Abstract

This paper represents results of investigation on choosing coupling agents for carbon fibers for production of carbon fiber-reinforced plastics based on thermoplastic heat-resistant matrixes – polyarilsulfones PSF-T1 and PSF-T2. Carbon fiber-reinforced plastics (CFRP) have got a number of advanced properties – low density, high elasticity modulus, strength, heat resistance, high durability, low temperature linear expansion coefficient. The drawback of these materials is a low shear strength because of poor adhesion of binder to carbon fiber surface. Dressing of carbon fibers were made by epoxy resins solutions, polyimides, polyether oligomers, rolivsan, polysulfone etc. Influence of coupling agent nature on mechanical properties of thermoplastic heat-resistant CFRP at room (20°C) and high temperatures (160 and 185°C) is shown. Strength characteristics data are presented.

Reference list
  1. Petrova G.N., Bejder Je.Ja., Izotova T.F., Malyshenok S.V. Kompozicionnye termoplastichnye materialy – sposoby poluchenija i pererabotki [Composite thermoplastic materials – methods of obtaining and processing] //Vse materialy. Jenciklopedicheskij spravochnik. 2013. №10. S. 10–17.
  2. Bejder Je.Ja., Petrova G.N., Izotova T.F., Gureeva E.V. Kompozicionnye termoplastichnye materialy i penopoliimidy [Thermoplastic composite materials and penopoliimidy] //Trudy VIAM. 2013. №11. St. 01 (viam-works.ru).
  3. Kablov E.N. Himija v aviacionnom materialovedenii [Composite and thermoplastic materials penopoliimidy] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  4. Bejder Je.Ja., Malyshenok S.V., Petrova G.N. Kompozicionnye termoplastichnye materialy – svojstva i sposoby pererabotki [Chemistry aviation materials] //Plasticheskie massy. 2013. №7. S. 56–60.
  5. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace Materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  6. Gunjaev G.M., Chursova L.V., Komarova O.A., Gunjaeva A.G. Konstrukcionnye ugleplastiki, modificirovannye nanochasticami [Structural carbon composites modified nanoparticles] //Aviacionnye materialy i tehnologii. 2012. №S. S. 277–286.
  7. Petrova G.N., Bejder Je.Ja. Konstrukcionnye materialy na osnove armirovannyh termo-plastov [Structural materials based on reinforced thermoplastics] //Rossijskij himicheskij zhurnal. 2010. T. LІV. №1. S. 30–40.
  8. Uglerodnye volokna i uglekompozity [Carbon fiber and uglekompozity]: Per. s ang. /Pod red. Je. Fitcera. M.: Mir. 1988. 336 s.
  9. Guljaev I.N., Vlasenko F.S., Zelenina I.V., Raskutin A.E. Napravlenija razvitija termostojkih ugleplastikov na osnove poliimidnyh i geterociklicheskih polimerov [Directions of development of heat-resistant carbon-fiber-based polyimide polymers and heterocyclic] //Trudy VIAM. 2014. №1. St. 04 (viam-works.ru).
  10. Varshavskij V.Ja. Uglerodnye volokna [carbon fiber]. M.: VINITI. 2005. 498 s.
  11. Gunjaev G.M., Kablov E.N., Aleksashin V.M. Modificirovanie konstrukcionnyh ugleplastikov uglerodnymi nanochasticami [Modification of structural carbon fiber with carbon nanoparticles] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 5–11.
  12. Stepashkin A.A., Churkov D.N. i dr. Poverhnostnaja obrabotka uglerodnyh volokon [Surface treatment of carbon fibers] //Materialovedenie. 2013. №2. S. 44–50.
  13. Bejder Je.Ja., Petrova G.N., Izotova T.F., Barbot'ko S.L. Stekloplastiki na termoplastichnoj matrice [Glass-reinforced on thermoplastic matrix] //Trudy VIAM. 2013. №7. St. 03 (viam-works.ru).
  14. Doneckij K.I., Hrul'kov A.V., Kogan D.I., Belinis P.G., Luk'janenko Ju.V. Primenenie ob`emno-armirujushhih preform dlja izgotovlenija izdelij iz PKM [Application of space-reinforcing preforms for the manufacture of RMB] //Aviacionnye materialy i tehnologii. 2013. №1. S. 35–39.
  15. Dushin M.I., Hrul'kov A.V., Muhametov R.R., Chursova L.V. Osobennosti izgotovlenija izdelij iz PKM metodom propitki pod davleniem [Features manufacture of RMB by pressure impregnation] //Aviacionnye materialy i tehnolo-gii. 2012. №1. S.18–26.