jeffektivnyh sposobov ego rafinirovanija [Influence of nitrogen impurities on the structure of single-crystal superal-loy nickel alloy ZHS30-VI and develop effective ways of refining its] //Aviacionnye materialy i tehnologii. 2012. №2. S. 32–36.
  4. Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E., Kablov D.E. Osobennosti tehnologii vyplavki i razlivki sovremennyh litejnyh vysokozharoprochnyh nikelevyh splavov [Technology features modern smelting and casting casting nickel-base superalloys] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. Spec. vyp. «Perspektivnye konstrukcionnye materialy i tehnologii». S. 68–78.
  5. Sidorov V.V., Rigin V.E., Gorjunov A.V., Kablov D.E. Vysokojeffektivnye tehnologii i sovremennoe oborudovanie dlja proizvodstva shihtovyh zagotovok iz litejnyh zharo-prochnyh splavov [Enabling technologies and modern equipment for production of charge billets casting superalloys] //Metallurg. 2012. №5. S. 26–30.
  6. Kablov D.E., Chabina E.B., Sidorov V.V., Min P.G. Issledovanie vlijanija azota na strukturu i svojstva monokristallov iz litejnogo zharoprochnogo splava ZhS30-VI [In-vestigation of the influence of nitrogen on the structure and properties of single crystals of cast superalloy ZHS30-VI] //MiTOM. 2013. №8. S. 3–7.
  7. Kablov D.E., Beljaev M.S., Sidorov V.V., Komarova T.I. Issledovanie vlijanija primesi azota na malociklovuju ustalost' monokristallov zharoprochnogo nikelevogo splava ZhS30-VI [Investigation of the influence of nitrogen impurity on the low-cycle fatigue of single crystals heat-resistant nickel alloy ZHS30-VI] //MiTOM. 2012. №7. S. 46–47.
  8. Yaoxiao Zhu, John Radavich et al. The development and Long-Time Structual Stadility of a Low Segregation Hf Free Supperalloy – DZ 125 /In: Superalloys-2000. 2000. P. 329–339.
  9. Chao Yuan, Fengshi Yin et al. Effect of Phosphorus on Microstructore and High Temperature Properties of a Cast Ni-base Supperalloy //J. Mater. Sci. Technol. 2002. V. 18. №6. P. 555–557.
  10. Zhuanggi H.V., Hongwei Song et al. Effect of Phosphorus on Microstructore and Creep Property of IN718b Superalloy //J. Mater. Sci. Technol. 2005. V. 21. P. 73–76.
  11. Kablov E.N., Petrushin N.V., Morozova G.I., Svetlov I.L. Fiziko-himicheskie faktory zharoprochnosti nikelevyh splavov, soderzhashhih renij [Physico-chemical factors of heat resisting nickel alloys containing rhenium] /V sb. Aviacionnye materialy i tehnologii. Vyp. «Vysokorenievye zharoprochnye splavy, tehnologii i oborudovanie dlja proizvodstva splavov i lit'ja monokristallicheskih turbinnyh lopatok GTD». M.: VIAM. 2004. S. 37–47.
  12. Kablov E.N., Svetlov I.L., Petrushin N.V. Nikelevye zharoprochnye splavy, legirovannye ruteniem [Nickel superalloys, ruthenium doped] /V sb. Aviacionnye materialy i tehnologii. Vyp. «Vysokorenievye zharoprochnye splavy, tehnologii i oborudovanie dlja proizvodstva splavov i lit'ja monokristallicheskih turbinnyh lopatok GTD». M.: VIAM. 2004. S. 80–90.
  13. Kablov E.N., Bondarenko Ju.A., Kablov D.E. Osobennosti struktury i zharoprochnyh svojstv monokristallov 001> vysokorenievogo nikelevogo zharoprochnogo splava, poluchennogo v uslovijah vysokogradientnoj napravlennoj kristallizacii [Structure and properties of single crystals of high-temperature 001> high-rhenium nickel superalloy prepared under the high-gradient directional crystallization] //Aviacionnye materialy i tehnologii. 2011. №4. S. 25–31.
  14. Kablov E.N., Bondarenko Ju.A., Echin A.B., Surova V.A. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [The development process of directional solidification of GTE blades with single crystal superalloys and composite structure] //Aviacionnye materialy i tehnologii. 2012. №1. S. 3–8.
  15. Kablov E.N., Sidorov V.V. Mikrolegirovanie RZM – sovremennaja tehnologija povyshenija svojstv litejnyh zharoprochnyh nikelevyh splavov [Microalloying REM - modern technology enhancing properties of cast heat-resistant nickel alloys] //Perspektivnye materialy. 2001. №1. S. 23–24.
  16. Sidorov V.V., Timofeeva O.B., Kalicev V.A., Gorjunov A.V. Vlijanie mikrolegirovanija RZM na svojstva i strukturno-fazovye prevrashhenija v intermetallidnom splave VKNA-25-VI [Effect of microalloying REM on properties and structural phase transi-tions in the intermetallic alloy VKNA-25-VI] //Aviacionnye materialy i tehnologii. 2012. №4. S. 8–13.
  17. Harris G.K., Wahl J.B. Development in supperalloy castability and new applications for advanced supperalloys //Materials Science and Technology. 2009. V. 25. №2. P. 147–153.
  18. Gorjunov A.V., Sidorov V.V., Rigin V.E., Zajcev D.V. Formirovanie nanostrukturirovannogo sostojanija v litejnom zharoprochnom splave VZhM4-VI pri mikrolegirovanii ego lantanom [Formation of nanostructured state in casting superalloy VZHM4-VI in his microalloying lanthanum] //Aviacionnye materialy i tehnologii. 2013. №3. S. 39–43.
  19. Sidorov V.V., Goryunov A.V., Kolmakova N.A. Effect of lanthanum on the high-temperature strength of single-crystals of highly refractory alloy VZhM4-VI containing rhenium and ruthenium //Metal science and heat treatment. 2012. V. 54. №3–4. R. 126–130.
  20. Pang H.T., Edmonds I.M., Jones C.N., Stone H.J., Rae C.M. Effect of Y and La additions on the processing and properties of a second generation single crystal nickel-base supperalloy CMSX-4 /In: Supperalloys-2012: International symposium on supperalloys. 2012. P. 301–310.
  21. Sidorov V.V., Rigin V.E., Zajcev D.E., Gorjunov A.V. Formirovanie nanostrukturirovannogo sostojanija v litejnom zharoprochnom splave pri mikrolegirovanii ego lantanom [Formation of nanostructured state in casting superalloy with microalloying its lanthanum] //Trudy VIAM. 2013. №1. St. 01 (viam-works.ru).