A. V. Losev, A. I. Gulyaev Transcrystallinity formation factors in thermoplastic composites and structural aspects of the transcrystalline layer in polyaryletherketones (review) // Proceedings of VIAM. 2026. No. 11 (165). С. 125-137. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-11-125-137.

Transcrystallinity formation factors in thermoplastic composites and structural aspects of the transcrystalline layer in polyaryletherketones (review)

A. V. Losev1, A. I. Gulyaev1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

The transcrystalline layer at the “fiber–polymer matrix” interface is a key structural component of thermoplastic composites, determining the effectiveness of interfacial interaction and the transfer of mechanical loads between the material components. Controlled formation of the transcrystalline layer is an effective tool for controlling the interfacial structure and performance properties of thermoplastic composites. Particular interest in transcrystallinity research is associated with the widespread adoption of high-temperature polymers, particularly polyaryletherketones.

Keywords
polyetheretherketone, polyetherketoneketone, crystallization, nucleation, thermoplastic, fiber–polymer, carbon fibers, interfacial layer

Reference list
  1. Kablov E.N., Semenova L.V., Petrova G.N. et al. Polymer Composite Materials with a Thermoplastic Matrix. Izvestiya vysshikh uchebnykh zavedeniy. Ser.: Khimiya i khimicheskaya tekhnologiya, 2016, vol. 59, no. 10, pp. 61–71.
  2. Kablov E.N., Sagomonova V.A., Sorokin A.E., Tselikin V.V., Gulyaev A.I. Investigation of the Structure and Properties of a Polymer Composite Material with an Integrated Vibration-Absorbing Layer. Vse materialy. Entsiklopedicheskiy spravochnik, 2020, no. 3, pp. 2–9.
  3. Gurov D.A., Pavlyukovich N.G., Tsapenko A.N. 3D printing with composite organic filament based on liquid crystal polymers and polyetheretherketone. Aviation materials and technologies, 2024, no. 4 (77), pp. 62–81. Available at: http://www.journal.viam.ru (accessed: June 14, 2026). DOI: 10.18577/2713-0193-2024-0-4-62-81.
  4. Losev A.V., Gulyaev A.I., Zhuravleva P.L., Antyufeeva N.V. Effect of isothermal annealing on the crystallinity degree of polyetherketon-eketone containing discrete carbon fibers. Trudy VIAM, 2026, no. 2 (156), pp. 58–72. Available at: http://www.viam-works.ru (accessed: June 14, 2026). DOI: 10.18577/2307-6046-2026-0-2-58-72.
  5. Ivanov М.S., Morozova V.S., Pavlukovich N.G. The influence of operational factors on the properties of carbon fiber based on polyetheretherketone. Aviation materials and technologies, 2024, no. 2 (75), pp. 99–108. Available at: http://www.journal.viam.ru (accessed: June 14, 2026). DOI: 10.18577/2713-0193-2024-0-2-99-108.
  6. Pavlukovich N.G., Ivanov М.S., Morozova V.S., Donskih I.N. Investigation of the thermal stability of the melt polyetheretherketone PEEK-50P and carbon fiber based on it. Aviation materials and technologies, 2024, no. 2 (75), pp. 90–98. Available at: http://www.journal.viam.ru (accessed: June 14, 2026). DOI: 10.18577/2713-0193-2024-0-2-90-98.
  7. Sorokin A.E., Ivanov M.S., Sagomonova V.A. Thermoplastic polymer composite materials based on polyetheretherketones of various manufacturers. Aviation materials and technologies, 2022, no. 1 (66), pp. 41–50. Available at: http://www.journal.viam.ru (accessed: June 14, 2026). DOI: 10.18577/2713-0193-2022-0-1-41-50.
  8. Irzhak V.I. Interfacial Layer in Polymer Nanocomposites. Vysokomolekulyarnye soyedineniya. Ser.: S, 2020, vol. 62, no. 1, pp. 55–65.
  9. Volynskii A.L., Yarysheva A.Yu., Rukhlya E.G. et al. Influence of Nanoscale Confinement on Structure Formation in Glassy and Crystalline Polymers. Vysokomolekulyarnye soyedineniya. Ser.: A, 2015, vol. 57, no. 5, pp. 1–39.
  10. Valenkov A.M., Gofman I.V., Nosov K.S. Polymer Composite Systems Modified with Carbon Allotropes (Review). Zhurnal prikladnoy khimii, 2011, vol. 84, no. 5, pp. 705–717.
  11. Yue H., Monreal-Bernal A., Fernández-Blázquez J. et al. Macroscopic CNT fibers inducing nonepitaxial nucleation and orientation of semicrystalline polymers. Scientific Reports, 2015, vol. 5, p. 16729. DOI: 10.1038/srep16729.
  12. Thomason J.L., Van Rooyen A.A. Transcrystallized interphase in thermoplastic composites. Part I. Influence of fibre type and crystallization temperature. Journal of Material Science, 1992, vol. 27, pp. 889–896. DOI: 10.1007/BF01197638.
  13. Wang C., Liu C.R. Transcrystallization of polypropylene composites: nucleating ability of fibres. Polymer, 1999, vol. 40, pp. 289–298.
  14. Wang C., Hwang L.M. Transcrystallization of PTFE fiber/PP composites (I). Crystallization kinetics and morphology. Journal of Polymer Science: Polymer Physics Edition, 1996, vol. 34, pp. 47–56.
  15. Chalykh A.E. Fundamental problems of adhesive interactions in polymer systems. Abstracts of the 3rd International Scientific and Technical Conference «Modern Advances in the Field of Adhesives and Sealants: Materials, Raw Materials, and Technologies». Nizhny Novgorod, 2019, 255 p.
  16. Kitayama T., Utsumi S., Hamada H. et al. Interfacial properties of PP/PP composites. Journal of Applied Polymer Science, 2003, vol. 88, no. 13, pp. 2875–2883.
  17. Brodowsky H., Mäder E. Investigation of transcrystalline interphases in polypropylene/glass fiber composites using micromechanical tests. Fibers, 2018, vol. 6, no. 16, pp. 1–12. DOI: 10.3390/fib6010016.
  18. Thomason J.L., Van Rooyen A.A. Transcrystallized interphase in thermoplastic composites. Part II. Influence of interfacial stress, cooling rate, fibre properties and polymer molecular weight. Journal of Material Science, 1992, vol. 27, pp. 897–907. DOI: 10.1007/BF01197639.
  19. Campbell D., Qayyum M.M. Melt crystallization of polypropylene: Effect of contact with fiber substrates. Journal of Polymer Science: Polymer Physics Edition, 1980, vol. 18, pp. 83–93. DOI: 10.1002/pol.1980.180180107.
  20. Klein N., Marom G. Thermal Expansion of Transcrystalline Strips. Advanced Composites Letters, 1995, vol. 4, no. 1, pp. 9–11.
  21. Nuriel H., Klein N., Marom G. The effect of the transcrystalline layer on the mechanical properties of composite materials in the fibre direction. Composites Science and Technology, 1999, vol. 59, pp. 1685–1690.
  22. Vaughan A.S., Bassett D.C. Early stages of spherulite growth in melt-crystallized polystyrene. Polymer, 1988, vol. 29, is. 8, pp. 1397–1401.
  23. Moon C.K. Effect of molecular weight and fiber diameter on the interfacial behavior in glass fiber/PP composites. Journal of Applied Polymer Science, 1998, vol. 67, no. 7, pp. 1191–1197.
  24. Zhang M.Q., Xu J.R., Zhang Z.Y. et al. Effect of transcrystallinity on tensile behaviour of discontinuous carbon fibre reinforced semicrystalline thermoplastic composites. Polymer, 1996, vol. 37, is. 23, pp. 5151–5158.
  25. Quan H., Zhong-Ming Li, Ming-Bo Yang et al. On transcrystallinity in semi-crystalline polymer composites. Composites Science and Technology, 2005, vol. 65, pp. 999–1021. DOI: 10.1016/j.compscitech.2004.11.015.
  26. Pompe G., MaÈder E. Experimental detection of a transcrystalline interphase in glass-fibre/polypropylene composites. Composites Science and Technology, 2000, vol. 60, pp. 2159–2167.
  27. Varga J., Karger-Kocsis J. The occurrence of transcrystallization or row-nucleated cylindritic crystallization as a result of shearing in a glass fiber-reinforced polypropylene. Composites Science and Technology, 1993, vol. 48, pp. 191–198.
  28. Ji H., Zhou X., Chen X. Effect of Solid-state stretching on microstructure evolution and physical properties of isotactic polypropylene sheets. Polymers, 2019, vol. 11, pp. 1–16.
  29. Zhang C., Hu H., Wang X. et al. Formation of cylindrite structures in shear-induced crystallization of isotactic polypropylene at low shear rate. Polymer, 2007, vol. 48, pp. 1105–1115.
  30. Looijmans S.F.S.P., Spanjaards M.M.A., Puskar L. Synergy of fiber surface chemistry and flow: multi-phase transcrystallization in fiber-reinforced thermoplastics. Polymers, 2022, vol. 14, is. 4850, pp. 1–16.
  31. Klein N., Marom G., Wachtel E. Microstructure of nylon 66 transcrystalline layers in carbon and aramid fibre reinforced composites. Polymer, 1996, vol. 14, pp. 5493–5498.
  32. Feldman A., Gonzalez M.F., Marom G. Transcrystallinity in surface modified aramid fiber reinforced nylon 66 composites. Macromolecular Materials and Engineering, 2003, vol. 288, no. 11, pp. 861–866.
  33. Feldman A.Y., Wachtel E., Vaughan G.B.M. The Brill Transition in Transcrystalline Nylon-66. Macromolecules, 2006, vol. 39, pp. 4455–4459.
  34. Van Staden J.K.L., Rodgers D.R., Pfau-Cloud M.R. et al. Interfacial crystallization of Poly(l-lactic acid) induced by carbon nanotubes in single fiber composites. Macromolecular chemistry and physics, 2025, vol. 226, is. 23, pp. 1–9.
  35. Chen H., Ji C., Yang Y. et al. Exploring the interlocking transcrystalline: forming a new structure of transcrystalline for improved mechanical performance of carbon fiber reinforced polyether ether ketone composites. Polymer Composites, 2026, vol. 47, pp. 1838–1846. DOI: 10.1002/pc.70256.
  36. Zhiyi Z., Zeng H. Nucleation and crystal growth of PEEK on carbon fiber. Journal of Applied Polymer Science, 1993, vol. 48, pp. 1987–1995.
  37. Hanmin Z., Zhiyi Z., Weizou P. et al. Transcrystalline structure of PEEK. European Polymer Journal, 1994, vol. 30, no. 2, pp. 235–237.
  38. Lustiger A. Morphological Aspects of the Interface in the PEEK-Carbon Fiber System. Polymer composites, 1992, vol. 13, no. 5, pp. 408–412.
  39. Yu K., Cong Z., Zhang Y. Unveiling the role of carbon fiber modulus on interfacial crystallization and mechanical properties of LM-PAEK composites. Polymer, 2026, vol. 355, art. 130010. DOI: 10.1016/j.polymer.2026.130010.
  40. Chen E.J.H., Hsiao B.S. The Effects of Transcrystalline lnterphase in Advanced Polymer Composites. Polymer Engineering and Science, 1992, vol. 32, no. 4, pp. 280–286.
  41. Ramani K., Tagle J. Thin-Film Thermoplastic-Metal Joining Process for Titanium to Poly (Etherketoneetherketoneketone). Polymer engineering and science, 1995, vol. 35, no. 24, pp. 1972–1978.
  42. Yu K., Zhang J., Liu G. et al. Inverse effects of cooling rates on the interfacial shear strength of carbon Fiber/PEEK composites with and without presence of transcrystal layers. Polymer, 2024, vol. 302, art. 127067. DOI: 10.1016/j.polymer.2024.127067.