Re and Ru influence on the microstructure formation and phase composition of single-crystal nickel-based superalloys during heat treatment and high-temperature creep.
1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
Samples of rhenium-containing alloy VIN4M and rhenium-ruthenium-containing alloys VZhM8 and VZhM10 after complete heat-treatment were studied. It was shown that interphase dislocations are observed in the axes of dendrites. In the structure of the VIN4M alloy, the boundaries of large y'-phase particles are decorated with dislocation clusters forming regular networks. The misfit in the VIN4M alloy is 0,60 % for large formations of the y'-phase in the interaxial spaces and 0,63 % for y'-phase particles in the axes of dendrites. The lowest misfit value of 0,46 % was obtained for the VZhM8 alloy, the highest 0,97 % – for the VZhM10 alloy. Stacking faults in the alloys are formed in γ-interlayers between lattice mismatch dislocations at the opposite boundaries of adjacent particles.
- Kablov E.N. Materials and technologies of VIAM for «Aviadvigatel». Permskiye aviatsionnye dvigateli, 2014, no. 31, pp. 43–47.
- Shalin R.E., Svetlov I.L., Kachanov E.B. et al. Single crystals of nickel heat-resistant alloys. Moscow: Mashinostroenie, 1997, 336 p.
- Visik E.M., Bityutskaya O.N., Gerasimov V.V., Pilipenko A.A., Moiseev A.S. Features of production of large casting turbine blades by directional crystallization of nickel corrosion resistent superalloy. Aviation materials and technologies, 2025, no. 2 (79), pp. 3–12. Available at: http://www.journal.viam.ru (accessed: August 25, 2025). DOI: 10.18577/2713-0193-2025-0-2-3-12.
- Min P.G., Vadeev V.E. The development and introduction into serial production of the new superalloy VZhL125 for the advanced aviation engines vanes. Aviation materials and technologies, 2023, no. 1 (70), pp. 3–16. Available at: http://www.journal.viam.ru (accessed: August 25, 2025). DOI: 10.18577/2713-0193-2023-0-1-3-16.
- Tolorayya V.N., Kablov E.N., Demonis I.M. Technology of producing single-crystal castings of turbine blades of gas turbine engines of a given crystallographic orientation from rhenium-containing heat-resistant alloys. Casting heat-resistant alloys. Effect of S.T. Kishkin. Moscow: Science, 2006, pp. 206–219.
- Argence D., Vernault C., Desvallées Y., Fournier D. MC-NG: a 4th generation single-crystal superalloy for future aeronautical turbine blades and vanes. Superalloys 2000. Pennsylvania: Minerals, Metals & Materials Society, 2010, pp. 829–837.
- Walston S., Cetel A., MacKay R. et al. Joint development of a fourth generation single crystal superalloy. Superalloys 2004. Pennsylvania: Minerals, Metals & Materials Society, 2004, pp. 15–24.
- Koizumi Y., Kobayashi T., Yokokawa T. et al. Development of next-generation Ni-base single crystal superalloys. Superalloys 2004. Pennsylvania: Minerals, Metals & Materials Society, 2004, pp. 35–43.
- Fifth generation nickel based single crystal superalloy TMS-196 (Development under NIMS / IHI collaboration), 2006, 4 p. Available at: http://sakimori.nims.go.jp (дата обращения: June 05, 2025).
- Sato A., Harada H., Yeh An.-C. et al. A 5th generation SC superalloy with balanced high temperature properties and processability. Superalloys 2008. Pennsylvania: Minerals, Metals & Materials Society, 2008, pp. 131–138.
- Petrushin N.V., Elyutin E.S., Visik E.M., Golynets S.A. Development of a single-crystal heat- resistant nickel alloy of the 5th generation. Metally, 2017, no. 6, pp. 38–51.
- Elyutin E.S. Development of heat-resistant nickel alloys of the 5th and 6th generations with increased long-term strength for single-crystal blades of advanced aircraft gas turbine engines: thesis abstract, Cand. Sc. (Tech.). Moscow, 2023, 27 p.
- Utada S., Yokokawa T., Kobayashi T. et al. Challenging the limit of strengthening by γ/γ′ lattice misfit on the high temperature creep properties of Ni-base single crystal superalloy. Metallurgical and Material Transaction A, 2026, vol. 57, pp. 1794–1812. DOI: 10.1007/s11661-025-08089-5.
- Harada H. Development of Superalloys for 1700 °C ultra-efficient gas turbines. Proceedings of the 9th Liége-Conference on Materials for Advanced Power Engineering. Julich, 2010, pp. 604–614. Available at: http://hdl.handle.net/2268/20701 (accessed: June 07, 2025).
- Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel- based superalloys alloyed with rhenium and ruthenium (review). Part 1. Aviation materials and technologies, 2023, no. 1 (70), pp. 30–50. Available at: http://www.journal.viam.ru (accessed: June 04, 2025). DOI: 10.18577/2713-0193-2023-0-1-30-50.
- Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel- based superalloys alloyed with rhenium and ruthenium (review). Part 2. Aviation materials and technologies, 2023, no. 2 (71), pp. 3–22. Available at: http://www.journal.viam.ru (accessed: June 04, 2025). DOI: 10.18577/2713-0193-2023-0-2-3-22.
- Reed R.C. The Superalloys. Fundamentals and Applications. Cambridge: United Kingdom at University Press, 2006, 372 p.
- Huang M., Zhu J. An overview of rhenium effect in single-crystal superalloys. Rare Metals, 2016, vol. 35, pp. 127–139. DOI: 10.1007/s12598-015-0597-z.
- Ding Q., Li S., Chen L.-Q. et al. Re segregation at interfacial dislocation network in nickel-base superalloys. Acta Materialia, 2018, vol. 154, pp. 137–146. DOI: 10.1016/j.actamat.2018.05.025.
- Rae C.M.F., Karunaratne M.S.A., Small C.J. et al. Topologically close packed phases in an experimental rhenium-containing single crystal superalloy. Superalloy 2000. Pennsylvania: Minerals, Metals & Materials Society, 2000, pp. 767–776.
- Cheng Y., Zhao X., Yue Q. et al. The nucleation of δ phases triggered by the stacking faults in a single crystal superalloy. Materials Research Letters, 2023, vol. 11, no. 11, pp. 957–963. DOI: 10.1080/201663831.2023.2272809.
- Matuszewski K., Rettig R., Matysiak H. et al. Effect of ruthenium on the precipitation of topologically close packed phases in Ni-base superalloys of 3rd and 4th generation. Acta Materialia, 2015, vol. 95, pp. 274–283. DOI: 10.1016/j.actamat.2015.05.033.
- Mori Y., Yokokawa T., Kobayashi T. et al. Phase stability of nickel-base single-crystal superalloys containing iridium substituting for ruthenium. Materials Transactions, 2016, vol. 57 (10), pp. 1845–1848. DOI: 10.2320/matertrans.MAW201606.
- Buntushkin V.P., Burkina V.I., Timofeeva O.B., Yushakova F.V. Composition, structure and properties of single-crystal alloy VKNA-25. Aviatsionnye materialy i tekhnologii, 2008, no. 1, pp. 10–14.
- Aviation materials: reference book in 13 vols Ed. E.N. Kablov. 7th ed., rev. and add. Moscow: NRC «Kurchatov Institute» – VIAM, 2022, vol. 3: Casting heat-resistant and intermetallic alloys on a nickel base, 192 p.
- Bazyleva O.A., Arginbaeva E.G., Nazarkin R.M., Nefedov D.G. Structural and phase parameters of intermetallic nickel alloys. Liteynoe proizvodstvo, 2015, no. 3, pp. 17–19.
- Nikolaev S.V. Combined alloying of nickel with rhenium and transition metals of groups V–VI: thesis abstract of Cand. Sci. (Chem.). Moscow, 2014, 24 p.
- Kevin E., Yoon A., Ronald D. et al. Effects of rhenium addition on the temporal evolution of the nanostructure and chemistry of a model Ni–Cr–Al superalloy. Part I. Experimental observations Acta Materialia, 2007, vol. 55, pp. 1145–1157.
- Logunov A.V., Shmotin Yu.N., Khramin R.V., Zavodov S.A., Danilov D.V. Influence of alloying elements on the strength properties of heat-resistant nickel alloys for gas turbine disks. Electrometallurgiya, 2021, no. 3, pp. 2–13.
- Kuzmina N.A., Pyankova L.A. Control of crystallographic orientation of monocrystalline nickel castings heat-resistant alloys by x-ray diffractometry. Trudy VIAM, 2019, no. 12 (84), pp 11–19. Available at: http://www.viam-works.ru (accessed: August 25, 2025). DOI: 10.18577/2307-6046-2019-0-12-11-19.
- Kuzmina N.A., Ostroukhova G.A. Blockiness and substructure in single-crystal castings of nickel heat-resistant alloys. Trudy VIAM, 2022, no. 7 (113), pp. 13–26. Available at: http://www.viam- works.ru (accessed: August 25, 2025). DOI: 10.18577/2307-6046-2022-0-7-13-26.