I. Benarieb, D. V. Zaytsev, Yu. A. Puchkov Study of crystal structure of quench-induced precipitates in aluminum alloy V-1341 of the Al–Mg–Si system // Proceedings of VIAM. 2026. No. 11 (165). С. 52-64. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-11-52-64.

Study of crystal structure of quench-induced precipitates in aluminum alloy V-1341 of the Al–Mg–Si system

I. Benarieb1, D. V. Zaytsev1, Yu. A. Puchkov2

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru 
2Federal State Budgetary Educational Institution of Higher Education «Bauman Moscow State Technical University (National Research University of Technology)», Moscow, Russia; bauman@bmstu.ru

Abstract

Quench-induced precipitates formed in a 1.2 mm thick sheet specimen of Al–0.73Mg–0.60Si–0.18Cu–0.27Mn–0.23Fe alloy (V-1341) after quenching at a cooling rate of 0.3 °C/s (below the critical cooling rate) and subsequent natural ageing were studied by transmission electron microscopy, Fourier-transform analysis, and energy-dispersive X-ray microanalysis. The precipitates were found to correspond predominantly to metastable β′(Mg9Si5) and B′(Al3Mg9Si7) phases. It was shown that copper can be incorporated into the quench-induced precipitates and, at increased local concentrations, may cause structural heterogeneity.

Keywords
Al–Mg–Si–(Cu) alloys, quench-induced precipitation, dispersoids, solid-solution decomposition, high-resolution transmission electron microscopy, Fourier transform analysis


Reference list
  1. Benarieb I., Sbitneva S.V., Zaytsev D.V., Shorstov S.Yu. Features of quench-induced precipitation in sheets of V-1341 aluminum alloy of Al–Mg–Si system. Trudy VIAM, 2025, no. 8 (150), pp. 53–66. Available at: http://www.viam-works.ru (accessed: April 22, 2026). DOI: 10.18577/2307-6046-2025-0-8-53-66.
  2. Chuistov K.V. Aging of Metal Alloys. 2nd ed., rev. and add. Kyiv: Akademperiodika, 2003, 567 p.
  3. Kolobnev N.I., Ber L.B., Khokhlatova L.B., Ryabov D.K. Structure, properties, and application of Al–Mg–Si–(Cu) system alloys. Metallovedenie i termicheskaya obrabotka metallov, 2011, no. 9, pp. 40–45.
  4. Yashin V.V., Aryshenskii E.V., Drits A.M. et al. Effect of a low degree of cold deformation on the strengthening of Al–Mg–Si alloy sheets during artificial aging. Metallovedenie i termicheskaya obrabotka metallov, 2025, no. 6 (840), pp. 19–27.
  5. Bochvar N.R., Dobatkin S.V., Rybalchenko O.V. et al. Investigation of the recrystallization process in Al–Mg–Si alloys with Sc, Zr, and Hf additions following various types of cold deformation. Tekhnologiya legkikh splavov, 2020, no. 1, pp. 19–27.
  6. Benarieb I., Puchkov Yu.A., Sbitneva S.V., Shorstov S.Yu., Shumeyko R.M. Quench sensitivity of wrought heat-treatable aluminum alloys of the Al–Mg–Si system (review). Trudy VIAM, 2025, no. 2 (144), pp. 25–46. Available at: http://www.viam-works.ru (accessed: May 06, 2025). DOI: 10.18577/2307-6046-2025-0-2-25-46.
  7. Grushko O.E., Ovsyannikov B.V., Ovchinnikov V.V. Calcium as an Element for Micro-alloying Wrought Aluminum Alloys: A Monograph. Moscow; Vologda: Infra-Inzheneriya, 2021, 296 p.
  8. Marioara C.D., Nordmark H., Andersen S.J., Holmestad R. Post-βʹʹ phases and their influence on microstructure and hardness in 6xxx Al–Mg–Si alloys. Journal of Materials Science, 2006, vol. 41, pp. 471–478.
  9. Marioara C.D., Andersen S., Hell C. et al. Atomic structure of clusters and GP-zones in an Al–Mg–Si alloy. Acta Materialia, 2024, vol. 269, p. 119811.
  10. Andersen S.J., Zandbergen H.W., Jansen J. et al. The crystal structure of the β″ phase in Al–Mg–Si alloys. Acta Materialia, 1998, vol. 46, pp. 3283–3298.
  11. Christiansen E., Marioara C., Holmedal B. et al. Nano-scale characterisation of sheared β′′ precipitates in a deformed Al–Mg–Si alloy. Scientific Reports, 2019, vol. 9, no. 1, p. 17446.
  12. Vissers R., van Huis M.A., Jansen J. et al. The crystal structure of the β′ phase in Al–Mg–Si alloys. Acta Materialia, 2007, vol. 55, no. 11, pp. 3815–3823.
  13. Sunde J.K., Marioara C.D., van Helvoort A.T.J., Holmestad R. The evolution of precipitate crystal structures in an Al–Mg–Si(–Cu) alloy studied by a combined HAADF-STEM and SPED approach. Materials Characterization, 2018, vol. 142, pp. 458–469.
  14. Sunde J.K., Marioara C.D., Holmestad R. The effect of low Cu additions on precipitate crystal structures in overaged Al‒Mg‒Si(‒Cu) alloys. Materials Characterization, 2020, vol. 160, p. 110087.
  15. Saito T., Mortsell E.A., Wenner S. et al. Atomic structures of precipitates in Al–Mg–Si alloys with small additions of other elements. Advanced Engineering Materials, 2018, vol. 20, no. 7, pp. 1800125.
  16. Ohmori Y., Long C., Matsuura Y. et al. Morphology and crystallography of β-Mg2Si precipitation in Al–Mg–Si alloys. Materials Transactions, 2001, vol. 42, no. 12, pp. 2576–2583.
  17. Ohmori Y., Doan L.C., Nakai K. Ageing processes in Al–Mg–Si alloys during continuous heating. Materials Transactions, 2002, vol. 43, no. 2, pp. 246–255.
  18. Gazizov M.R., Boev A.O., Gazizova M.Yu., Kaibyshev R.O. Intermetallic particles in Al–Cu–Mg(–Si, –Ag) alloys: atomic-resolution transmission electron microscopy. Abstracts of the Int. Conf. «Physical Mesomechanics: Materials with a Multilevel Hierarchically Organized Structure and Intelligent Manufacturing Technologies». Tomsk, 2023, pp. 102–103.
  19. Ma Y., Liu C., Miao K. et al. Effects of cooling rate and cryogenic temperature on the mechanical properties and deformation characteristics of an Al–Mg–Si–Fe–Cr alloy. Journal of Alloys and Compounds, 2023, vol. 947, p. 169559.
  20. Liu S., Wang X., Pan Q. et al. Investigation of microstructure evolution and quench sensitivity of Al–Mg–Si–Mn–Cr alloy during isothermal treatment. Journal of Alloys and Compounds, 2020, vol. 826, p. 154144.
  21. Strobel K., Easton M., Sweet L. et al. Relating quench sensitivity to microstructure in 6000 series aluminium alloys. Materials Transactions, 2011, vol. 52, no. 5, pp. 914–919.
  22. Gao C., Liu X., Zhao D. et al. Recent Progress in Testing and Characterization of Hardenability of Aluminum Alloys: A Review. Materials, 2023, vol. 16, p. 4736.
  23. Yang M., Ruan Z., Lin H. et al. Quantified effect of quench rate on the microstructures and mechanical properties of an Al–Mg–Si alloy. Journal of Materials Research and Technology, 2023, vol. 24, pp. 6753–6761.
  24. Marioara C.D., Andersen S.J., Stene T.N. et al. The effect of Cu on precipitation in Al‒Mg‒Si alloys. Philosophical Magazine, 2007, vol. 87, no. 23, pp. 3385–3413.
  25. Li K., Song M., Du Y., Fang X. Effect of minor Cu addition on the precipitation sequence of an as-cast Al–Mg–Si 6005 alloy. Archives of Metallurgy and Materials, 2012, vol. 57, no. 2, pp. 458–466.
  26. Weng Y., Jia Z., Ding L. et al. The multiple orientation relationships and morphology of β' phase in Al‒Mg‒Si‒Cu alloy. Journal of Alloys and Compounds, 2018, vol. 767, pp. 81–89.
  27. Chen H., Lu J., Kong Y. et al. Atomic scale investigation of the crystal structure and interfaces of the B′ precipitate in Al‒Mg‒Si alloys. Acta Materialia, 2020, vol. 185, pp. 193–203.
  28. Ding L., Jia Z., Nie J.F. et al. The structural and compositional evolution of precipitates in Al‒Mg‒Si‒Cu alloy. Acta Materialia, 2018, vol. 145, pp. 437–450.
  29. Matsuda K., Uetani Y., Sato T., Ikeno S. Metastable phases in an Al–Mg–Si alloy containing copper. Metallurgical and Materials Transactions A, 2001, vol. 32, no. 6, pp. 1293–1299.
  30. Maeda T., Kaneko K., Namba T. et al. Structural and compositional study of precipitates in underaged Cu added Al‒Mg‒Si alloy. Nature, 2018, vol. 8, art. 16629.
  31. Saito T., Marioara C., Royset J. et al. The effects of quench rate and pre-deformation on precipitation hardening in Al‒Mg‒Si alloys with different Cu amounts. Materials Science and Engineering: A, 2014, vol. 609, pp. 72–79.
  32. Gazizov M., Marioara C.D., Friis J. et al. Unique hybrid precipitate structures forming in an Al–Cu–Mg–Si alloy. Journal of Alloys and Compounds, 2020, vol. 826, art. 153977.
  33. Gazizov M.R., Holmestad R., Marioara C.D., Kaibyshev R.O. Quantitative analysis of {100}Al plate/lath- and <100>Al rod-shaped precipitates in an aged Al‒Cu‒Mg‒Si alloy using TEM. IOP Conference Series: Material Science and Engineering, 2021, vol. 1014, art. 012013.
  34. Garric V., Colas K., Donnadieu P. et al. Correlation between quenching rate, mechanical properties and microstructure in thick sections of AlMgSi (Cu) alloys. Materials Science and Engineering: A, 2019, vol. 753, pp. 253–261.
  35. Bartawi E.H., Marioara C.D., Shaban G. et al. Atomic structure of hardening precipitates in Al–Mg–Si alloys: influence of minor additions of Cu and Zn. ACS nano, 2023, vol. 17, no. 23, pp. 24115–24129.
  36. Sbitneva S.V., Lukina E.А., Zaytsev D.V. Investigation of the features of the decomposition of a solid solution during aging of alloys of the Al–Mg–Si–Cu system. Trudy VIAM, 2021, no. 12 (106), pp. 12–40. Available at: http://www.viam-works.ru (accessed: April 22, 2026). DOI: 10.18577/2307-6046-2021-0-12-14-20.
  37. Benarieb I., Puchkov Yu.A., Sbitneva S.V., Zaitsev D.V. Investigation of the decomposition of a supersaturated solid solution during the quenching of sheets made of an Al–Mg–Si system aluminum alloy. Fizika metallov i metallovedenie, 2023, vol. 124, no. 9, pp. 838–845. DOI: 10.31857/S0015323023600843.
  38. Kablov E.N., Duyunova V.A., Benarieb I. et al. Features of the decomposition of a supercooled solid solution during the quenching of sheets made of the advanced Al–Mg–Si system alloy V-1341. Tekhnologiya legkikh splavov, 2020, no. 3, pp. 20–33.
  39. Sbitneva S.V., Zaytsev D.V., Benarieb I. Features of the structure of age-hardenable aluminum alloy AlSi10MgCu produced by selective laser melting. Trudy VIAM, 2024, no. 9 (139), pp. 15–24. Available at: http://www.viam-works.ru (accessed: April 22, 2026). DOI: 10.18577/2307-6046-2024-0-9-15-24.
  40. Xia C., Deng S., Ni C. et al. Study on laminar structure and process on high strength brazed aluminum alloy for heat exchangers. Vacuum, 2023, vol. 215, p. 112303.
  41. Fan Z., Lei X., Wang L. et al. Influence of quenching rate and aging on bendability of AA6016 sheet. Materials Science and Engineering: A, 2018, vol. 730, pp. 317–327.