I. G. Lukachevskaia, O. V. Startsev, D. R. Nizin, A. A. Dyakonov, A. L. Tereshkin Effect of moisture content on the strength of Etal-247 epoxy polymer cured with different hardeners // Proceedings of VIAM. 2026. No. 11 (165). С. 65-80. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-11-65-80.

Effect of moisture content on the strength of Etal-247 epoxy polymer cured with different hardeners

I. G. Lukachevskaia1, O. V. Startsev2, D. R. Nizin1, A. A. Dyakonov1, A. L. Tereshkin1

1Federal Research Centre «Yakut Scientific Centre of the Siberian Branch of the Russian Academy of Sciences», Yakutsk, Russia; presidium@prez.ysn.ru 
2Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

The effect of moisture content on the tensile strength of unfilled Etal-247 epoxy polymer cured with Etal-1472, Etal-45M, Etal-45TZ2 and Etal-M7 was studied. Increasing water content reduced the strength of all compositions, while the character and intensity of the relationship depended on the hardener. Etal-45TZ2- and Etal-M7-based systems showed the highest sensitivity to initial moisture uptake. Surface morphology may influence the initial stage of water ingress, whereas the principal mechanism governing the change in mechanical properties is plasticization of the bulk polymer network.

Keywords
epoxy polymer, Etal-247, hardener, moisture content, tensile strength, plasticization, glass-transition temperature, climatic ageing

Reference list
  1. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  2. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 122–144. Available at: http://www.journal.viam.ru (accessed: July 31, 2026). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  3. Kablov E.N., Startsev V.O., Laptev A.B. Aging of Polymer Composite Materials. Moscow: NRC «Kurchatov Institute» – VIAM, 2023, 520 p.
  4. Abiodun M.-I.B., Oluwole O.I., Damilola A.A. et al. Applications of epoxy resin: adhesives, coatings, and composites. Epoxy: Materials, Applications and Advanced Technologies. London: IntechOpen, 2025, pp. 1–15. DOI: 10.5772/intechopen.1012261.
  5. Corcione C.E., Freuli F., Frigione M. Cold-curing structural epoxy resins: analysis of the curing reaction as a function of curing time and thickness. Materials, 2014, vol. 7, pp. 6832–6842. DOI: 10.3390/ma7096832.
  6. Barannikov A.A., Veshkin E.A., Sudin Yu.I., Chertischev V.Yu. To the issue of helicopter rotor blades repair from polymer composite materials in field conditions. Trudy VIAM, 2024, no. 4 (134), p. 83–97. Available at: http://www.viam-works.ru (accessed: July 31, 2026). DOI: 10.18577/2307-6046-2024-0-4-83-97.
  7. Lettieri M., Frigione M. Natural and artificial weathering effects on cold-cured epoxy resins. Journal of Applied Polymer Science, 2011, vol. 119, pp. 1635–1645.
  8. He W., Jiang X., He R. et al. A review on the aging behavior of BADGE-based epoxy resin. Buildings, 2025, vol. 15, art. 2450. DOI: 10.3390/buildings15142450.
  9. Singh K.K., Singh A.K., Singh A. Environmental degradation of carbon/epoxy advanced polymer matrix composites. Journal of Materials Science: Composites, 2025, vol. 6, art. 13. DOI: 10.1186/s42252-025-00078-6.
  10. Kablov E.N., Startsev O.V., Medvedev I.M. Corrosivity of a Marine Atmosphere. Part 2. New Approaches to Assessing the Corrosivity of Marine Atmospheres. Korroziya: materialy, zashchita, 2016, no. 1, pp. 1–15.
  11. Kablov E.N., Startsev V.O. Climatic Aging of Polymer Composite Materials for Aviation Applications. 1. Assessment of the Influence of Significant Exposure Factors. Deformatsiya i razrusheniye materialov, 2019, no. 12, pp. 7–16.
  12. Startsev V.O., Lebedev M.P., Khrulev K.A. et al. Effect of outdoor exposure on the moisture diffusion and mechanical properties of epoxy polymers. Polymer Testing, 2018, vol. 65, pp. 281–296.
  13. Kablov E.N., Startsev O.V., Panin S.V. Moisture Transport in Carbon-Fiber-Reinforced Plastic with a Degraded Surface. Doklady Akademii nauk, 2015, vol. 461, no. 4, pp. 433–436.
  14. Zhelezina G.F., Kulagina G.S., Kan A.Ch., Startsev V.O. Research of the climate stability of hybrid layered metal polymer materials based on aluminium and aramid organoplastics. Trudy VIAM, 2024, no. 7 (137), pp. 34–44. Available at: http://www.viam-works.ru (accessed: July 31, 2026). DOI: 10.18577/2307-6046-2024-0-7-34-44.
  15. Nikolaev E.V., Slavin A.V., Startsev V.O., Laptev A.B. Modern approaches to assessing the impact of external factors on materials and complex technical systems (to the 120th anniversary of G.V. Akimov). Trudy VIAM, 2021, no. 9 (103), pp. 117–130. Available at: http://www.viamworks.ru (accessed: July 31, 2026). DOI: 10.18577/2307-6046-2021-0-9-117-130.
  16. Joo J.-H., Jeong J.-R., Yim Y.-J. et al. Recent advances in epoxy resin applications. COJ Technical & Scientific Research, 2025, vol. 5, art. 000612. DOI: 10.31031/COJTS.2025.05.000612.
  17. Blaznov A.N., Zhurkovsky M.E., Firsov V.V. et al. Investigation of the Physico-Mechanical Properties of a Binder Based on the Etal-45M Hardener. Yuzhno-Sibirskiy nauchnyy vestnik, 2019, no. 3 (27), pp. 100–107.
  18. Kanaeva N.S. Prediction of Dynamic Fatigue in Epoxy Polymers Subjected to Climatic Exposure: thesis, Cand. Sc. (Tech.). Saransk, 2023, 275 p.
  19. Blaznov A.N., Samoilenko V.V., Firsov V.V. et al. Investigation of the Loss of Elastic Properties in Fiberglass-Reinforced Plastics Based on Epoxy Binders with Etal Hardeners Due to Chemical Aging in an NaOH Solution. Yuzhno-Sibirskiy nauchnyy vestnik, 2020, no. 6, pp. 91–94. DOI: 10.25699/p7780-1227-2890-v.
  20. State Standard 11262–2017. Plastics. Tensile Test Method. Moscow: Standartinform, 2018, 28 p.
  21. State Standard R 56762–2015. Polymer Composites. Method for Determining Moisture Absorption and Equilibrium State. Moscow: Standartinform, 2016, 36 p.
  22. ISO 6721-1:2019. Plastics – Determination of dynamic mechanical properties – Part 1: General principles. Geneva: International Organization for Standardization, 2019, 23 p.
  23. Huang J., Fu P., Li W. et al. Influence of crosslinking density on the mechanical and thermal properties of plant oil-based epoxy resin. RSC Advances, 2022, vol. 12, pp. 23048–23056. DOI: 10.1039/d2ra04206a.
  24. Startsev O.V., Startsev V.O., Kogan A.M., Vardanyan A.M. Сhanges in the plasticizing effect of moisture during climatic aging of polymer composite materials. Russian Metallurgy (Metally), 2024, vol. 2024, no. 2, pp. 413–422. DOI: 10.31044/1814-4632-2024-1-16-26.
  25. Startsev V.O., Molokov M.V., Grebeneva T.A., Tkachuk A.I. Dynamic mechanical and thermomechanical analysis of reversible plasticization of epoxy-diane resindiaminodiphenylsulfon system by moisture. Polymer Science. Series A, 2017, vol. 59, no. 5, pp. 640–648. DOI: 10.1134/S0965545X17050157.
  26. Taysun M.B., Dam-Johansen K., Bi H. Hydrogen bonding and anti-plasticization in epoxy coatings: Molecular insights into water uptake and network stability. Progress in Organic Coatings, 2025, vol. 209, art. 109602. DOI: 10.1016/j.porgcoat.2025.109602.
  27. Kornienko G.V., Startsev O.V., Krotov A.S., Koval T.V. Dependence modeling of the CFRP shear modulus on moisture content. Aviation materials and technologies, 2025, no. 3 (80), pp. 161–178. Available at: http://www.journal.viam.ru (accessed: July 31, 2026). DOI: 10.18577/2713-0193-2025-0-3-161-178.
  28. Startsev O.V., Nikishin E.F. Ageing of polymeric composite materials in outer space. Mehanika kompozitnyh materialov, 1993, vol. 29, no. 4, pp. 457–467.