Casting of magnesium alloys in disposable moulds produced by new methods

Leonov A.A., Duyunova V.A., Stupak E.V., Trofimov N.V.
Leonov A.A., Duyunova V.A., Stupak E.V., Trofimov N.V. Casting of magnesium alloys in disposable moulds produced by new methods // Proceedings of VIAM. 2014. No. 12. DOI: 10.18577/2307-6046-2014-0-12-1-1. URL: https://viam-works.ru/en/journal/2014/12/1
Abstract

The article considers the methods of casting of domestic castable magnesium alloys (VML18, VML20) in disposable moulds made of sand-clay mixture, cold box mixture and moulds produced by 3D-printing 3D-models of parts of the steering system com-ponents from magnesium castable VML 18 and VML 20 alloys were developed for the three-dimensional printing.

Reference list
  1. Kablov E.N. Osnovnye itogi i napravlenija razvitija materialov dlja perspektivnoj aviacionnoj tehniki [The main results and directions of development of promising materials for aircraft equipment] /V sb. 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: Jubilejnyj nauch.-tehnich. sb. M.: VIAM. 2007. S. 20–26.
  2. Kablov E.N. VIAM: prodolzhenie puti [VIAM: continuation of the path] //Nauka v Rossii. 2012. №3. S. 36–44.
  3. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials - the basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  4. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace Materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  5. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements - materials of current and future high-tech] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  6. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  7. Kornysheva I.S., Volkova E.F., Goncharenko E.S., Muhina I.Ju. Perspektivy primenenija magnievyh i litejnyh aljuminievyh splavov [Prospects for the use of magnesium and aluminum foundry alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 212–222.
  8. Goncharenko E.S., Aljab'ev I.P., Trapeznikov A.V., Ogorodov D.V. Tehnologija poluchenija fasonnyh otlivok iz tehnologicheskogo germetichnogo splava AL4MS [Technology for producing shaped castings of technological sealed alloy AL4MS] //Litejshhik Rossii. 2014. №7. S. 12–14.
  9. Goncharenko E.S., Trapeznikov A.V., Ogorodov D.V. Litejnye aljuminievye splavy (k 100-letiju so dnja rozhdenija M.B. Al'tmana) [Casting aluminum alloys (for the 100th anniversary of the birth of Mikhail Altman)] //Trudy VIAM. 2014. №4. St. 02 (viam-works.ru).
  10. Dujunova V.A., Goncharenko E.S., Muhina I.Ju. i dr. Nauchnoe nasledie akademika I.N. Fridljandera. Sovremennye issledovanija magnievyh i litejnyh aljuminievyh splavov v VIAM [Scientific Heritage of Academician I.N. Friedlander. Modern studies of magnesium and cast aluminum alloys VIAM] //Cvetnye metally. 2013. №9. S. 71–78.
  11. Korchagina V.A. Radi kachestva magnievyh otlivok [For the sake of the quality of magnesium castings] //Inzhenernaja gazeta. 2006. №33–34. S. 5.
  12. Dujunova V.A. Magnievye splavy: nauchnye issledovanija Central'nogo ajerogidrodinamicheskogo instituta i Vsesojuznogo instituta aviacionnyh materialov. 1930–1935 gg. [Magnesium alloys: research of the Central hydrodynamic Institute and the All-Union Institute of Aviation Materials. 1930-1935 years.] //Istorija nauki i tehniki. 2012. №10. S. 27–35.
  13. Karimova S.A., Pavlovskaja T.G. Razrabotka sposobov zashhity ot korrozii konstrukcij, rabotajushhih v uslovijah kosmosa [Development of methods of corrosion protection structures operating in space] //Trudy VIAM. 2013. №4. St. 02 (viam-works.ru).
  14. Kozlov I.A., Karimova S.A. Korrozija magnievyh splavov i sovremennye metody ih zashhity [Corrosion of Magnesium Alloys and modern methods of protection] //Aviacionnye materialy i tehnologii. 2014. №2. S. 15–20.
  15. Dujunova V.A. Metody zashhity magnievyh splavov v otechestvennom litejnom proizvodstve s 1930-h gg. do nastojashhego vremeni [Methods of protection of magnesium alloys in the domestic foundry with the 1930s. up to date] //Litejshhik Rossii. 2010. №10. S. 35–37.
  16. Dujunova V.A., Uridija Z.P. Issledovanie vosplamenjaemosti litejnyh magnievyh splavov sistemy Mg–Zn–Zr [Study the flammability of casting magnesium alloys Mg–Zn–Zr] //Litejshhik Rossii. 2012. №11. S. 21–23.
  17. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  18. Kablov E.N., Muhina I.Ju., Korchagina V.A. Prisadochnye materialy dlja formovochnyh smesej pri lit'e magnievyh splavov [Filler materials for molding compounds for casting magnesium alloys] //Litejnoe proizvodstvo. 2007. №5. S. 15–18.
  19. Dujunova V.A., Muhina I.Ju., Uridija Z.P. Novye protivoprigarnye prisadochnye materialy dlja litejnyh form magnievyh otlivok [New antiscorching filler materials for molds magnesium castings] //Litejnoe proizvodstvo. 2009. №9. S. 18–21.
  20. Dujunova V.A., Kozlov I.A. Holodnotverdejushhie formovochnye smesi: perspektivy ispol'zovanija pri lit'e magnievyh splavov [Cold-molding materials: prospects for the use in the casting of magnesium alloys] //Vse materialy. Jenciklopedicheskij spravochnik. 2011. №1. S. 41–43.
  21. Muhina I.Ju., Dujunova V.A., Uridija Z.P. Perspektivnye litejnye magnievye splavy [Prospective casting magnesium alloys] //Litejnoe proizvodstvo. 2013. №5. S. 2–5.
  22. Frolov A.V., Muhina I.Ju., Dujunova V.A., Uridija Z.P. Vlijanie tehnologicheskih parametrov plavki na strukturu i svojstva novyh magnievyh splavov [Effect of process parameters on the structure and melting properties of the novel magnesium alloys] //Metallurgija mashinostroenija. 2014. №2. S. 26–29.