Determination of arsenic and selenium in high-temperature nickel alloys by ICP-MS method with hydride generation of vapor

Alekseev A.V., Yakimovitch P.V.
Alekseev A.V., Yakimovitch P.V. Determination of arsenic and selenium in high-temperature nickel alloys by ICP-MS method with hydride generation of vapor // Proceedings of VIAM. 2014. No. 11. DOI: 10.18577/2307-6046-2014-0-11-9-9. URL: https://viam-works.ru/en/journal/2014/11/9
Abstract

Now in the modern aviation industry and engine-manufacturing high - temperature nickel alloys, subjecting to huge thermal and power loadings are widely used. Arsenic and selenium presence in nickel alloys leads to catastrophic deterioration of their phys-ical and mechanical properties. In this paper a determination of arsenic and selenium in standard samples of nickel alloys was carried out by mass spectrometry with inductively coupled plasma (ICP-MS), combined with a hydride vapor generation. A technique of dissolution of the probe and its preparation for analysis is given. Spectral interferences were eliminated by separation of the elements determined, using hydrides formation. The detection limit was 0,00001% Se by mass, 0,000005% As by mass, range of determined concentrations: of 0,00006–0,0012% by mass, relative standard deviation of less than 0,05.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Mazalov I.S., Filonova E.V., Lomberg B.S. Formirovanie struktury pri deformacii i termicheskoj obrabotke zagotovok detalej iz nikelevogo vysokoprochnogo svarivaemogo splava VZh172 [The formation of structure in the deformation and heat-treated blanks of high-nickel alloy welded VZH172] //Trudy VIAM. 2013. №12. St. 01 (viam-works.ru).
  3. Kablov E.N., Svetlov I.L., Petrushin N.V. Nikelevye zharoprochnye splavy dlja lit'ja lopatok s napravlennoj i monokristallicheskoj strukturoj [Nickel superalloys for blades casting with directional and single-crystal structure] (Chast' I) //Materialovedenie. 1997. №4. S. 32–39.
  4. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharoprochnye nikelevye splavy dlja detalej gazoturbinnyh dvigatelej [High-temperature heat-resistant nickel alloys for turbine engines parts] //Aviacionnye materialy i tehnologii. 2012. №S. C. 52–57.
  5. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokolenija [Casting nickel superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36–52.
  6. Min P.G., Sidorov V.V. Opyt pererabotki litejnyh othodov splava ZhS32-VI na nauchno-proizvodstvennom komplekse VIAM po izgotovleniju lityh prutkovyh (shihtovyh) zagotovok [Experience in processing of waste foundry alloy ZhS32-VI at the scientific-industrial complex for the production of cast VIAM of bar (charge) blanks] //Aviacionnye materialy i tehnologii. 2013. №4. S. 20–25.
  7. Ponomarenko D.A., Moiseev N.V., Skugorev A.V. Proizvodstvo diskov GTD iz zharoprochnyh splavov na izotermicheskih pressah [Production GTE disks of superalloys isothermal presses] //Aviacionnye materialy i tehnologii. 2013. №1. S. 13–16.
  8. Kablov E.N., Bondarenko Ju.A., Echin A.B., Surova V.A. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [The development process of directional solidification of gas turbine engine blades with a single-crystal superalloys and composite structure] //Aviacionnye materialy i tehnologii. 2012. №1. S. 3–8.
  9. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements – materials for current and future high-tech] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  10. Kablov E.N., Ospennikova O.G., Lomberg B.S. Kompleksnaja innovacionnaja tehnologija izotermicheskoj shtampovki na vozduhe v rezhime sverhplastichnosti diskov iz superzharoprochnyh splavov [Integrated innovative technology isothermal forging in air superplasticity disks from super heat-resistant alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 129–141.
  11. Liu H., Chen S. at al. Determination of bismuth, selenium andtellurium in nickel-based alloys and pure copper by flow-injection hydride generation atomic absorption spec-trometry with ascorbic acid prereduction and cupferron chelation extraction //Analytica Chimica Acta. 2002. V. 459. P. 161–168.
  12. Chen Z. and Jiang S. Determination of Ge, As and Se in nickel-based alloys by flow injection hydride generation dynamic reaction cell inductively coupled plasma mass spec-trometry//J. Anal. At. Spectrom. 2006.V. 21. P. 566–573.
  13. GOST 6689.13–92. Nikel', splavy nikelevye i medno-nikelevye. Metody opredelenija mysh'jaka [Nickel, nickel and copper-nickel. Methods defined division of arsenic].
  14. GOST 13047.25–2002. Nikel'. Kobal't. Metody opredelenija selena v nikele [Nickel. Cobalt. Methods for determination of selenium in nickel].
  15. Pupyshev A.A., Jepova E.N. Spektral'nye pomehi poliatomnyh ionov v metode mass-spektrometrii s induktivno svjazannoj plazmoj [Spectral interferences of polyatomic ions in the method of mass spectrometry with inductively coupled plasma] //Analitika i kontrol'. 2001. T.5. №4. S. 335–369.
  16. D’Ilio S., Violante N. at al. Dynamic reaction cell ICP-MS for determination of total As, Cr, Se and V in complex matrices: Still a challenge? (a review)//Analytica Chimica Acta. 2011.V. 698. P. 6–13.
  17. Gao Y., Liu R. at al. Application of chemical vapor generation in ICP-MS: A review //Chinа Sci. Bull. 2013. V. 58. №8. P. 1980–1991.
  18. Guo X., Xu S. at al. Determination of As, Pb, Sn, Sb and Bi in high temperature iron and nickel-based alloy by graphite furnace atomic absorption spectrometry combined with liquid-liquid extraction //Spectroscopy and spectral analysis. 2006. V. 6. P. 1167–1169.
  19. Campbell A.D. A critical survey of hydride generation techniquesin atomic spectroscopy //Pure &Appl. Chem. 1992. V. 64. №2. P. 227–244.
  20. Danadurai K., Hsu Y. Determination of selenium in nickel-based alloys by flow injection hydride generation reaction cell inductively coupled plasma mas-spectrometry //J. Anal. At. Spectrom. 2002. V.17. P. 552–555.
  21. Chen Z. and Jiang S. Determination of Ge, As and Se in nickel-based alloys by flow injection hydride generation dynamic reaction cell inductively coupled plasma mass spectrometry //J. Anal. At. Spectrom. 2006. V. 21. P. 566–573.
  22. Nie X., Liang Y. Determination of trace elements in high purity nickel by high resolution inductively coupled plasma mass spectrometry //J. Cent. South Univ. 2012. V. 19. P. 2416−2420.
  23. Ganeev A.A., Gubal' A.R., Uskov K.N., Potapov S.V. Analiticheskaja mass-spektrometrija s tlejushhim razrjadom [Analytical mass spectrometry with a glow discharge] //Izvestija Akademii nauk. Ser. Himicheskaja. 2012. №4. S. 1–17.
  24. Jakubenko E.V., Vojtkova Z.A., Chernikova I.I., Ermolaeva T.N. Mikrovolnovaja probopodgotovka dlja opredelenija Si, P, V, Cr, Mn, Ni, Cu, W metodom AJeS-ISP v konstrukcionnyh staljah [Microwave sample preparation for the determination of Si, P, V, Cr, Mn, Ni, Cu, W by ICP-AES in structural steels] //Zavodskaja laboratorija. Diagnostika materialov. 2014. T. 80. №1. S. 12–15.
  25. Dvoreckov R.M., Karachevcev F.N., Zagvozdkina T.N., Mehanik E.A. Opredelenie legirujushhih jelementov nikelevyh splavov aviacionnogo naznachenija metodom AJeS-ISP v sochetanii s mikrovolnovoj probopodgotovkoj [Determination of alloying elements nickel alloys for aircraft industry by AES-ICP in combination with microwave sample preparation] //Zavodskaja laboratorija. Diagnostika materialov. 2013. T. 79. №9. S. 6–9.