The influence of natural exposure on the properties and microstructure of carbon fiber plastic VKU-38TP
Nacharkina A.V., Zelenina I.V., Kurshev E.V., Evdokimov A.A. The influence of natural exposure on the properties and microstructure of carbon fiber plastic VKU-38TP // Proceedings of VIAM. 2026. No. 3. DOI: 10.18577/2307-6046-2026-0-3-124-140. URL: https://viam-works.ru/en/journal/2026/3/10
Keywords
polymer composite materials (PCM), high-temperature carbon plastics, phthalonitrile resin, natural aging, moisture absorption, water absorption, strength characteristics
Abstract
The article presents the study results on effect of natural aging in the climatic zones of Moscow and Gelendzhik on the structure and properties of carbon fiber based on phthalonitrile binder and 3D braided preform. Study results of carbon fiber surface degradation after natural aging under various conditions have been presented. Physical parameters such as density, amount of sorbed moisture, moisture and water absorption, stress-related properties of carbon fiber after natural aging compared to the initial values before exposure
Reference list
- Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
- Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 122–144. Available at: http://www.journal.viam.ru (accessed: January 31, 2025). DOI: 10.18577/2713-0193-2023-0-2-122-144.
- Gunyaeva A.G., Kurnosov A.O., Slavin A.V. Experience in the use of polymer composite materials developed by NRC «Kurchatov Institute» – VIAM in engines for civil aircraft. Aviation materials and technologies, 2024, no. 4 (77), pp. 82–94. Available at: http://www.journal.viam.ru (accessed: January 31, 2025). DOI: 10.18577/2713-0193-2024-0-4-82-94.
- Evdokimov A.A., Gulyaev I.N., Zelenina I.V. Investigation of the physicomechanical properties and microstructure of volume-reinforced carbon fiber reinforced plastic. Trudy VIAM, 2019, no. 4 (76), pp. 38–47. Available at: http://www.viam-works.ru (accessed: February 11, 2025). DOI: 10.18577/2307-6046-2019-0-4-38-47.
- Saleh M.N., Soutis C. Recent advancements in mechanical characterisation of 3D woven composites. Mechanics of Advanced Materials and Modern Processes, 2017, no. 3, pp. 1–17. DOI: 10.1186/s40759-017-0027-z.
- Gao M., Wu Q., Li T. et al. Rediscovering phthalonitrile resins: a novel liquid monomer towards high-performance resins. Polymer Chemistry, 2024, vol. 15, is. 21, pp. 2157–2166. DOI: 10.1039/d4py00100a.
- Domingues D.D., Jones H.N., Keller T.M. The effect of curing additive on the mechanical properties of phthalonitrile-carbon fiber composites. Polymer Composites, 2004, vol. 25, no. 5, pp. 554–561.
- Wang Z., Zhou X., Zheng K. et al. Achieving high heat resistance for phthalonitrile/boron blends through formation of protective phases derived from boron powder. Composites Communications, 2024, vol. 45, p. 101777. DOI: 10.1016/j.coco.2023.101777.
- Yang Z., Gu Y., Liu Y. et al. Thermal-oxidative aging mechanism of carbon fiber reinforced self-catalytic phthalonitrile resin matrix composite laminates at 450 °С ~500 °С. Composites Part A: Applied Science and Manufacturing, 2025, vol. 190, p. 108689. DOI: 10.1016/j.compositesa.2024.108689.
- Bogomolov P.I., Kozlov I.A., Birulya M.A. Review of modern technologies for the manufacture of volumetric-reinforcing preforms for advanced composite materials. Tekhniko-tekhnologicheskie problemy servisa, 2017, no. 1, pp. 22–27.
- Sergeev V.T. Development of the structure and manufacturing technology of multilayer combined fabric from carbon and quartz threads: thesis abstract, Cand. Sc. (Tech.). Moscow, 2014, 16 p.
- Belinis P.G., Donetskiy K.I., Lukyanenko Yu.V., Rogozhnikov V.N., Mayer Yu., Bystrikova D.V. Volume reinforcing solid-woven preforms for manufacturing of polymer composite materials (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 18–26. DOI: 10.18577/2071-9140-2019-0-4-18-26.
- Belinis P.G., Lukyanenko Yu.V., Rogozhnikov V.N., Tsykun R.G., Donetskiy K.I. Design research on a constructural multilayer woven preform of an integral panel fragment for aircraft. Aviation materials and technologies, 2023, no. 3 (72), pp. 114–124. Available at: http://www.journal.viam.ru (accessed: January 31, 2025). DOI: 10.18577/2713-0193-2023-0-3-114-124.
- Khusnullina A.R. Review of modern technologies for the manufacture of solid-woven volume-reinforced preforms used for the production of polymer composite materials. Proceedings of the XX All-Rus. with int. participation scientific and practical conference with elements of a scientific school for students and young scientists (Kazan, May 13–15, 2024). Kazan, 2024, pp. 322–325.
- Mekham M. Snecma and its partner AES create a new technology for the manufacture of composite blades. Available at: http://www.ato.ru/content/snecma-i-ee-partner-aec-sozdayut-novuyu-tehnologiyu-izgotovleniya-kompozitnyh-lopatok (accessed: May 16, 2025).
- Novikov A.S., Karimbaev T.D., Luppov A.A., Afanasyev D.V., Mezentsev M.A. Innovations in the Application of Composite Materials in Aircraft Engines. Dvigatel, 2015, no. 2 (98), pp. 6–9.
- Karimbaev T.D., Luppov A.A., Afanasyev D.V. Carbon Fiber Fan Blades for Advanced Engines. Achievements and Challenges. Dvigatel, 2011, no. 6, pp. 4–9.
- Kondrashov E.K., Kuznetsova V.A., Lebedeva T.A., Semenova L.V. Main Directions for Improving the Performance, Technological, and Environmental Characteristics of Paint and Varnish Coatings for Aircraft Equipment. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 96–102.
- Shunmugapriya K., Kale Shirish S., Gouda G., Jayapal Р. Paints for aerospace applications. Aerospace Materials and Material Technologies, 2017, vol. 1, pp. 539–562.
- Zhang Ti., Zhang Te., He Y. et al. Corrosion and aging of organic aviation coatings: A review. Chinese Journal of Aeronautics, 2023, vol. 36, no. 4, pp. 1–35.
- Startsev O.V., Koval T.V., Dvirnaya E.V., Kornienko G.V., Veligodsky I.M. Research of the properties of carbon fiber reinforced plastic with coatings after 8 and 13 years of aging in a moderately warm climate. Part 3. Condition of the polymer matrix of а composite. Trudy VIAM, 2025, no. 4 (146). pp. 96‒106. Available at: http://www.viam-works.ru (accessed: February 15, 2025). DOI: 10.18577/2307-6046-2025-0-4-96-106.
- Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
- Abramova M.G., Lutsenko A.N., Varchenko E.A. Concerning the aspects of validation of climate resistance of airborne materials at all life cycle stages (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 86–94. DOI: 10.18577/2071-9140-2020-0-1-86-94.
- Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), pp. 70–80. Available at: http://www.journal.viam.ru (accessed: May 14, 2024). DOI: 10.18577/2713-0193-2021-0-4-70-80.
- Laptev A.B., Pavlov M.R., Novikov A.A., Slavin A.V. Current trends in the development of testing materials for resistance to climate factors (review). Part 1. Testing of new materials. Trudy VIAM, 2021, no. 1 (95), pp. 114–122. Available at: http://www.viam-works.ru (accessed: April 20, 2025). DOI: 10.18577/2307-6046-2021-0-1-114-122.
- Mukhametov R.R., Shimkin A.A., Gulyaev A.I., Kucherovsky A.I. Phthalonitrile binder for heat-resistant composites. Materialovedenie, 2015, no. 11, pp. 48–53.
- Liu L., Du M., Liu F. Recent advances in interface microscopic characterization of carbon fiber-reinforced polymer composites. Frontiers in Materials, 2023, vol. 10, pp. 1–18.
- Tandon G.P., Ragland W.R., Shoeppner G.A. Using Optical Microscopy to Monitor Anisotropic Oxidation Growth in High-Temperature Polymer Matrix Composites. Journal of composite materials, 2009, vol. 43, no. 5, pp. 583–603.
- Deev I.S., Kurshev E.V., Lonskiy S.L. The influence of long-term climatic aging on the surface microstructure of epoxy carbon fiber reinforced plastics. Voprosy materialovedeniya, 2018, no. 3, pp. 157–169.
- Guo H., Chen Z., Yang X. et al. Self-promoted curing phthalonitrile with high glass transition temperature for advanced composites. Journal of Polymer Research, 2012, vol. 19, no. 7, pp. 1–8.
- Han B., Li Y., Wan J. et al. Progress in high temperature resistant phthalonitrile resins and their composites for aerospace applications. Reactive and Functional Polymers, 2025, vol. 214, p. 106293. DOI: 10.1016/j.reactfunctpolym.2025.106293.
- Feng J., Wang D., Hu J. et al. Optimizing the thermal properties of fiber reinforced phthalonitrile composites. Journal of Applied Polymer Science, 2023, vol. 141, is. 2. DOI: 10.1002/app.54772.
- Valevin E.O., Zelenina I.V., Marakhovsky P.S., Gulyaev A.I., Bukharov S.V. Study of heat and humidity effects on a phthalonitrile matrix. Materialovedenie, 2015, no. 9 (222), pp. 15–19.
- Valevin E.O. Effect of heat and humidity effects on the properties of heat-resistant polymer composite materials based on a phthalonitrile matrix: thesis, Cand. Sc. (Tech.). Moscow, 2018, 130 p.
- Kurshev E.V., Lonskiy S.L., Egorov Yu.A., Zelenina I.V. Study of changes in the microstructure and chemical composition of polyimide carbon fiber reinforced plastic after exposure to simulated operational factors. Voprosy materialovedeniya, 2024, no. 4, pp. 88–102.
- Startsev V.O., Valevin E.O., Gulyaev A.I. The influence of polymer composite materials’ surface weathering on its mechanical properties. Trudy VIAM, 2020, no. 8 (90), pp. 64–76. Available at: http://www.viam-works.ru (accessed: February 11, 2025). DOI: 10.18577/2307- 6046-2020-0-8-64-76.
- Gulyev I.N., Zelenina I.V., Valevin E.O., Khaskov M.A. Influence of climatic ageing on the properties of high-temperature carbon fiber reinforced plastics. Trudy VIAM, 2021, no. 2 (96), pp. 39–51. Available at: http://www.viam-works.ru (accessed: February 12, 2025). DOI: 10.18577/2307-6046-2021-0-2-39-51.
- Salnikov V.G., Startsev O.V., Lebedev M.P. et al. Effect of Daily and Seasonal Changes in Relative Humidity and Temperature on Moisture Saturation of Carbon Fiber Reinforced Plastics in Open Climate Conditions. Vse materialy. Entsiklopedicheskiy spravochnik, 2022, no. 5, pp. 2–10. DOI: 10.31044/1994-6260-2022-0-5-2-10.
- Panin S.V. Study of Changes in Surface Relief and Moisture Transfer in Polymer Composite Materials during Climatic Aging: thesis, Cand. Sc. (Tech.). Moscow, 2015, 131 p.
- Valevin E.O., Startsev V.O., Zelenina I.V. Thermal aging, surface degradation and water transfer in carbon fiber reinforced plastic VKU-38TR. Trudy VIAM, 2020, no. 6–7 (89), pp. 118–128. Available at: http://www.viam-works.ru (accessed: April 06, 2025). DOI: 10.18577/2307-6046-2020-0-67-118-128.