UDC
669.018.44:669.245
DOI
10.18577/2307-6046-2026-0-11-15-31
Article PDF (Russian)
(1.69 MB)
How to cite
M. M. Karashaev, A. V. Vostrikov, D. I. Sukhov Relationship between the structure and mechanical properties of nickel-based heat-resistant alloys and the technology of producing disc blanks produced by granule metallurgy // Proceedings of VIAM. 2026. No. 11 (165). С. 15-31. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-11-15-31.
Relationship between the structure and mechanical properties of nickel-based heat-resistant alloys and the technology of producing disc blanks produced by granule metallurgy
1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
Abstract
This paper presents the key principles of modern disk blank production from nickel-based heat-resistant alloy powder granules produced by the granule metallurgy method (as-HIP). The results of studies devoted to this area are analyzed, and reflect the relationship between the structure and mechanical properties of nickel-based superalloys and the process parameters for producing disk blanks obtained using hot isostatic pressing technology.
Keywords
granule metallurgy, superalloys, hot isostatic pressing, PREP method, quenching, aging
Reference list
- Erasov V. S., Oreshko E. I., Lutsenko A. N. Multilevel large-scale complex research of deformation of metal materials. Aviation materials and technologies, 2022, no. 1 (66), pp. 129–142. Available at: http://www.journal.viam.ru (accessed: June 08, 2026). DOI: 10.18577/2713-0193-2022-0-1-129-142.
- Movenko D. A., Shurtakov S. V. Microcrack formation and controlling in nickel superalloys processed by selective laser melting (review). Aviation materials and technologies, 2022, no. 2 (67), pp. 43–51. Available at: http://www.journal.viam.ru (accessed: June 08, 2026). DOI: 10.18577/2713-0193-2022-0-2-43-51.
- Kablov E. N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Svetlov I. L., Petrushin N. V., Epishin A. I., Karashaew M. M., Elyutin E. S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 1. Aviation materials and technologies, 2023, no. 1 (70), pp. 30–50. Available at: http://www.journal.viam.ru (accessed: June 08, 2026). DOI: 10.18577/2713-0193-2023-0-1-30-50.
- Svetlov I. L., Petrushin N. V., Epishin A. I., Karashaew M. M., Elyutin E. S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 2. Aviation materials and technologies, 2023, no. 2 (71), pp. 3–22. Available at: http://www.journal.viam.ru (accessed: June 08, 2026). DOI: 10.18577/2713-0193-2023-0-2-3-22.
- Zaysev D. V., Sbitneva S. V., Ber L. B., Zavodov A. V. Determination of the main phase’s particles chemical composition in products from granulated nickel superalloy EP741NP. Trudy VIAM, 2016, no. 9, pp. 61–71. Available at: http://www.viam-works.ru (accessed: June 08, 2026). DOI: 10.18577/2307-6046-2016-0-9-8-8.
- Garibov G. S., Grits N. M., Vostrikov A. V., Fedorenko E. V., Volkov A. M. Development of a promising high-strength powder-metallurgy nickel-based superalloy for turbine disks in next-generation aircraft components. Tekhnologiya legkikh splavov, 2012, no. 3, pp. 64–69.
- Garibov G. S., Vostrikov A. V., Grits N. M., Fedorenko E. A. Development of new powder-metallurgy nickel-based superalloys for the production of aircraft engine disks and shafts. Tekhnologiya legkikh splavov, 2010, no. 1, pp. 34–43.
- Garibov G. S., Grits N. M., Volkov A. M., Vostrikov A. V., Fedorenko E. A. Metallurgical aspects of producing disk preforms from powder-metallurgy nickel-based superalloys via hot isostatic pressing (HIP). Tekhnologiya legkikh splavov, 2014, no. 3, pp. 54–58.
- Garibov G. S. Theory of crystallization of granular heat-resistant nickel-based alloys. Tekhnologiya legkikh splavov, 2016, no. 1, pp. 107–118.
- Belov A. F. The Present and Future of Granule Metallurgy. Metallurgiya granul, 1983, is. 1, pp. 5–13.
- Dobatkin V. I. The Role of Kinetic and Thermodynamic Factors in the Crystallization of Granules. Metallurgiya granul, 1983, is. 1, pp. 23–33.
- Dobatkin V. I. Principles of Rapid Crystallization as a Basis for Selecting the Compositions of Alloys to be Granulated. Metallurgiya granul, 1988, is. 4, pp. 11–23.
- Zvereva E. A. Investigation of the influence of crystallization conditions on the granule structure and properties of compacted products made from heat-resistant nickel-based alloys: thesis abstract, Cand. Sc. (Tech.). Moscow, 1979, 23 p.
- Belov A. F., Anoshkin N. F., Garibov G. S. Development and implementation of an industrial technology for the production of large-sized disks and hollow shafts from heat-resistant nickel-based alloy granules via hot isostatic pressing. Metallurgiya granul, 1983, is. 1, pp. 173–186.
- Garibov G. S. Development of Academician A.F. Belov’s concepts for the radical enhancement of the operational characteristics of disks for advanced gas-turbine engines. Advanced Technologies for Light and Special Alloys: In Honor of the 100th Anniversary of the Birth of Academician A.F. Belov. Moscow: Fizmatlit, 2006, pp. 44–63.
- Koshelev V. Ya., Garibov G. S., Sukhov D. I. Fundamental principles of the process for producing heat-resistant alloy granules via plasma atomization of a rotating workpiece. Tekhnologiya legkikh splavov, 2015, no. 3, pp. 97–103.
- Vostrikov A. V., Garibov G. S., Ber L. B., Shlyapin S. D. Investigation of the physical-mechanical properties and structure of granules made from a new high-strength nickel alloy using the PREP method. Tekhnologiya legkikh splavov, 2013, no. 2, pp. 69–75.
- Musienko V. T. Development of theoretical foundations and production technology for metal powders subjected to high and ultra-high cooling rates via centrifugal atomization, for the manufacture of gas-turbine engine disks: thesis, Dr. Sc. (Tech.). Moscow, 1991, 459 p.
- Ber L. B., Kazberovich A. M. Influence of alloying and certain structural factors on the set of properties of disk preforms made from powder-metallurgy (granulated) heat-resistant nickel-based alloys EP741NP, VV750P, VV751P, VV752P, and VV753P. Tekhnologiya legkikh splavov, 2019, no. 3, pp. 16–33.
- Rogozhkin S. V., Ber L. B., Nikitin A. A. et al. Investigation of a powder-metallurgy (granulated) heat-resistant nickel-based alloy using atom probe tomography. Fizika metallov i metallovedeniye, 2020, vol. 121, no. 1, pp. 60–71.
- Kazberovich A. M., Ber L. B., Egorov D. A., Zhivushkin A. A., Polyansky S. B., Mukhina T. A. Improving the set of properties of disk preforms made from granules of the EP741NP alloy for advanced gas turbine engines. Tekhnologiya legkikh splavov, 2020, no. 4, pp. 36–46.
- Ber L. B., Rogozhkin S. V., Khomich A. A., Zaluzhny A. G. Distribution of alloying element atoms between the γ- and γʹ-phase particles in a heat-resistant nickel-based alloy. Fizika metallov i metallovedeniye, 2022, vol. 123, no. 2, pp. 177–191.
- Belov A. F., Anoshkin N. F., Grits N. M. et al. Specifics of Alloying Heat-Resistant Alloys Produced via Powder Metallurgy. Heat-Resistant and Oxidation-Resistant Steels and Nickel-Based Alloys. Moscow: Nauka, 1984, 31 p.
- State Standard R 52802–2007. Granulatable Heat-Resistant Nickel Alloys (Grades). Moscow: Standartinform, 2008, 3 p.
- Garibov G. S., Grits N. M., Vostrikov A. V. et al. Development and Investigation of a New Granulatable High-Strength Heat-Resistant Nickel Alloy, VV752P, for Advanced Aviation Components. Tekhnologiya legkikh splavov, 2011, no. 1, pp. 7–11.
- Garibov G. S. V.I. Dobatkin and the Powder Metallurgy of Heat-Resistant Nickel Alloys. Tekhnologiya legkikh splavov, 2015, no. 2, pp. 34–39.
- Inozemtsev A. A., Anoshkin N. F., Bashkatov I. G. et al. Application of Disks Made from Granulated Heat-Resistant Nickel Alloys in Serial Gas Turbine Engines for Aviation and Ground-Based Equipment. Advanced Technologies for Light and Special Alloys. Moscow: Fizmatlit, 2006, pp. 371–376.
- Garibov G. S. Current State of Development in the Powder Metallurgy of Heat-Resistant Nickel Alloys. Tekhnologiya legkikh splavov, 2000, no. 6, pp. 58–68.
- Volkov A. M., Vostrikov A. V., Bakradze M. M. Development principles and alloying features of p/m Ni-base superalloys for jet-engine disks application. Trudy VIAM, 2016, no. 8, pp. 10–16. Available at: http://www.viam-works.ru (accessed: June 08, 2026). DOI: 10.18577/2307-6064-2016-0-8-2-2.
- Samarov V., Barre Ch., Seliverstov D. Net Shape HIP for Complex Shape PM Parts as a Cost-Efficient Industrial Technology. Proceedings of HIP-05 International Conference. Paris, 2005, 515 p.
- Samarov V. N., Anoshkin N. F. Development of Hot Isostatic Pressing (HIP) Technology for Complex-Shaped Parts Made from Granular Materials. Advanced Technologies for Light and Special Alloys: In Honor of the 100th Anniversary of the Birth of Academician A.F. Belov. Moscow: Fizmatlit, 2006, pp. 103–113.
- Garibov G. S., Tlyusten T. Yu. Hot Isostatic Presses (Gas-Static Presses) at VILS. Zagotovitelnye proizvodstva v mashinostroyenii, 2010, no. 7, pp. 28–33.
- Svenchansky A. D. Industrial Electric Furnaces: A Textbook for Higher Education Institutions: in 2 parts. Moscow: Energiya, 1975, part 1, 384 p.
- Volkov A. M., Garibov G. S., Grits N. M., Vostrikov A. V., Fedorenko E. A. Investigation of Heating and Cooling Processes During the Quenching of Large-Sized Disk Preforms Made from Heat-Resistant Nickel Alloy Granules. Tekhnologiya legkikh splavov, 2013, no. 3, pp. 66–72.
- Sizova R. N., Nozhnitskiy Yu. A. Specifics of low-cycle fatigue resistance in disk materials manufactured via powder metallurgy. Metallurgiya granul, 1983, is. 1, pp. 405–412.
- Garibov G. S., Grits N. M., Vostrikov A. V., Fedorenko E. A., Egorov D. A. Improving the strength characteristics and low-cycle fatigue resistance of nickel-based superalloys produced from powder by reducing powder particle size. Tekhnologiya legkikh splavov, 2012, no. 3, pp. 56–63.
The article was submitted
2026-07-24
approved and accepted for publication after reviewing
2026-08-07