Influence of air oxygen and thickness of salt deposits on corrosion cracking of titanium alloys at high temperatures in contact with NaCl

Zakharova L.V.
Zakharova L.V. Influence of air oxygen and thickness of salt deposits on corrosion cracking of titanium alloys at high temperatures in contact with NaCl // Proceedings of VIAM. 2014. No. 10. DOI: 10.18577/2307-6046-2014-0-10-12-12. URL: https://viam-works.ru/en/journal/2014/10/12
Abstract

Titanium alloys find a wide application in aircraft equipment operating in all-climatic conditions, where a sea salt deposition on their surface causing hot salt corrosion at raised temperatures (≥250°C) is possible. An influence of salt deposits thickness on corrosion cracking of titanium alloys under conditions of raised temperatures and stretching or alternating loads and also a role of air oxygen in the course of hot salt cor-rosion was studied in this work. As a result of the conducted researches it was established that oxygen of air takes an active part in the process of hot salt corrosion and the main component of hard products of corrosion is TiO2. It was shown that thickness of salt deposits has an impact on cracking resistance of titanium alloys at high temperatures under loads and salt layers of ~50 microns of thickness have the highest aggression.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials - the basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  3. Karimova S.A., Pavlovskaja T.G. Razrabotka sposobov zashhity ot korrozii konstrukcij, rabotajushhih v uslovijah kosmosa [Development of methods of corrosion protection structures operating in the space environment] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 35–40.
  4. Kablov E.N. Materialy dlja izdelija «Buran» – innovacionnye reshenija formirovanija shestogo tehnologicheskogo uklada [Materials for the product «Buran» – innovative solutions forming the sixth technological order] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  5. Horev A.I. Fundamental'nye i prikladnye raboty po titanovym splavam dlja «Burana» i perspektivnye napravlenija ih razvitija [Fundamental and applied research in titanium alloys for «Buran» and future directions of their development] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 10–14.
  6. Horev A.I., Belov S.P., Glazunov S.G. Metallovedenie titana i ego splavov [Physical metallurgy of titanium and its alloys]. M.: Metallurgija. 1992. 352 s.
  7. Kashapov O.S., Novak A.V., Nochovnaja N.A., Pavlova T.V. Sostojanie, problemy i perspektivy sozdanija zharoprochnyh titanovyh splavov dlja detalej GTD [Status, problems and prospects for the creation of high-temperature titanium alloys for GTD parts] //Trudy VIAM. 2013. №3. St. 02 (viam-works.ru).
  8. Horev A.I. Fundamental'nye i prikladnye raboty po konstrukcionnym titanovym splavam i perspektivnye napravlenija ih razvitija [Fundamental and applied research in structural titanium alloys and future directions of their development] //Trudy VIAM. 2013. №2. St. 04 (viam-works.ru).
  9. Hopev A.I. Vlijanie kompleksnogo legipovanija na mehanicheskie svojstva svapnyh soedinenij i osnovnogo metalla (α+β)- i β-titanovyh splavov [Influence of complex legipovaniya on the mechanical properties of the welded joints and base metal (α+β)- and β-titanium alloys] //Tehnologija mashinostroenija. 2007. №2. S. 29–34.
  10. Solonina O.P., Glazunov S.G. Titanovye splavy. Zharoprochnye titanovye splavy [Titanium alloys. Heat-resistant titanium alloys]. M.: Metallurgija. 1976. 448 s.
  11. Gorynin I.V., Ushakov S.S., Hatuncev A.N., Loshakova I.L. Titanovye splavy dlja morskoj tehniki [Titanium alloys for marine equipment]. SPb.: Politehnika. 2007. 387 s.
  12. Sinjavskij S.V. Soprotivlenie titanovyh splavov razlichnym vidam korrozionnogo rastreskivanija [Resistance of titanium alloys, various types of stress-corrosion cracking] //Tehnologija legkih splavov. 2010. №4. S. 80–85.
  13. Li S.Q., Lei J.F., Liu Y.-Y., Yu B.-X., Li Y.-L., Yang R. Fushi Kexue yu Fandhu Jishu. Hot-salt stress corrosion of titanium alloys of Ti811 and TC4 //Corros. Sci. And Prol. Tehnol. 2010. V. 22. №2. P. 79–84.
  14. Bacos M.-P., Thomas M., Raviart J.-L., Morel A., Mercier S., Josso P. Influence of an oxidation protective coating upon hot corrosion and mechanical behavior of Ti–48Al–2Cr–2Nb alloy //Intermetallics. 2011. V. 19. №8. P. 1120–1129.
  15. Yingun Hua, Yuchuan Bai, Yunxia Ye, Qing Xue, Haixie Liu, Ruifang Chen, Kangmin Chen. Hot corrosion behavior of TC11 titanium alloy treated by laser shock processing //Applied Surface Science. 2013. V. 283. №15. P. 775–780.
  16. Xiong Y., Zhu S., Wang F. Synergistic corrosion behavior of coated Ti60 alloys with NaCl deposit in moist air at elevated temperature //Corros. Sci. 2008. V. 50. P. 15–22.
  17. Ulrich Zwicker. Titan und Titanlegierungen. Springer-Verlag Berlin. Heidelberg. New York. 1974. 512 p.