Determination of additive elements in cobalt-based alloys by ICP AES method

Dvoretskov R.M., Savina K.V.
Dvoretskov R.M., Savina K.V. Determination of additive elements in cobalt-based alloys by ICP AES method // Proceedings of VIAM. 2026. No. 3. DOI: 10.18577/2307-6046-2026-0-3-167-182. URL: https://viam-works.ru/en/journal/2026/3/13
Keywords
analysis technique, cobalt alloys, microwave decomposition, dissolution of alloys, atomic emission spectrometry with inductively coupled plasma (AES ICP)
Abstract

A method is proposed for the simultaneous determination of the matrix element Co and alloying elements (Cr, Ni, W, Si, Mn, Fe, Mo, Ti, Ta, V) in cobalt alloys for various purposes by inductively coupled plasma atomic emission spectrometry with preliminary microwave sample opening. A scheme for dissolving samples of cobalt alloys of different grades in a microwave decomposition system in 2 stages is described, which ensures the complete transition of the elements into solution. Analytical lines of elements free from significant spectral influences are selected. The metrological characteristics of the method are evaluated based on the results of the analysis of reference materials.

Reference list
  1. Arzamasov B.N., Solovieva T.V., Gerasimov S.A. et al. Handbook of Structural Materials. Moscow: BMSTU Publ. House, 2005, 640 p.
  2. Sorokin V.G. Steels and Alloys. Brand Book. Moscow: Intermet Engineering, 2001, 608 p.
  3. Rosert R. Cobalt-Based Alloys for Surfacing. Avtomaticheskaya svarka, 2015, no. 5-6 (742), pp. 108–113.
  4. Usoltsev E.A. Development of Technology for Manufacturing Wear-Resistant Products from Cast Cobalt-Based Hard Alloys: thesis, Cand. Sc. (Tech.). Ekaterinburg, 2020, 115 p.
  5. Sviridov A.V., Evgenov A.G., Afansiev-Khodykin A.N., Galushka I.A. Brazing of a native wear-resistant stellite V5K on the working blades of the GTE from nickel super alloys. Aviation materials and technologies, 2022, no. 3 (68), pp. 27‒36. Available at: http://www.journal.viam.ru (accessed: June 16, 2025). DOI: 10.18577/2713-0193-2022-0-3-27-36.
  6. Demin D.V., Chugunov V.A. Modern understanding of materials in implantology. Dentistry – science and practice, development prospects: proc. Int. sci.-pract. conf. (Volgograd, October 24, 2024). Volgograd: VolSMU, 2024, pp. 56–60.
  7. Piskorsky V.P., Korolev D.V., Valeev R.A. et al. Magnet industry – problems and achievements. Physics and engineering of permanent magnets. Moscow: VIAM, 2018, pp. 3–50.
  8. Dvoretskaya E.V., Korolev D.V., Piskorskii V.P., Valeev R.A., Koplak O.V., Morgunov R.B. Magnetron sputtering of the iron shell and microinclusions in microwires PrDyFeCoB. Aviation materials and technologies, 2022, no. 2 (67), pp. 85–96. Available at: http://www.journal.viam.ru (accessed: June 16, 2025). DOI: 10.18577/2713-0193-2022-0-2-85-96.
  9. Kablov E.N., Ospennikova O.G., Davydova E.A., Buzenkov A.V., Valeev R.A., Morgunov R.B., Piskorskii V.P. Effect of annealing of Pr‒Dy‒Fe‒Co‒B alloy on its phase composition and properties of sintered magnets made from it. Metally, 2018, no. 2, pp. 28–32.
  10. Kablov E.N., Ospennikova O.G., Piskorskii V.P. et al. Magnetic properties and spin dynamics of multilayer granular CoFeB‒SiO2 heterostructures. Fizika tverdogo tela, 2016, vol. 58, no. 6, pp. 1086–1092.
  11. Dvoretskov R.M., Karachevtsev F.N., Isachenko Ya.A., Zagvozdkina T.N. ICP-AES determination of basic and alloying elements in thermostable magnetic materials of REM–Fe–Co–B system. Trudy VIAM, 2014, no. 11, pр. 62–65. Available at: http://www.viam-works.ru (accessed: June 16, 2025). DOI: 10.18577/2307-6046-2014-0-11-10-10.
  12. Mazalov P.B., Suhov D.I., Sulyanova E.A., Mazalov I.S. Heat-resistant cobalt-based alloys. Aviation materials and technologies, 2021, no. 3 (64), pp. 3‒10. Available at: http://www.journal.viam.ru (accessed: June 16, 2025). DOI: 10.18577/2713-0193-2021-0-3-3-10.
  13. Sviridov A.V., Evgenov A.G., Afansiev-Khodykin A.N., Galushka I.A. Hardening of nickel superalloy parts by the composite brazing method using cobalt based stellite V5K. Aviation materials and technologies, 2024, no. 1 (74), pp. 3‒13. Available at: http://www.journal.viam.ru (accessed: June 17, 2025). DOI: 10.18577/2713-0193-2024-0-1-3-13.
  14. Mazalov I.S., Sukhov D.I., Nerush S.V., Sulyanova E.A. Features of the formation of the microstructure of alloys of the Co–Cr–Ni–W–Ta system and their mechanical properties. Kristallographiya, 2019, vol. 64, no. 4, pp. 544–549.
  15. Nerush S.V., Sviridov A.V., Afansiev-Khodykin A.N., Galushka I.A., Tarasov S.A. Development of brazing technology for parts obtained by additive technologies from cobalt based metal powder composition. Aviation materials and technologies, 2022, no. 2 (67), pp. 18–29. Available at: http://www.journal.viam.ru (accessed: June 18, 2025). DOI: 10.18577/2713-0193-2022-0-2-18-29.
  16. Petrushin N.V. Cobalt alloys. Great Russian Encyclopedia: scientific and educational portal. Available at: https://bigenc.ru/c/kobal-tovye-splavy-e5fc6e/?v=8286708 (accessed: June 17, 2025).
  17. Stepanovskikh V.V. Metrological traceability of the results of determining the chemical composition of metallurgical materials. Practical issues. Analitika, 2024, vol. 14, no. 2, pp. 184–186. DOI: 10.22184/2227-572X.2024.14.2.184.186.
  18. Filichkina V.A., Skorskaya O.L., Muravyova I.V. Methods and means of analytical control of materials. Chemical and physicochemical methods of analytical control: textbook. Moscow: Publishing house MISiS, 2015, 107 p.
  19. Karachevtsev F.N. Capabilities of modern methods of chemical-analytical analysis of alloys. Modern approaches and trends in the development of structural-phase, chemical-analytical methods of analysis: Reports of the XV All-Rus. Conf. on Testing and Research of Materials Properties «TestMat» (Moscow, February 10, 2023). Moscow: NRC «Kurchatov Institute» – VIAM, 2023, pp. 34–52.
  20. Karpov Yu.A., Baranovskaya V.B. The Role and Possibilities of Analytical Control in Metallurgy. II All-Rus. Conf. on Testing and Research of Materials Properties «TestMat–2013» (Moscow, February 28, 2013). Moscow: VIAM, 2013, р. 35.
  21. Pupyshev A.A., Danilova D.A. Atomic Emission Spectral Analysis with Inductively Coupled Plasma and Glow Discharge According to Grimm. Analitika i kontrol, 2003, vol. 7, no. 1, p. 101.
  22. Dvoretskov R.M., Uridia Z.P., Karachevtsev F.N., Zagvozdkina T.N. Determination of the chemical composition of magnesium alloys by the atomic emission spectrometry with inductively coupled plasma. Trudy VIAM, 2019, no. 12 (84), pp. 88‒98. Available at: http://www.viam-works.ru (accessed: June 16, 2025). DOI: 10.18577/2307-6046-2019-0-12-88-98.
  23. Dvoretskov R.M., Karachevtsev F.N., Demin S.A. Analytical control of the chemical composition of galvanic electrolytes of nickel plating by the ICP AES and ICP MS methods. Trudy VIAM, 2023, no. 3 (121). pp. 117‒131. Available at: http://www.viam-works.ru (accessed: June 16, 2025). DOI: 10.18577/2307-6046-2023-0-3-117-131.
  24. Shalygina L.V., Popkova G.N. Determination of tantalum in steels by inductively coupled plasma atomic emission spectrometry. Zavodskaya laboratoriya. Diagnostika materialov, 2023, vol. 89, no. 2-2, pp. 65–69. DOI: 10.26896/1028-6861-2023-89-2-II-65-69.
  25. Letov A.F. Application of instrumental methods of analysis to determine the chemical composition of new aviation materials. I All-Rus. Conf. on Testing and Research of Materials Properties «TestMat–2012» (Moscow, December 4–5, 2012). Moscow: VIAM, 2012, p. 10.
  26. Zolotov Yu.A. Methodological Aspects of Analytical Chemistry. Zhurnal analiticheskoy khimii, 2021, vol. 76, no. 1, pp. 5–19. DOI: 10.31857/S0044450221010175.
  27. Dvoretskov R.M. Multielement Spectral Analysis of Aviation Heat-Resistant Nickel Alloys: thesis, Cand. Sc. (Chem.). Moscow, 2019, 211 p.
  28. Lidin R.A., Molochko V.A., Andreeva L.L. Chemical Properties of Inorganic Substances. Moscow: Khimiya, 2000, 480 p.
  29. Karpov Yu.A., Savostin A.P. Methods of Sampling and Sample Preparation. Moscow: BINOM. Laboratoriya znaniy, 2003, 243 p.
  30. Bock R. Decomposition Methods in Analytical Chemistry. Moscow: Khimiya, 1984, 432 p.
  31. Volchenkova V.A., Blagoveshchensky Yu.V., Kazenas E.K. et al. Improving Analysis Schemes for Tungsten Carbide-Based Materials. Fizika i khimiya obrabotki materialov, 2024, no. 1, pp. 65–76. DOI: 10.30791/0015-3214-2024-1-65-76.
  32. Chernikova I.I., Ostroukhova U.A., Ermolaeva T.N. Microwave Sample Preparation in the Analysis of Ferrotungsten, Silicocalcium, and Ferroboron by Inductively Coupled Plasma Atomic Emission Spectrometry. Zavodskaya laboratoriya. Diagnostika materialov, 2018, vol. 84, no. 2, pp. 1–17. DOI: 10.26896/1028-6861-2018-84-2-11-17.
  33. Pupyshev A.A. Spectral interference and its correction in atomic emission spectral analysis. Zavodskaya laboratoriya. Diagnostika materialov, 2019, vol. 85, no. 1–2, pp. 15–32. DOI: 10.26896/1028-6861-2019-85-1-II-15-32.
  34. Stepanovskikh V.V., Kolpakova E.K., Khuzagaleeva R.K. Analytical control of raw materials and products in metallurgy based on the use of certified reference materials. Analytika, 2024, vol. 14, no. 6, pp. 488–491. DOI: 10.22184/2227-572X.2024.14.6.488.491.
  35. Stepanovskikh V.V., Kolpakova E.K., Khuzagaleeva R.K. Analytical control of ferrous metallurgy materials based on the use of certified reference materials developed by ISO JSC. Reference materials in measurements and technologies: report summary of the VI Int. scientific conf. (Ekaterinburg, September 3–6, 2024). Ekaterinburg: VNIIM im. D.I. Mendeleyev, 2024, pp. 157–158.