Changes in the properties of aviation PCM after 6 years of exposure in typical climatic zones of Russia

Part 1. Moisture transfer and deformability
Kornienko G.V., Dvirnaya E.V., Startsev O.V., Krotov A.S.
Kornienko G.V., Dvirnaya E.V., Startsev O.V., Krotov A.S. Changes in the properties of aviation PCM after 6 years of exposure in typical climatic zones of Russia. Part 1. Moisture transfer and deformability // Proceedings of VIAM. 2026. No. 5. DOI: 10.18577/2307-6046-2026-0-5-75-93. URL: https://viam-works.ru/en/journal/2026/5/6
Keywords
fiber reinforced polymers, outdoor weathering, moisture diffusion, plasticization, shear modulus, Fick's law of diffusion, Langmuir adsorption model
Abstract

Studies of changes in the diffusion characteristics of glass and carbon fiber reinforced polymers in their initial state and after exposure for 6 years in 5 climatic zones of the Russian Federation have been conducted. The value of the coefficient of determination of the approximation by the Fick and Langmuir models for the weighing results obtained at the stages of drying and humidification is equal to 1.00. Using the non-destructive plate twist method during conditioning, diagrams of shear modulus change were obtained and then approximated using the similar models. The modeling results allowed to distinguish the influence of climatic zones on the properties of the materials.

Reference list
  1. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), pp. 70–80. Available at: http://www.journal.viam.ru (accessed: August 06, 2025). DOI: 10.18577/2713-0193-2021-0-4-70-80.
  2. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 122–144. Available at: http://www.journal.viam.ru (accessed: August 06, 2025). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  3. Raveendran P., Alagarsamy S.V., Chanakyan C. et al. A hybrid approach for prediction of machining performances of glass fiber reinforced plastic (Epoxy) composites. Surface Topography: Metrology and Properties, 2021, vol. 9, no. 3, art. 035046.
  4. Startsev V.O., Slavin A.V. Carbon and glass reinforced polymer based on solventfree binders resistance to the impact of a moderate cold and moderate warm climate. Trudy VIAM, 2021, no. 5 (99), pp. 114–126. Available at: http://www.viam-works.ru (accessed: July 20, 2025). DOI: 10.18577/2307-6046-2021-0-5-114-126.
  5. Gulyev I.N., Zelenina I.V., Valevin E.O., Khaskov M.A. Influence of climatic ageing on the properties of high-temperature carbon fiber reinforced plastics. Trudy VIAM, 2021, no. 2 (96), pp. 39–51. Available at: http://www.viam-works.ru (accessed: July 20, 2025). DOI: 10.18577/2307-6046-2021-0-2-39-51.
  6. Chauhan V., Kärki T., Varis J. Review of natural fiber-reinforced engineering plastic composites, their applications in the transportation sector and processing techniques. Journal of Thermoplastic Composite Materials, 2022, vol. 35, no. 8, pp. 1169–1209.
  7. Huang S., Yan L., Kasal B., Wei Y. Moisture diffusion and tensile properties of epoxy-based and polyurethane-based flax-glass hybrid FRP under hygrothermal and weathering environments. Composites. Part B: Engineering, 2023, vol. 267, art. 111049.
  8. Xu B., van den Hurk B., Liu T. et al. Effect of UV-water weathering on the mechanical properties of flax-fiber-reinforced polymer composites. Polymer Composites, 2024, vol. 45, no. 5, pp. 4266–4280.
  9. Sawpan M.A., Alshahrani H., Kafi A. Durability of pultruded GFRP rebar subjected to natural weathering in alkaline solution for 10 years. Journal of Polymers and the Environment, 2023, vol. 31, no. 3, pp. 1090–1101.
  10. Namrata B., Pai Y., Nair V.G. et al. Analysis of aging effects on the mechanical and vibration properties of quasi-isotropic basalt fiber-reinforced polymer composites. Scientific Reports, 2024, vol. 14, no. 1, art. 26730.
  11. Kim J., Kang S., Seong I. et al. Advancing CFRP durability: Interfacial and weathering performance of epoxy and acrylic matrices. Composites. Part B: Engineering, 2025, vol. 297, art. 112315.
  12. Semitekolos D., Konstantopoulos G., Trompeta A.F. et al. Mechanical Properties, Surface Assessment, and Structural Analysis of Functionalized CFRPs after Accelerated Weathering. Polymers, 2021, vol. 13, no. 23, art. 4092.
  13. Nezafatkhah S., Margoto O.H., Sassani F., Milani A.S. Understanding natural and accelerated weathering degradation mechanisms of glass and natural fiber composites: A review. Journal of Reinforced Plastics and Composites, 2025, vol. 45, pp. 1–23. DOI: 10.1177/07316844251337240.
  14. Rohem Gualberto H., dos Reis J.M.L., Calixto de Andrade M. et al. Effect of outdoor environmental exposure on the mechanical behavior of steel/GFRP single-lap joints. The Journal of Adhesion, 2024, vol. 100, no. 14, pp. 1323–1346.
  15. Nishizaki I., Sakuraba H., Tomiyama T. Durability of pultruded GFRP through ten-year outdoor exposure test. Polymers, 2015, vol. 7, no. 12, pp. 2494–2503.
  16. Sousa J.M., Correia J.R., Cabral-Fonseca S. Durability of glass fibre reinforced polymer pultruded profiles: comparison between QUV accelerated exposure and natural weathering in a Mediterranean climate. Experimental Techniques, 2016, vol. 40, no. 1, pp. 207–219.
  17. Srivabut C., Khamtree S., Homkhiew C. et al. Comparative effects of different coastal weathering on the thermal, physical, and mechanical properties of rubberwood–latex sludge flour reinforced with polypropylene hybrid composites. Composites. Part C: Open Access, 2023, vol. 12, art. 100383.
  18. Rosa I.C., Castelo A., Sousa J.M. Natural Weathering of GFRP Structures: Case Studies, Data Survey, and Proposal of a Moisture Conversion Factor for Durability Design. Journal of Composites for Construction, 2024, vol. 28, no. 6, art. 04024063.
  19. Evdokimov A.A., Petrova A.P., Pavlovskiy K.A., Gulyaev I.N. The influence of climatic ageing on the properties of PCM-based epoxy resin systems. Trudy VIAM, 2021, no. 3 (97), pp. 128–136. Available at: http://www.viam-works.ru (accessed: August 08, 2025). DOI: 10.18577/2307-6046-2021-0-3-128-136.
  20. Shi Y., Qin J., Tao Y. et al. Natural weathering severity of typical coastal environment on polystyrene: Experiment and modeling. Polymer Testing, 2019, vol. 76, pp. 138–145.
  21. Starkova O., Aiello M.A., Aniskevich A. Long-term moisture diffusion in vinylester resin and CFRP rebars: A 20-year case study. Composites Science and Technology, 2023, vol. 242, art. 110167.
  22. Osa-Uwagboe N., Silberschmidt V.V., Baxevanakis K.P., Demirci E. Effects of moisture absorption on penetration performance of FRP sandwich structures. Composite Structures, 2024, vol. 344, art. 118319.
  23. Sugai M., Koyama M. Effect of moisture on interfacial and mechanical properties of GFRP containing particles of two sizes. Results in Materials, 2023, vol. 17, art. 100356.
  24. Svetlik-Haley S., Karbhari V.M. Humidity and immersion based hygrothermal aging of pultruded GFRP composites: Moisture uptake and diffusion. Journal of Composite Materials, 2025, vol. 59, no. 8, pp. 991–1011.
  25. Sun Y., Jin Z., Zhang X., Zhu D. Experimental and molecular dynamics study on the deterioration mechanism of GFRP bars in distilled water and salt solution environments. Journal of Building Engineering, 2022, vol. 60, art. 105224.
  26. Wang P., Wu H.L., Leung C.K., Li W.W. Hygrothermal aging effects on the diffusion-degradation process of GFRP composite: Experimental study and numerical simulation. Construction and Building Materials, 2023, vol. 379, art. 131075.
  27. Wang P., Wu H.L., Leung C.K. Hygrothermal aging effect on the water diffusion in glass fiber reinforced polymer (GFRP) composite: experimental study and numerical simulation. Composites Science and Technology, 2022, vol. 230, art. 109762.
  28. da Silva G.A.S., d’Almeida J.R.M., Cardoso D.C.T. Investigation on moisture absorption behavior on GFRP and neat epoxy systems in hygrothermal salt fog aging. Composites. Part B: Engineering, 2024, vol. 272, art. 111214.
  29. Startseva L.T., Panin S.V., Startsev O.V., Krotov A.S. Diffusion of moisture in fiberglass after their climatic aging. Doklady akademii nauk, 2014, vol. 456, no. 3, pp. 305–309.
  30. Startsev V.O., Lebedev M.P., Khrulev K.A. Effect of outdoor exposure on the moisture diffusion and mechanical properties of epoxy polymers. Polymer testing, 2018, vol. 65, pp. 281–296.
  31. Kornienko G.V., Startsev O.V., Krotov A.S., Koval T.V. Dependence modeling of the CFRP shear modulus on moisture content. Aviation materials and technologies, 2025, no. 3 (80), pp. 161–178. Available at: http://www.journal.viam.ru (accessed: September 18, 2025). DOI: 10.18577/2713-0193-2025-0-3-161-178.
  32. Lebedev M.P., Startsev O.V., Kornienko G.V. Diffusion model of elastic properties of polymer composite materials in a humid environment. Doklady Rossiyskoy akademii nauk. Khimiya, nauki o materialakh, 2024, vol. 519, no. 1, pp. 25–31.
  33. Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R., Grashchenkov D.V. Complex research of influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis. Part 4. Natural climatic tests of polymeric composite materials on the basis of epoxy matrix. Trudy VIAM, 2016, no. 6, pp. 93–108. Available at: http://www.viam-works.ru (accessed: September 05, 2025). DOI: 10.18577/2307-6046-2016-0-6-11-11.
  34. Kutsevich K.E., Dementeva L.A., Lukina N.F. Properties and application of polymer composite materials based on glue prepregs. Trudy VIAM, 2016, no. 8, pp. 52–59. Available at: http://www.viam-works.ru (accessed: September 05, 2025). DOI: 10.18577/2307-6046-2016-0-8-7-7.
  35. Veligodskiy I.M., Koval T.V., Kurnosov A.O., Marakhovskiy P.S. Study of resistance of glass fiber reinforced plastic to natural weathering in different climatic conditions. Trudy VIAM, 2022, no. 11 (117), pp. 134–148. Available at: http://www.viam-works.ru (accessed: September 05, 2025). DOI: 10.18577/2307-6046-2022-0-11-134-148.
  36. Startsev V.O., Nechaev A.A. The influence of natural and accelerated weathering on the nanomodified CFRP’S strength. Aviation materials and technologies, 2023, no. 3 (72), pp. 134–151. Available at: http://www.journal.viam.ru (accessed: September 05, 2025). DOI: 10.18577/2713-0193-2023-0-3-134-151.
  37. Kablov E.N., Startsev V.O. Measurement and forecasting of materials samples’ temperature during weathering in different climatic zones. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 47–58. DOI: 10.18577/2071-9140-2020-0-4-47-58.
  38. Crank J. The mathematics of diffusion. Second edition. Oxford: Clarendon press, 1975, 414 p.
  39. Carter H.G., Kibler K.G. Langmuir-type model for anomalous moisture diffusion in composite resins. Open Journal of Composite Materials, 1978, vol. 12, pp. 118–131.
  40. Uzay C., Boztepe M.H., Bayramoğlu M., Geren N. Effect of post-curing heat treatment on mechanical properties of fiber reinforced polymer (FRP) composites. Materials Testing, 2017, vol. 59, no. 4, pp. 366–372.
  41. Sambayi P.M.K., Heyns P.S. Effects of multiple post cure cycles on properties of composite carbon fibre and epoxy materials. Journal of Composite Materials, 2023, vol. 57, no. 15, pp. 2467–2481.