Bending tests of aircraft floor sandwich honeycomb panel samples

Shershak P.V., Yakovlev N.O., Barannikov A.A.
Shershak P.V., Yakovlev N.O., Barannikov A.A. Bending tests of aircraft floor sandwich honeycomb panel samples // Proceedings of VIAM. 2026. No. 5. DOI: 10.18577/2307-6046-2026-0-5-159-173. URL: https://viam-works.ru/en/journal/2026/5/13
Keywords
sandwich honeycomb panels, floor panels, sandwich structures, bending, three-point bending, four-point bending, deflection
Abstract

The work examines the requirements for conducting bending tests of aircraft floor sandwich honeycomb panel samples and the most common errors in the interpretation of test methods. An analysis of the requirements of aircraft developers for property indicators during bending tests is conducted, along with data from manufacturers of aircraft floor panels. Due to the lack of standards establishing requirements specifically for the bending tests of floor panels, the work provides justifications for applying methodologies that differ from GOST standards, which set requirements for testing sandwich structures.

Reference list
  1. Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, рр. 907–916. DOI: 10.31857/S0869587323100055.
  2. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 122–144. Available at: http://www.journal.viam.ru (accessed: November 08, 2025). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  3. Shershak P.V., Yakovlev N.O., Shokin G.I., Kutsevich K.E., Popkova E.A. Evaluation method and factors influencing the bonding quality between face and honey-comb cores in floor and interior aircraft panels. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 81–88. DOI: 10.18577/2071-9140-2020-0-2-81-88.
  4. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  5. Komarov V.A., Kutsevich K.E., Pavlova S.A., Tyumeneva T.Yu. Optimization of three-layer honeycomb floor panels made of low-flammability polymer composite materials based on high-strength carbon and glass fibers and an adhesive binder. Vestnik Samarskogo universiteta. Ser.: Aerokosmicheskaya tekhnika, tekhnologii i mashinostroyenie, 2020, vol. 19, no. 3, pp. 51–72. DOI: 10.18287/2541-7533-2020-19-3-51-72.
  6. Ilyushenkov S.F., Batizat D.V., Sereduta P.I. Development of three-layer honeycomb floor panels for passenger aircraft made of polymer composites. Polimernye materialy, 2025, no. 3 (310), pp. 14–21.
  7. Mikhailin Yu.A. Fibrous polymer composite materials in engineering. St. Petersburg: Scientific Foundations and Technologies, 2023, 720 p.
  8. Giyasov B.I., Seregin N.G., Seregin D.N. Three-layer panels made of polymer composite materials: a tutorial. Moscow: ASV Publishing House, 2015, 64 p.
  9. Mikhailin Yu.A. Special polymer composite materials. St. Petersburg: Scientific Foundations and Technologies, 2008, 660 p.
  10. Characteristics of Hexcel honeycomb cores. Available at: https://www.hexcel.com/Resources/Data Sheets/Honeycomb (accessed: November 08, 2025).
  11. Collins Aerospace's three-layer honeycomb floor panels. Available at: https://www.collinsaerospace.com/what-we-do/industries/business-aviation/cabin/structures/honeycomb-panels (accessed: November 08, 2025).
  12. Shershak P.V., Shokin G.I., Egorov V.N. Technological Features of the Production of Three-Layer Honeycomb Aircraft Floor Panels. Aviatsionnaya promyshlennost, 2014, no. 3, pp. 34–42.
  13. Technical Requirements. Three-Layer Honeycomb Panels for the Manufacture of the RRJ-95 Aircraft Floor. Available at: https://rostender.info/region/moskva-gorod/32180045-tender-dopolnenie-perechnya-postavshchikov-trehslojnyh-sotovyh-panelej-pola-dlya-vs-semejstvarrj?ysc
  14. lid=mf5qwacqiy574752643 (accessed: November 08, 2025).
  15. Technical requirements for composite panels of the passenger cabin floor, the floor of the flight deck, side panels, partitions and ceilings of the flight deck of the MC21 aircraft. Available at: https://tenmon.ru/1/31806547983 (accessed: November 08, 2025).
  16. Barannikov A.A., Veshkin E.A., Postnov V.I., Strelnikov S.V. On the issue of production of floor panels from polymer composite materials for aircraft (review article). Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2017, vol. 19, no. 4 (2), pp. 198–213.
  17. Erasov V.S., Sibayev I.G. Scheme for the development and evaluation of properties of structural aviation composite materials. Aviation materials and technologies, 2023, no. 1 (70), pp. 61–81. Available at: http://www.journal.viam.ru (accessed: November 08, 2025). DOI: 10.18577/2713-0193-2023-0-1-61-81.
  18. Sarychev I.A., Serkova E.A., Khmelnitsky V.V., Zastroginа O.B. Thermosetting binders for aircraft floor panel materials (review). Trudy VIAM, 2019, no. 7 (79), pр. 26–33. Available at: http://www.viam-works.ru (accessed: November 08, 2025). DOI: 10.18577/2307-6046-2019-0-7-26-33.
  19. Strelnikov S.V., Petukhov V.I., Postnov V.I., Shvets N.I. New solutions in the technology of manufacturing prepregs for interior panels. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2011, vol. 13, no. 4 (2), pp. 498–507.
  20. Starkov A.I., Kutsevich K.E., Tyumeneva T.Yu., Petrova A.P. Low-combustibility adhesive prepregs designed for the manufacture of integral and three-layer honeycomb structures aircraft technology. Trudy VIAM, 2022, no. 5 (111), рр. 41–52. Available at: http://www.viam-works.ru (accessed: November 25, 2025). DOI: 10.18577/2307-6046-2022-0-5-41-52.
  21. Technical specifications of floor panels from The Gill Corporation. Available at: https://www.thegillcorp.com/products/floor-panels/ (accessed: November 08, 2025).
  22. Technical specifications for floor panels from AIM Altitude Ltd. Available at: https://www.yumpu.com/pt/document/view/52337885/aim-composites-ltd-flitelam-uns2-technical-data-lindberg-lund-as (accessed: November 08, 2025).
  23. Technical characteristics of floor panels from Euro-Composites group. Available at: https://www.euro-composites.com/en/portfolio/aviation/ (accessed: November 08, 2025).
  24. Showa Aircraft Industry Floor Panel Specifications. Available at: https://www.showaaircraft.com/product-category/honeycomb-panel/ (accessed: November 08, 2025).
  25. Erasov V.S., Sibayev I.G., Sutubalov A.I. Testing of samples from three-layer structures with honeycomb filler. Trudy VIAM, 2025, no. 10 (152), pp. 133–155. Available at: http://www.viam-works.ru (accessed: November 08, 2025). DOI: 10.18577/2307-6046-2025-0-10-133-155.
  26. Shershak P.V., Kurilenko N.V., Kosarev V.A. Influence of the height of the polymer honeycomb filler on the stiffness of three-layer honeycomb aircraft floor panels. Aviatsionnaya promyshlennost, 2016, no. 2, pp. 49–52.
  27. Dushin M.I., Ermolaev A.M., Katyrev I.Ya. et al. Carbon fiber reinforced plastics in floor panels of three-layer structure. Aviatsionnaya promyshlennost, 1978, no. 6, pp. 8–12.
  28. Abramova M.G., Lutsenko A.N., Varchenko E.A. Concerning the aspects of validation of climate resistance of airborne materials at all life cycle stages (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 86–94. DOI: 10.18577/2071-9140-2020-0-1-86-94.