G.S. Sevalnev , A.V. Sheremetiev , T.G. Sevalneva , K.V. Dulnev Study of the change in electrical resistance depending on the structure evolution in austenitic nitrogen‑containing corrosion‑resistant steel VNS53‑Sh // Proceedings of VIAM. 2026. No. 7 (161). С. 16–25. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-7-16-25.

Study of the change in electrical resistance depending on the structure evolution in austenitic nitrogen‑containing corrosion‑resistant steel VNS53‑Sh

G.S. Sevalnev , A.V. Sheremetiev , T.G. Sevalneva , K.V. Dulnev
Abstract

The change in electrical resistivity of austenitic nitrogen-containing steel VNS53-Sh has been studied depending on heat treatment in the temperature range of 200–1000 °C. Using the IACS standard resistivity measurement method, the relationship between electrical resistivity and structural-phase transformations has been established, including chromium nitride precipitation, formation of discontinuous decomposition zones, and recrystallization. Threshold values of electrical resistivity for non-destructive testing of the phase composition of the steel under production conditions have been determined.
 

Keywords
nitrogen-containing steel, complex-alloyed austenitic steel, microstructure, phase composition, hardness, specific electrical resistivity
Reference list
  1. Filippov M.A., Litvinov V.S., Nemirovsky Yu.R. Steels with metastable austenite. Moscow: Metallurgiya, 1988, 256 p.
  2. Mushnikova S.Yu., Kostin S.K., Sagaradze V.V., Kataeva N.V. Structure, properties and resistance to stress corrosion cracking of nitrogen-containing austenitic steel strengthened by thermomechanical treatment. Fizika metallov i metallovedenie, 2017, vol. 118, no. 11, pp. 1223–1235. DOI: 10.7868/S0015323017110092.
  3. Svyazhin A.G., Kaputkina L.M. Nitrogen and high-nitrogen steels. Industrial technologies and properties. Izvestiya vysshikh uchebnykh zavedeniy. Chernaya Metallurgiya, 2019, no. 62 (3), pp. 173–187. DOI: 10.17073/0368-0797-2019-3-173-187.
  4. Kushnereva D.S., Sapozhnikov G.V. Study of the properties of new high-strength stainless steels. Khimicheskaya fizika i mezoskopiya, 2019, vol. 21, no. 1, pp. 39–44.
  5. Sevalnev G.S., Druzhinina M.E., Voznesenskaya N.M. et al. Structural changes in surface layers during wear testing of high-strength austenitic steel VNS-53. Metally, 2023, no. 4, pp. 76–81.
  6. Parmenova O.N. Effect of Cold Deformation on the Corrosion Resistance of Austenitic Steels in Seawater. Ural School of Young Metallurgists: Coll. of Materials and Reports of the XIX Int. Scientific and Technical. Ural School-Seminar of Metallurgists – Young Scientists. Ekaterinburg: Ural Univ. Publ. House, 2018, pp. 332–333.
  7. Bubnov V.A. Mechanism of the Transition of Austenite to Martensite during Cold Plastic Deformation of Austenitic Steels. Izvestiya vysshikh uchebnykh zavedeniy. Mashinostroyenie, 2018, no. 11 (704), pp. 14–19.
  8. Kostina M.V., Kudryashov A.E., Spitsina I.V. et al. Study of the Effect of Hot Rolling and Heating Temperature for Quenching on the Structure and Hardness of Fe–13%Cr Steels Alloyed with Nitrogen, Vanadium, and Niobium. Metally, 2024, no. 3, pp. 21–31. DOI: 10.31857/S0869573324032131.
  9. Lukin E.I., Blinov V.M., Bannykh I.O. et al. Effect of cold rolling on the structure and mechanical properties of corrosion-resistant nitrogen-containing martensitic-austenitic-ferritic steel 03Kh17AN2F. Electrometallurgiya, 2025, no. 2, pp. 11–19. DOI: 10.31044/1684-5781-2025-0-2-11-19.
  10. Betsofen S.Ya., Lukin E.I., Ashmarin A.A. et al. Effect of Cold Rolling on the Phase Composition, Texture, and Residual Stresses in Steels with 15,9 and 17,7 % Mn. Russian Metallurgy (Metally), 2025, vol. 2025, no. 3, pp. 603–610. DOI: 10.1134/S0036029525700168.
  11. Sevalnev G.S., Dulnev K.V., Ryzhkov P.V., Leonov A.V., Voznesenskaya N.M. Optimization of heat treatment for high-strength corrosion-resistant nitrogen-containing steel to produce seamless thin-walled tubes. Trudy VIAM, 2025, no. 8 (150), pp. 41–52. Available at: http://www.viam-works.ru (accessed: October 11, 2025). DOI: 10.18577/2307-6046-2025-0-8-41-52.
  12. Sevalnev G.S., Gromov V.I., Dulnev K.V., Sevalneva T.G. Contact endurance of nitrogenous austenitic-martensitic steels with different hardening mechanism. Aviation materials and technologies, 2024, no. 2 (75), pp. 3–14. Available at: http://www.journal.viam.ru (accessed: January 25, 2026). DOI: 10.18577/2713-0193-2024-0-2-3-14.
  13. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
  14. Pichugin S.S., Shitikov V.S., Golovkov A.N. Non-destructive methods for residual stress assessment. Trudy VIAM, 2024, no. 1 (131), pp. 101–112. Available at: http://www.viam-works.ru (accessed: January 11, 2026). DOI: 10.18577/2307-6046-2024-0-1-101-112.
  15. Lednev I.S. Magnetic methods of non-destructive testing of aircraft parts. Aviation materials and technologies, 2024, no. 1 (74), pp. 111–120. Available at: http://www.journal.viam.ru (accessed: January 11, 2026). DOI: 10.18577/2713-0193-2024-0-1-111-120.
  16. Lin G., Zhang Z., Wang H. et al. Enhanced strength and electrical conductivity of Al–Mg–Si alloy by thermo-mechanical treatment. Materials Science and Engineering: A, 2016, vol. 650, pp. 210–217.
  17. Cui X., Wu Y., Zhang G. et al. Study on the improvement of electrical conductivity and mechanical properties of low alloying electrical aluminum alloys. Composites. Part B: Engineering, 2017, vol. 110, pp. 381–387.
  18. Bannykh I.O. Structural features and prospects for the application of high-nitrogen austenitic steels. Metallovedenie i termicheskaya obrabotka metallov, 2019, no. 5, pp. 22–29.
  19. Bannykh O.A., Blinov V.M. On the effect of discontinuous decomposition on the structure and properties of high-nitrogen steels and on methods for suppression thereof. Steel research, 1991, vol. 62, no. 1, pp. 38–45.
  20. Sagaradze V.V., Fomina O.V., Vikhareva T.V. et al. Features of delta-ferrite decomposition in nitrogen-containing austenitic steels. Fizika metallov i metallovedenie, 2018, vol. 119, no. 3, pp. 296–302.
  21. Belomyttev M.Yu. Regularities of austenite grain formation in 12% chromium heat-resistant ferritic-martensitic steels. Izvestiya vysshikh uchebnykh zavedeniy. Chernaya Metallurgiya, 2023, vol. 66, no. 2, pp. 168–176.
  22. Bannykh I.O. Correlation of grain structure and mechanical properties of high-nitrogen austenitic steel 02Kh20AG10N4MFB after annealing. Deformatsiya i razrusheniye materialov, 2015, no. 12, pp. 25–29.
  23. Potak Ya.M. High-strength steels. Moscow: Metallurgiya, 1972, 208 p.
  24. Eliseev E.A., Leonov A.V., Voznesenskaya N.M., Nefedkin D.Yu. Study of structure changes under the influence of various technological factors on the properties of cold-rolled strip made of nickel-beryllium alloy grade 97NL-VI. Problemy chernoy metallurgii i materialovedeniya, 2022, no. 1, pp. 29–34.