D. A. Melnikov, A. Yu. Albagachiev, A. V. Slavin, A. A. Rybin The influence of vibration parameters on the structure formation processes in fiberglass based on glass fiber and dispersed fillers during continuous winding // Proceedings of VIAM. 2026. No. 8 (162). С. 82-91. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-8-82-91.

The influence of vibration parameters on the structure formation processes in fiberglass based on glass fiber and dispersed fillers during continuous winding

D. A. Melnikov1, A. Yu. Albagachiev2, A. V. Slavin1, A. A. Rybin1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
2Mechanical Engineering Research Institute of the Russian Academy of Sciences, Moscow, Russia; info@imash.ru

Abstract

This article examines the influence of vibration on a mandrel during the production of fiberglass pipes using the continuous winding method. Porosity reduction mechanisms associated with deaeration, improved filler wetting, and vibration compaction of the structure are considered. The influence of vibration frequency and amplitude on the pore volume fraction was experimentally determined. The maximum porosity reduction was 69,8 % at a frequency of 100 Hz and an amplitude of 0,4 mm. A regression model for predicting porosity and optimizing process parameters was developed.

Keywords
polymer composite materials, fiberglass, pipes, continuous winding, modeling, vibration impact
Reference list
  1. Aminov L.A. Use of Fiberglass Pipes to Improve the Pipeline System. Aktualnye problemy voyenno-nauchnykh issledovaniy, 2022, no. 12, pp. 15–18.
  2. Ivanov S.V. Fiberglass – a Composite Material for Pipes. Truboprovody i ekologiya, 2001, no. 2, p. 7.
  3. Modern Composite Materials. Ed L. Brautian, R. Krok. Moscow: Mir, 1970, 672 p.
  4. Krysin V.N., Krysin M.V. Technological Processes of Molding, Winding, and Gluing Structures. Moscow: Mashinostroenie, 1989, 240 p.
  5. Kablov E.N., Gunyaev G.M., Ilchenko S.I. et al. Structural carbon fiber reinforced plastics with increased conductivity. Aviatsionnye materialy i tekhnologii, 2004, no. 2, pp. 25–36.
  6. Veshkin E.A., Slavin A.V., Postnova M.V., Apalkova A.V. The role of temperature-time curing conditions in the formation of unidirectional and equally strong carbon fiber plastics properties. Aviation materials and technologies, 2025, no. 2 (79), pp. 59–71. Available at: http://www.journal.viam.ru (accessed: May 19, 2026). DOI: 10.18577/2713-0193-2025-0-2-59-71.
  7. Nacharkina A.V., Valueva M.I., Zelenina I.V., Shosheva A.L. High-temperature carbon fiber reinforced plastics based on bismaleinimide binders. Aviation materials and technologies, 2024, no. 4 (77), pp. 43–61. Available at: http://www.journal.viam.ru (accessed: May 19, 2026). DOI: 10.18577/2713-0193-2024-0-4-43-61.
  8. Prokopenkov V.G., Morozov Yu.A., Petrov A.I. Regarding density determination of glass reinforced plastics based on hollow fibers. Aviation materials and technologies, 2025, no. 3 (80), pp. 83–95. Available at: http://www.journal.viam.ru (accessed: May 19, 2026). DOI: 10.18577/2713-0193-2025-0-3-83-95.
  9. Bolotin V.V. Delaminations in composite structures: Its origin, buckling, growth and stability. Composites. Part B: Engineering, 1996, vol. 27, is. 2, pp. 129–145. DOI: 10.1016/1359- 8368(96)00035-6.
  10. Kushnir S. Ya., Gorkovenko A. I., Gerber A. D., Ignatko V. M. Strength characteristics of fiberglass pipes and loss of pipeline stability. Izvestiya vysshikh uchebnykh zavedeniy, 2003, no. 3 (39), pp. 55–56.
  11. Gulyaev I.N., Klimenko O.N., Lonskii S.L., Slavin A.V., Cherfas L.V. Determination of the composition and structure of polymer composite materials. Aviation materials and technologies, 2025, no. 4 (81), pp. 32–47. Available at: http://www.journal.viam.ru (accessed: May 19, 2026). DOI: 10.18577/2713-0193-2025-0-4-32-47.
  12. Adegova L.A., Bobrysheva M.V., Shcherbinina A.E. Study of the Loss of Buckling of a Cylindrical Shell Made of Composite Material. Vestnik Sibirskogo gosudarstvennogo avtomobilno-dorozhnogo universiteta, 2021, vol. 18, no. 3 (79), pp. 330–350.
  13. Lizin V.T., Pyatkin V.A. Design of Thin-Walled Structures. Moscow: Mashinostroenie, 1994. 381 p.
  14. Tsyplakov O.G. Scientific Foundations of Composite-Fiber Materials Technology: in 2 parts. Perm: Perm Book Publ. House, 1985, part 2, 274 p.
  15. Adler Yu.P., Markova E.V., Granovsky Yu.V. Planning an Experiment in the Search for Optimal Conditions. Moscow: Nauka, 1976, 279 p.
  16. Khoun L., Centea T., Hubert P. Characterization methodology of thermoset resins for the processing of composite materials – case study: CYCOM 890RTM epoxy resin. Journal of Composite Material, 2010, vol. 44, pp. 1397–1415.