Analysis of factors affecting the preservation and accuracy of the properties determined during the stretching of carbon monofilament
1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
This article analyzes key aspects affecting the stability of the physical and mechanical properties of carbon fibers and demonstrates the relationship between these properties and the thermodynamic stability of carbon fiber, which does not guarantee the retention of properties due to the degradation of the sizing agent under external factors. A review of existing monofilament tensile testing standards (GOST, ISO, ASTM) is provided. Systematic errors in determining fiber diameter and cross-sectional area, in conducting monofilament tensile testing, and in recording strain are discussed.
1. Mallick P.K. Fiber-Reinforced Composites: Materials, Manufacturing, and Design. 3rd ed. CRC Press, 2007, 632 p.
2. Gulyaev I.N., Klimenko O.N., Lonskii S.L., Slavin A.V., Cherfas L.V. Determination of the composition and structure of polymer composite materials. Aviation materials and technologies, 2025, no. 4 (81), pp. 32–47. Available at: http://www.journal.viam.ru (accessed: April 17, 2026). DOI: 10.18577/2713-0193-2025-0-4-32-47.
3. Zhelezina G.F., Kulagina G.S., Sidorina A.I., Soloveva N.A. Fatigue of constructional organoplastics. Aviacionnye materialy i tehnologii, 2014, no. 1, pp. 89–100. Available at: http://www.journal.viam.ru (accessed: April 17, 2026). DOI: 10.18577/2713-0193-2024-0-1-89-100.
4. Shershak P.V., Yakovlev N.O., Shokin G.I., Kutsevich K.E., Popkova E.A. Evaluation method and factors influencing the bonding quality between face and honey-comb cores in floor and interior aircraft panels. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 81–88. DOI: 10.18577/2071-9140-2020-0-2-81-88.
5. Gulyaev A.I., Yakovlev N.O., Krylov V.D., Lashov O.A. Application of fractographic analysis in the study of interlayer fracture of PCM. Aviacionnye materialy i tehnologii, 2017, no. 3 (48), pp. 65–73. DOI: 10.18577/9140-2071-2017-0-3-65-73.
6. Chand S. Review: Carbon fibers for composites. Journal of Materials Science, 2000, vol. 35, p. 1303–1313. DOI: 10.1023/A:1004780301489.
7. Harikrishnan R., Mohite P.M., Upadhyay C.S. Generalized Weibull model-based statistical tensile strength of carbon fibres. Archive of Applied Mechanics, 2018, vol. 88, pp. 1617–1636. DOI: 10.1007/s00419-018-1391-9.
8. Chevallier A., Boutenel F., Guicheret V. et al. Single fibre tensile testing: analysing the influence of fibre misalignment. 21st European Conference on Composite Materials. Nantes, France, 2024, art. hal-04738979.
9. Li Q., Woodhead A.L., Church J.S., Naebe M. On the detection of carbon fibre storage contamination and its effect on the fibre–matrix interface. Scientific Reports, 2018, vol. 8, art. 16446. DOI: 10.1038/s41598-018-34609-y.
10. Sutulalov A.I., Podzhivotov N.Yu., Shershak P.V., Yakovlev N.O. Evaluation of homogeneity of physical and mechanical properties of semi-finished products for aviation purpose. Aviation materials and technologies, 2024, no. 1 (74), pp. 121–135. Available at: http://www.journal.viam.ru (accessed: April 17, 2026). DOI: 10.18577/2713-0193-2024-0-1-121-135.
11. Huang X. Fabrication and Properties of Carbon Fibers. Materials, 2009, vol. 2, pp. 2369–2403. DOI: 10.3390/ma2042369.
12. Nacharkina A.V., Zelenina I.V., Valueva M.I., Voronina O.G. Influence of additional sizing of carbon fiber in producing volume-reinforced preforms on the properties of high-temperature carbon fiber. Trudy VIAM, 2021, no. 1 (95), pp. 54–65. Available at: http://www.viam-works.ru (accessed: April 17, 2026). DOI: 10.18577/2307-6046-2021-0-1-54-65.
13. Sizing agent for carbon fiber, carbon fiber, carbon fiber-reinforced composite material, and method of producing carbon fiber-reinforced composite material: pat. WO 2015/049567 A1; appl. 30.09.14; publ. 09.04.15.
14. Sizing agent for carbon fiber, method for sizing carbon fiber by said sizing agent, sized carbon fiber and knitted or woven fabric using said carbon fiber: pat. US 7135516 B2; appl. 30.07.02; publ. 14.11.06.
15. Beider E.Ya., Petrova G.N., Izotova T.F. An influence of coupling agent on properties of thermoplastic glass reinforced plastics. Trudy VIAM, 2014, no. 9, pp. 47–52. Available at: http://viam-works.ru (accessed: April 17, 2026). DOI: 10.18577/2307-6046-2014-0-9-7-7.
16. Shenghe Tech. Carbon Fiber Storage Life and Handling Requirements. Available at: https://shenghetech.com/info-detail/carbon-fiber-storage-life-and-handling-requirements (accessed: March 02, 2026)
17. Zhang S., Gu H., Zhao M. et al. Effect of sizing agents on tensile properties of carbon fiber filament wound structures. Journal of Engineered Fibers and Fabrics, 2024, vol. 19, pp. 1–8. DOI: 10.1177/15589250231183159.
18. Yang T., Zhao Y., Liu H. et al. Effect of sizing agents on surface properties of carbon fibers and interfacial adhesion of carbon fiber/bismaleimide composites. ACS Omega, 2021, vol. 6, pp. 23028–23037. DOI: 10.1021/acsomega.1c01103.
19. Volkova O.Yu., Tatus N.A. Modern methods for determining fiber characteristics. Vestnik nauchno-tekhnicheskogo razvitiya, 2025, no. 177, pp. 3–14. Available at: http://www.vntr.ru (accessed: February 25, 2026). DOI: 10.18411/vntr2025-177-1.
20. Erasov V.S., Sibayev I.G., Sutubalov A.I., Popkova E.A., Gorbovets M.A. Methods of mechanical testing to determine the strength of carbon fibers. Aviation materials and technologies, 2024, no. 2 (75), pp. 137–148. Available at: http://www.journal.viam.ru (accessed: April 17, 2026). DOI: 10.18577/2713-0193-2024-0-2-137-148.
21. Ilankeeran P.K., Mohite P.M., Kamle S. Axial Tensile Testing of Single Fibres. Modern Mechanical Engineering, 2012, vol. 2, pp. 151–156. DOI: 10.4236/mme.2012.24020.
22. Agrawal M., Prabhakaran R.T.D. Effect of Fiber Sizing on Mechanical Properties of Carbon Reinforced Composites: A Review. Organic Polymer Material Research, 2019, vol. 1, no. 2, pp. 1–5. DOI: 10.30564/opmr.v1i2.1683
23. Norris R.E., Ennis B.L., Clarke R.J. et al. Initial assessment of alternative carbon fiber geometries for design of cost-effective compressive performance: Size effect studies. Composites Part B, 2025, vol. 296, art. 112181.
24. Program for calculating the geometric parameters of carbon fiber: certificate of state registration of the computer program No. 2023683908 dated November 10, 2023.
25. Kumar R., Mikkelsen L.P., Lilholt H., Madsen B. Understanding the mechanical response of glass and carbon fibres: stress–strain analysis and modulus determination. IOP Conference Series: Materials Science and Engineering, 2020, vol. 942, art. 012033. DOI: 10.1088/1757-899X/942/1/012033.
26. Curtis G.J., Milne J.M., Reynolds W.N. Non-hookean behaviour of strong carbon fibres. Nature, 1968, vol. 220, pp. 1024–1025.