Determination of phosphorus mass content (less than 0,001% wt.) in standard specimens of nickel alloys was carried out by mass-spectrometry method with inductively coupled plasma (ICP-MS). Spectral interferences were eliminated using mathematical correction equation. The technique of sample dissolving and its preparation for analysis was presented. Relative standard deviation doesn’t exceed 0,05 in the concentration range of 0,0006–0,0065% wt. A detection limit in solution is 0,7μg/l, a detection limit in alloys – 0, 0004 % wt.

Reference list
  1. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements - materials for current and future high-tech] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  2. Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Gorjunov A.V. Sovremennye tehnologii poluchenija prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokolenija [Modern technologies for bar stock of casting superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. C. 97–105.
  3. Kablov E.N., Bondarenko Ju.A., Echin A.B., Surova V.A. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [The development process of directional solidification of gas turbine engine blades with a single-crystal superalloys and composite structure] //Aviacionnye materialy i tehnologii. 2012. №1. S. 3–8.
  4. Bondarenko Ju.A., Kablov E.N. Napravlennaja kristallizacija zharoprochnyh splavov s povyshennym temperaturnym gradientom [Directional solidification of superalloys with a high temperature gradient] //MiTOM. 2002. №7. S. 20–23.
  5. Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E., Kablov D.E. Osobennosti tehnologii vyplavki i razlivki sovremennyh litejnyh vysokozharoprochnyh nikelevyh splavov [Technology features smelting and casting foundry modern nickel-base superalloys] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2.
  6. S. 68–78.
  7. Min P.G., Sidorov V.V. Opyt pererabotki litejnyh othodov splava ZhS32-VI na nauchno-proizvodstvennom komplekse VIAM po izgotovleniju lityh prutkovyh (shihtovyh) zagotovok [Experience in processing of waste foundry alloy ZhS32-VI at the scientific-industrial complex for the production of cast VIAM of bar (charge) blanks] //Aviacionnye materialy i tehnologii. 2013. №4. S. 20–25.
  8. Kashapov O.S., Novak A.V., Nochovnaja N.A., Pavlova T.V. Sostojanie problemy i perspektivy sozdanija zharoprochnyh titanovyh splavov dlja detalej GTD [State of the problem and the prospects for the creation of high-temperature titanium alloys for GTE parts] //Trudy VIAM. 2013. №3. St. 02 (viam-works.ru).
  9. Kablov E.N., Bondarenko Ju.A., Kablov D.E., Osobennosti struktury i zharoprochnyh svojstv monokristallov 001> vysokorenievogo nikelevogo zharoprochnogo splava, poluchennogo v uslovijah vysokogradientnoj napravlennoj kristallizacii [Features of the structure and properties of single crystals of high-temperature 001> vysokorenievogo nickel superalloy, obtained with high-gradient directional solidification] //Aviacionnye materialy i tehnologii. 2011. №4. S. 25–31.
  10. Kablov E.N., Petrushin N.V., Bronfin M.B., Alekseev A.A. Osobennosti monokristallicheskih zharoprochnyh nikelevyh splavov, legirovannyh reniem [Features single-crystal high-temperature nickel alloys, alloyed with rhenium] //Metally. 2006. №5. S. 47–57.
  11. Kablov D.E., Sidorov V.V., Min P.G. Vlijanie primesi azota na strukturu monokristallov zharoprochnogo nikelevogo splava ZhS30-VI i razrabotka jeffektivnyh sposobov ego rafinirovanija [Influence of nitrogen impurities on the structure of single-crystal nickel superalloys ZhS30-VI and develop effective ways of refining it] //Aviacionnye materialy i tehnologii. 2012. №2. S. 32–36.
  12. Kablov D.E., Chabina E.B., Sidorov V.V., Min P.G. Issledovanie vlijanija azota na strukturu i svojstva monokristallov iz litejnogo zharoprochnogo splava ZhS30-VI [Investigation of the influence of nitrogen on the structure and properties of single crystals of cast superalloy ZhS30-VI] //MiTOM. 2013. №8. S. 3–7.
  13. Kablov D.E., Sidorov V.V., Min P.G. Zakonomernosti povedenija azota pri poluchenii monokristallov zharoprochnogo nikelevogo splava ZhS30-VI i ego vlijanie na jekspluatacionnye svojstva [Of the behavior of nitrogen in the preparation of single crystals of heat-resistant nickel alloy ZhS30-VI and its impact on the performance of the] //MiTOM. 2014. №1. S. 8–12.
  14. Sidorov V.V., Rigin V.E., Timofeeva O.B., Min P.G. Vlijanie kremnija i fosfora na zharoprochnye svojstva i strukturno-fazovye prevrashhenija v monokristallah iz vysokozharoprochnogo splava VZhM4-VI [Effect of silicon and phosphorus on the heat-resistant properties and structural phase transitions in single crystals of a highly heat resistant alloy VZhM4-VI] //Aviacionnye materialy i tehnologii. 2013. №3. S. 32–38.
  15. Sidorov V.V., Rigin V.E., Filonova E.V., Timofeeva O.B. Strukturnye issledovanija i svojstva monokristallov splavov VZhM4-VI i VZhM5-VI, soderzhashhih povyshennye kolichestva fosfora [Structural studies of the properties of single crystals and alloys VZhM4-VI-VI and VZhM5 containing elevated levels of phosphorus] //Trudy VIAM. 2014. №3. St. 02 (viam-works.ru).
  16. Zhu Y., Radavich J. at al. The development and Long-Time structural stability of a low segregation Hf free supper alloy – DZ 125 //Supper alloys. 2000. P. 329–339.
  17. Yuan C., Yin F. at al. Effect of phosphorus on microstructure and high temperature properties of a cast Ni-base supper alloy //J. Mater. Sci. Technol. 2002. V. 18. №6.
  18. P. 555–557.
  19. Hu Z., Song H. at al. Effect of phosphorus on microstructure and creep property of In 718b supper alloy //J. Mater. Sci. Technol. 2005. V. 21. P. 73–76.
  20. GOST 6689.19–92. Nikel', splavy nikelevye i medno-nikelevye. Metody opredelenija fosfora [Nickel, nickel and copper-nickel. Methods for the determination of phosphorus].
  21. ASTM E 1917–13. Standard Test Method for Determination of Phosphorus in Nickel, Ferronickel, and Nickel Alloys by Phosphovanadomolybdate Spectrophotometry.
  22. Pupyshev A.A., Danilova D.A. Ispol'zovanie atomno-jemissionnoj spektrometrii s induktivno svjazannoj plazmoj dlja analiza materialov i produktov chernoj metallurgii [Using atomic emission spectrometry with inductively coupled plasma analysis of materials and products of ferrous metallurgy] //Analitika i kontrol'. 2007. T. 11. №2–3.
  23. S. 131–181.
  24. Jakubenko E.V., Vojtkova Z.A., Chernikova I.I., Ermolaeva T.N. Mikrovolnovaja probopodgotovka dlja opredelenija Si, P, V, Cr, Mn, Ni, Cu, W metodom AJeS-ISP v konstrukcionnyh staljah [Microwave sample preparation for the determination of Si, P, V, Cr, Mn, Ni, Cu, W by ICP-AES in structural steels] //Zavodskaja laboratorija. Diagnostika materialov. 2014. T. 80. №1. S. 12–15.
  25. Hoffmann V., Kasik M., Robinson P.K. at al. Glow discharge mass spectrometry //Anal Bioanal Chem. 2005. V. 381. P. 173–188.
  26. Finkeldei S., Staats G. ICP-MS – A powerful analytical technique for the analysis of traces of Sb, Bi, Pb, Sn and P in steel //Fresenius J. Anal Chem. 1997. V. 359. P. 357–360.
  27. Hu J., Wang H. Determination of Trace Elements in Super Alloy by ICP-MS //Mikrochim. Acta. 2001. V. 137. P. 149–155.
  28. Yang C., Jiang S. Determination of B, Si, P and S in steels by inductively coupled plasma quadrupole mass spectrometry with dynamic reaction cell //Spectrochimica Acta. Part B. 2004. V. 59. P. 1389–1394.
  29. Pupyshev A.A., Jepova E.N. Spektral'nye pomehi poliatomnyh ionov v metode mass-spektrometrii s induktivno svjazannoj plazmoj [Spectral interferences of polyatomic ions in the method of mass spectrometry with inductively coupled plasma] //Analitika i kontrol'. 2001. T. 5. №4. S. 335–369.
  30. Kovacevic M., Goessler W. аt al. Matrix effects during phosphorus determination with quadrupole inductively coupled plasma mass spectrometry //Anal. Bioanal. Chem. 2005. V. 383. P. 145–151.
  31. Microwave Sample Preparation Note: 5MT-14 (Ni–Cr Alloy). 1998. CEM Corp.
  32. Grebneva O.N., Kubrakova I.V., Kudinova T.F., Kuzmin N.M. Direct determination of trace elements in niobium, tantalum and their oxides by inductively coupled plasma atomic emission spectrometry after microwave dissolution //Spectrochimica Acta. Part B: Atomic spectroscopy. 1997. V. 52. №8. P. 1151–1159.
  33. Ganeev A.A., Gubal' A.R., Uskov K.N., Potapov S.V. Analiticheskaja mass-spektrometrija s tlejushhim razrjadom [Analytical mass spectrometry with a glow discharge] //Izvestija RAN. Ser. Himicheskaja. 2012. №4. S. 1–17.
  34. Dvoreckov R.M., Karachevcev F.N., Zagvozdkina T.N., Mehanik E.A. Opredelenie legirujushhih jelementov nikelevyh splavov aviacionnogo naznachenija metodom AJeS-ISP v sochetanii s mikrovolnovoj probopodgotovkoj [Determination of alloying elements nickel alloys for aircraft industry by ICP-AES in combination with microwave sample preparation] //Zavodskaja laboratorija. Diagnostika materialov. 2013. T. 79. №9. S. 6–9.