Features of preparation and conducting tests to determine the transverse tensile strength of samples of laminated carbon fiber reinforced plastics

Vasilchuk E.A., Gubin A.M., Gulyaev I.N., Klimenko O.N.
Vasilchuk E.A., Gubin A.M., Gulyaev I.N., Klimenko O.N. Features of preparation and conducting tests to determine the transverse tensile strength of samples of laminated carbon fiber reinforced plastics // Proceedings of VIAM. 2026. No. 1. DOI: 10.18577/2307-6046-2026-0-1-197-208. URL: https://viam-works.ru/en/journal/2026/1/15
Keywords
polymer composite material, carbon fiber reinforced plastic, transverse strength, mechanical testing
Abstract

The article presents the features of manufacturing, preparation for testing and testing of samples of layered carbon fiber reinforced plastics for transverse tensile strength. The features of laying out thick-walled plates and typical damage to the structure of the material during the manufacture of samples, as well as their influence of structural defects on the values obtained during testing are described. Differences in samples and their destruction are shown. At present, the Institute continues to improve the methods of testing layered carbon fiber reinforced plastics for the most complete description of the properties of PCM.

Reference list
  1. Erasov V.S., Oreshko E.I. Mechanical Testing and Properties of Structural Metallic Aviation Materials: Textbook. Ed. E.N. Kablov. Moscow: NRC «Kurchatov Institute» – VIAM, 2023, 344 p.
  2. Goldenblat I.I., Kopnov V.A. Strength Criterion of Anisotropic Materials. Mekhanika, 1965, no. 6, pp. 77–83.
  3. Levin V.E., Laperdina N.A., Olegin I.P. Numerical Approach to Determining the Elastic Properties of Unidirectionally Reinforced Composites. Nauchno-tekhnicheskiy vestnik Povolzhya, 2019, no. 11, pp. 141–145.
  4. Gunyaeva A.G., Kurnosov A.O., Slavin A.V. Experience in the use of polymer composite materials developed by NRC «Kurchatov Institute» – VIAM in engines for civil aircraft. Aviation materials and technologies, 2024, no. 4 (77), pp. 82–94. Available at: http://www.journal.viam.ru (accessed: March 02, 2025). DOI: 10.18577/2713-0193-2024-0-4-82-94.
  5. Shershak P.V., Yakovlev N.O., Sutubalov A.I. Standards for testing polymer composite materials. Part 1. Tensile properties. Aviation materials and technologies, 2023, no. 3 (72), pp. 152–166. Available at: http://www.journal.viam.ru (accessed: April 05, 2025). DOI: 10.18577/2713-0193-2023-0-3-152-166.
  6. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 122–144. Available at: http://www.journal.viam.ru (accessed: April 09, 2025). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  7. Sutubalov A.I., Podzhivotov N.Yu., Shershak P.V., Yakovlev N.O. Evaluation of homogeneity of physical and mechanical properties of semi-finished products for aviation purpose. Aviation materials and technologies, 2024, no. 1 (74), рр. 121–135. Available at: http://www.journal.viam.ru (accessed: April 25, 2025). DOI: 10.18577/2713-0193-2024-0-1-121-135.
  8. Hancox N.L. The compression strength of unidirectional carbon fibre reinforced plastic. Journal of materials science, 1975, vol. 10, pp. 234–242. DOI: 10.1007/BF00540347.
  9. Berkov N.A., Arkhangelsky A.I., Arkhangelskaya M.V. Nonlinear analysis of composite shell connections. New technologies of higher education. Science, technology, pedagogy. Moscow: Moscow Polytechnic, 2021, pp. 113–119.
  10. Pyataev S.F. Effect of temperature on the strength of linearly reinforced boron-plastics under complex loading. Zhurnal Sibirskogo federal'nogo universiteta. Ser.: Matematika i fizika, 2012, vol. 5 (2), pp. 246–255.
  11. Lee S., Waas A.M. Compressive response and failure of fiber reinforced unidirectional composites. International Journal of Fracture, 1999, vol. 100, pp. 275–306. DOI: 10.1023/A:1018779307931.
  12. State Standard 25.603–82. Methods of mechanical testing of composite materials with a polymer matrix (composites). Moscow: Publ. House of Standards, 1983, 15 p.
  13. Fedonyuk N.N., Maslich E.A. Application of polymer composite materials in foreign shipbuilding. St. Petersburg: Krylov State Research Center, 2024, 304 p.
  14. Suknev S.V. Non-local failure criteria. Point stress criteria. Nauka i obrazovanie, 2008, no. 1 (49), p. 27–32.
  15. Minibaev M.I., Raskutin A.E., Goncharov V.A. Peculiarities of technology production specimens of PCM on CNC machines (review). Trudy VIAM, 2019, no. 1 (73), pp. 105–114. Available at: http://www.viam-works.ru (accessed: April 30, 2025). DOI: 10.18577/2307-6046-2019-0-1-105-114.
  16. Khrulkov I.A., Gulyaev I.N., Mishkin S.I. Features of cutting polymer composite materials with diamond wheels (review). Trudy VIAM, 2022, no. 4 (110), pp. 22–31. Available at: http://www.viam-works.ru (accessed: May 18, 2025). DOI: 10.18577/2307-6046-2022-0-4-22-31.
  17. Minibaev M.I., Usacheva M.N., Dyshenko V.S., Goncharov V.A. A device and tool for making sample from polymer composite materials on a CNC machine (review). Trudy VIAM, 2021, no. 4 (98), pp. 100–109. Available at: http://www.viam-works.ru (accessed: April 22, 2025). DOI: 10.18577/2307-6046-2021-0-4-100-109.
  18. Kanatov A.V., Zaitsev D.A., Zaporozhan D.Yu. Features of cutting special composite materials with a mechanical point tool. Improving energy and resource efficiency and environmental safety of processes and equipment in the chemical and related industries: in 2 vols. Moscow: Publ. House of the Kosygin Rus. State Univ., 2021, vol. 1, pp. 289–292.
  19. Zhelezina G.F., Kulagina G.S., Sidorina A.I., Soloveva N.A. Fatigue of constructional organoplastics. Aviacionnye materialy i tehnologii, 2014, no. 1, pp. 89–100. Available at: http://www.journal.viam.ru (accessed: May 15, 2025). DOI: 10.18577/2713-0193-2024-0-1-89-100.
  20. State Standard 57864–2017. Method for determining the ultimate strength and elastic modulus under tension in the direction of specimen thickness. Moscow: Standartinform, 2017, 17 p.