Complex protection of beryllium alloys from oxidation and sublimation of toxic beryllium vapors

Rosenenkova V.A., Solntsev St.S., Mironova N.A.
Rosenenkova V.A., Solntsev St.S., Mironova N.A. Complex protection of beryllium alloys from oxidation and sublimation of toxic beryllium vapors // Proceedings of VIAM. 2013. No. 5. URL: https://viam-works.ru/en/journal/2013/5/3
Abstract

Composite protective coating providing high-quality protection of beryllium from oxidation and sublimation of toxic beryllium vapors at high-temperature and long treating is developed.