Modeling of technological process of PCM on a base of VSE-21 resin and Tenax-E style 450 fabric manufacture by infusion method

Goncharov V.A., Sorokin K.V., Fedotov M.Y., Raskutin A.E.
Goncharov V.A., Sorokin K.V., Fedotov M.Y., Raskutin A.E. Modeling of technological process of PCM on a base of VSE-21 resin and Tenax-E style 450 fabric manufacture by infusion method // Proceedings of VIAM. 2014. No. 10. DOI: 10.18577/2307-6046-2014-0-10-4-4. URL: https://viam-works.ru/en/journal/2014/10/4
Abstract

A sequence of operations for modeling of PCM based on VSE-21 resin and Tenax-E Style 450 fabric manufacture by infusion method is described. Phenomenological processes appearing at forming and also critical characteristics which have to be taken into account during the imitation process are given. Abilities of modeling usage for forming parameters identification even on the stage of calculation and algorithm of model realization to get a high convergence during modeling are described.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies for aircraft equipment] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  3. Kablov E.N., Karimova S.A., Semenova L.V. Korrozionnaja aktivnost' ugleplastikov i zashhita metallicheskih silovyh konstrukcij v kontakte s ugleplastikom [Corrosiveness CFRP and protection of metal bearing structures in contact with the carbon fiber] //Korrozija: materialy, zashhita. 2011. №12. S. 1–7.
  4. Kablov E.N. Korrozija ili zhizn' [Corrosion or life] //Nauka i zhizn'. 2012. №11. S. 16–21.
  5. Raskutin A.E., Goncharov V.A. Komp'juternoe modelirovanie tehnologicheskogo processa izgotovlenija PKM metodom vakuumnoj infuzii [Computer simulation of the technological process of RMB by vacuum infusion] //Aviacionnye materialy i tehnologii. 2012. №S. S. 286–291.
  6. Dushin M.I., Muhametov R.R., Platonov A.A., Merkulova Ju.I. Issledovanie fil'tracionnyh harakteristik armirujushhih napolnitelej i svjazujushhih pri razrabotke tehnologii bezavtoklavnogo formovanija polimernyh kompozicionnyh materialov [Study of the filtration characteristics of reinforcing fillers and binders in the development of technology bezavtoklavnogo molding of polymer composites] //Aviacionnye materialy i tehnologii. 2013. №2. S. 22–25.
  7. Grigor'ev M.M., Kogan D.I., Tverdaja O.N., Panina N.N. Osobennosti izgotovlenija PKM metodom RFI [Peculiarities of RMB by RFI] //Trudy VIAM. 2013. №4. St. 03 (viam-works.ru).
  8. Sokolov I.I., Raskutin A.E. Ugleplastiki i stekloplastiki novogo pokolenija [Carbon and fiberglass new generation] //Trudy VIAM. 2013. №4 (viam-works.ru).
  9. Dushin M.I., Hrul'kov A.V., Muhametov R.R., Chursova L.V. Osobennosti izgotovlenija izdelij iz PKM metodom propitki pod davleniem [Features the manufacture of RMB by pressure impregnation] //Aviacionnye materialy i tehnologii. 2012. №1. S. 24–33.
  10. Mihajlin Ju.A. Konstrukcionnye polimernye kompozicionnye materialy Structural polymer composite materials [Structural polymer composite materials]. SPb.: Nauchnye osnovy i tehnologii. 2008. 822 s.
  11. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. III. Znachimye faktory starenija [Climatic aging of composite materials for aircraft industry. III. Significant factors of aging] //Deformacija i razrushenie materialov. 2011. №1. S. 34–40.
  12. Kirillov V.N., Starcev O.V., Efimov V.A.Klimaticheskaja stojkost' i povrezhdaemost' polimernyh kompozicionnyh materialov, problemy i puti reshenija [Weather resistance and a defect of polymeric composite materials, problems and solutions] //Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.
  13. Kirillov V.N., Efimov V.A., Shvedkova A.K., Nikolaev E.V.Issledovanie vlijanija klimaticheskih faktorov i mehanicheskogo nagruzhenija na strukturu i mehanicheskie svojstva PKM [Investigation of the influence of climatic factors and mechanical loading on the structure and mechanical properties of the PCM] //Aviacionnye materialy i tehnologii. 2011. №4. S. 41–45.
  14. Chursova L.V., Dushin M.I., Kogan D.I., Panina N.N., Kim M.A., Gurevich Ja.M., Platonov A.A. Plenochnye svjazujushhie dlja RFI-tehnologii [Film binders for RFI-technology] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 63–66.
  15. Goncharov V.A., Shienok A.M., Sorokin K.V., Fedotov M.Ju., Zelenskij P.V. Modelirovanie infuzionnyh tehnologij izgotovlenija sloistyh polimernyh kompozicionnyh materialov [Simulation of infusion technology manufacturing laminates of polymer composite materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2013. №1.
  16. S. 43–49.
  17. Goncharov V.A., Fedotov M.Ju., Sorokin K.V., Raskutin A.E. Modelirovanie stadii propitki poluchenija ugleplastikov na osnove jepoksidnyh svjazujushhih dlja RTM i VARTM tehnologij [Modeling of the impregnation step, obtaining carbon-fiber epoxy binders for RTM and VARTM technology] //Spravochnik. Inzhenernyj zhurnal. 2013. №12. S. 24–28.
  18. Goncharov V.A. Modelirovanie infuzionnyh tehnologij izgotovlenija PKM na osnove jepoksidnyh svjazujushhih i uglerodnyh tkanej Porcher [Modeling infusion manufacturing techniques PCM epoxy binder and carbon fabrics Porcher] //Novosti materialovedenija. Nauka i tehnika. 2013. №5. St. 08 (materialsnews.ru).
  19. Bunakov V.A., Golovkina G.S. Armirovannye plastiki [Reinforced plastics]. M.: MAI. 1997. 404 s.
  20. Koefoed M.S. Modeling and Simulation of the VARTM Process for Wind Turbine Blades. Industrial Ph.D. Dissertation. 2003. P. 5–10.
  21. Weitzenbock J.R., Shenoi R.A., Wilson P.A. Radial flow permeability measurement. Part А: Theory. Composites Part A: Applied Science and Manufacturing. 1999. V. 30(6). Р. 781–796.
  22. Kotov V.V. Modelirovanie proizvodstva kompozicionnyh materialov – vyzov vremeni [Modeling of composite materials – call time] //Perspektivnye materialy dlja aviakosmicheskoj promyshlennosti. 2011. №1. S. 21–23.
  23. Mastbergen D.В. Simulation and Testing of Resin Infusion Manufacturing Processes for Large Composite Structures, SAND2006-7856P Unlimited Release Printed October. 2007. Р. 12–53.
  24. Hrul'kov A.V., Dushin M.I., Popov Ju.O., Kogan D.I. Issledovanija i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovanija PKM [Research and development and autoclave molding technology bezavtoklavnogo PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  25. Goncharov V.A., Fedotov M.Ju., Shienok A.M. Modelirovanie polimernyh kompozicionnyh materialov [Simulations of polymer composite materials] /V sb. trudov konf. «Novye materialy i tehnologii glubokoj pererabotki syr'ja – osnova innovacionnogo razvitija jekonomiki Rossii». M.: VIAM. 2010. S. 8.
  26. Goncharov V.A., Fedotov M.Ju. Modelirovanie fiziko-mehanicheskih svojstv intellektual'nogo ugleplastika s optovolokonnymi sensorami [Modeling of physical and mechanical properties of carbon fiber with fiber optic smart sensors] /V sb. materialov V Mezhdunarodnoj konferencii «Deformacija i razrushenie materialov i nanomaterialov» DFMN 2013. M. 2013. S. 822–823.
  27. Li J., Zhang C., Liang R., Wang B., Walsh S. Modeling and analysis of thickness gradient and variations in vacuum-assisted resin transfer molding process //Polymer Composites. 2008. V. 29. P. 473–482.
  28. Ouagne P., Bréard J. Continuous transverse permeability of fibrous media //Composites Part A: Applied Science and Manufacturing. 2010. V. 41. P. 22–28.
  29. Yenilmez B., Senan M., Murat Sozer E. Variation of part thickness and compaction pressure in vacuum infusion process //Composites Science and Technology. 2009.
  30. V. 69. Р. 1710–1719.
  31. Antonucci V., Esposito M., Ricciardi M. R., Raffone M., Zarrelli M., Giordano M. Permeability characterization of stitched carbon fiber preforms by fiber optic sensors //Express Polymer Letters. 2011. V. 5. P. 1075–1084.
  32. Porto J., Letzow M., Dos Santos E., Amico S., Souza J., Isoldi L. Computational modeling of RTM and LRTM processes applied to complex geometries //Engenharia Térmica (Thermal Engineering). 2012. V. 11. P. 93–99.