Inverse opals based on ZnO(Al)
Martynova N.A., Taibarei N.O., Kuznetsova N.N., Savilov S. V. Inverse opals based on ZnO(Al) // Proceedings of VIAM. 2026. No. 2. DOI: 10.18577/2307-6046-2026-0-2-154-166. URL: https://viam-works.ru/en/journal/2026/2/14
Keywords
inverse opals, transparent semiconductor coatings, zinc oxide, electrochemically induced deposition, cyclic voltammetry, photoluminescent spectroscopy, optical spectroscopy
Abstract
A method for electrochemical formation of inverse opals based on ZnO and ZnO(Al) using colloidal crystals as a template has been developed. The dependence of the phase composition and microstructure of inverse opals on the conditions of a two-stage synthesis, involving electrochemically induced deposition and subsequent annealing, were studied. Annealing resulted in the formation of single-phase aluminum-doped zinc oxide with a given inverse opal structure. The photoluminescence and photonic properties of inverse opals based on ZnO(Al) were studied.
Reference list
- Sudzhanskaya I.V., Lebedeva Yu.E., Vaganova M.L., Shchegoleva N.E. Effect of co-doped of CeO2, Y2O3 on microstructure and mechanical properties of ceramic spinel MgAl2O4. Aviation materials and technologies, 2025, no. 2 (79), pp. 91–102. Available at: http://www.journal.viam.ru (accessed: November 06, 2025). DOI: 10.18577/2713-0193-2025-0-2-91-102.
- Sokolov A.V., Deynega G.I., Kuzmina N.A., Kuzmina I.G. Structural and mechanical properties of a composite material based on partially stabilized zirconium dioxide doped with magnesium aluminate spinel. Aviation materials and technologies, 2021, no. 3 (64), pp. 78–85. Available at: http://www.journal.viam.ru (accessed: November 06, 2025). DOI: 10.18577/2713-0193-2021-0-3-78-85.
- Babashov V.G., Stepanova E.V., Zimichev A.M., Basargin O.V. Oxide continuous fibers as a part of flexible high temperature insulation. Aviation materials and technology, 2021, no. 1 (62), pp. 34–43. Available at: http://www.journal.viam.ru (accessed: November 06, 2025). DOI: 10.18577/2713-0193-2021-0-1-34-43.
- Doronin O.N., Artemenko N.I., Stekhov P.A., Voronov V.A. Deposition of ceramic layers of heat protection coatings based on the system Gd2O3–ZrO2–HfO2 and Sm2O3–Y2O3–HfO2. Aviation materials and technologies, 2022, no. 3 (68), pp. 108–119. Available at: http://www.journal.viam.ru (accessed: November 06, 2025). DOI: 10.18577/2713-0193-2022-0-3-108-119.
- Sakharov K.A., Simonenko E.P., Simonenko N.P. et al. Glycol-citrate synthesis of fine-grained oxides La2–xGdxZrO2O7 and preparation of corresponding ceramics using FAST/SPS process. Ceramics International, 2018, vol. 44, no. 7, pp. 7647–7655.
- Wang H., Li K., Tao Y. et al. Smooth ZnO:Al – AgNWs composite electrode for flexible organic light-emitting device. Nanoscale Research Letters, 2017, vol. 12 (77), pp. 1–7. DOI: 10.1186/s11671-017-1841-2.
- Lee S.-H., Han S.-H., Jung H.S. et al. Al-doped ZnO Thin Film: A New Transparent conducting layer for ZnO nanowire-based dye-sensitized solar cells. Journal of Physical Chemistry C, 2010, vol. 114 (15), pp. 7185–7189. DOI: 10.1021/jp1008412.
- Treharne R.E., Hutchings K., Lamb D.A. et al. Combinatorial optimization of Al-doped ZnO films for thin-film photovoltaics. Journal of Physics D: Applied Physics, 2012, vol. 45, p. 335102. DOI: 10.1088/0022-3727/45/33/335102.
- Pathirane M.K., Khaligh H.H., Goldthorpe I.A., Wong W.S. Al-doped ZnO/Ag-nanowire composite electrodes for flexible 3-dimensional nanowire solar cells. Scientific Reports, 2017, vol. 8916, pp. 1–7. DOI: 10.1038/s41598-017-07180-1.
- Lim X., Ye W., Zhou X. et al. Increased efficiency for perovskite photovoltaics based on aluminum-doped zinc oxide transparent electrodes via surface modification. Journal of Physical Chemistry C, 2017, vol. 121, pp. 10282–10288. DOI: 10.1021/acs.jpcc.7b00419.
- Pradhan A.K., Mundle R.M., Santiago K. et al. Extreme tunability in aluminum doped zinc oxide plasmonic materials for near-infrared applications. Scientific Reports, 2014, vol. 4 (1), p. 6415. DOI: 10.1038/srep06415.
- Baruah A., Jindalm A., Acharya C. Microfluidic reactors for the morphology controlled synthesis and photocatalytic study of ZnO nanostructures. Journal of Micromechanics and Microengineering, 2017, vol. 27, p. 035013.
- Bui Q.C., Consonni V., Boubenia S. et al. High figure-of-merit in Al-doped ZnO thin films grown by ALD through the Al content adjustment. Materialia, 2023, vol. 31, p. 101863. DOI: 10.1016/j.mtla.2023.101863.
- Azzouz I., Habba Y.G., Capochichi-Gnambodoe M. et al. Zinc oxide nano-enabled microreactor for water purification and its applicability to volatile organic compounds. Microsystems & Nanoengineering, 2018, vol. 4, p. 17093. DOI: 10.1038/micronano.2017.93.
- Gerstl M., Hutterer A., Fleig J. et al. Model composite microelectrodes as a pathfinder for fully oxidic SOFC anodes. Solid State Ionics, 2016, vol. 298, pp. 1–8. DOI: 10.1016/j.ssi.2016.10.013.
- Pullini D., Pruna A., Zanin S., Mataix D.B. High-efficiency electrodeposition of large scale ZnO nanorod arrays for thin transparent electrodes. Journal of the Electrochemical Society, 2012, vol. 159 (2), pp. 45–51. DOI: 10.1149/2.093202jes.
- Martynova N.A., Svishchev V.N., Lepnev L.S. et al. Electrochemical coprecipitation of zinc and aluminum in aqueous electrolytes for ZnO and AZO coverage deposition. International Journal of Photoenergy, 2019, vol. 2019, art. 6808347. DOI: 10.1155/2019/6808347.
- Wang M., Wang X. Electrodeposition zinc-oxide inverse opal and its application in hybrid photovoltaics. Solar Energy Materials and Solar Cells, 2008, vol. 92 (3), pp. 357–362.
- Abramova V., Sinitskii A. Large-scale ZnO inverse opal films fabricated by a sol–gel technique. Superlattices and Microstructures, 2009, vol. 45 (6), pp. 624–629. DOI: 10.1016/j.spmi.2009.03.003.
- Krężel A., Maret W. The biological inorganic chemistry of zinc ions. Archives of Biochemistry and Biophysics, 2016, vol. 611, pp. 3–19. DOI: 10.1016/j.abb.2016.04.010.
- Kang D., Lee D., Choi K.-S. Electrochemical synthesis of highly oriented, transparent, and pinhole-free ZnO and Al-doped ZnO films and their use in heterojunction solar cells. Langmuir, 2016, vol. 32, pp. 10459–10466.
- Martynova N.A., Lepnev L.S., Tsymbarenko D.M. et al. Galvanic synthesis of ZnO and ZnA(Al) coatings from dimethylsulfoxide electrolytic baths. Journal of Advanced Materials and Technologies, 2023, vol. 8 (1), pp. 8–19. DOI: 10.17277/jamt.2023.01.pp.008-019.
- Martynova N.A. Nanomaterials with inverted opal structure: electrochemical synthesis and optical properties: thesis, Cand. Sc. (Chem.). Moscow, 2022, 175 p.
- Taibarei N.O., Kytin V.G., Konstantinova E.A. et al. Doping nature of group V elements in ZnO single crystals grown from melts at high pressure. Crystal Growth & Design, 2022, vol. 22 (4), pp. 2452–2461. DOI: 10.1021/acs.cgd.1c01507.
- Thandavan T.M., Gani S.M., Wong C.S., Nor R.M. Enhanced photoluminescence and Raman properties of Al-Doped ZnO nanostructures prepared using thermal chemical vapor deposition of methanol assisted with heated brass. PLOS One, 2015, vol. 10 (5), pp. 1–18.
- Yoshinaga S., Ishikawa Y., Araki S. et al. Numerical analysis of monocrystalline silicon solar cells with fine nanoimprinted textured surface. Japanese Journal of Applied Physics, 2017, vol. 56, p. 022301.