Investigation of the resistance of thermoplastic polyurethane during thermooxidative and thermochemical treatment with diethylene glycole by gel permeation chromatography and microstructural analysis
UDC
678.012:543.544.15:620.187.3
DOI
10.18577/2307-6046-2026-0-1-67-84
Article PDF (Russian)
(1.11 MB)
How to cite
Ponomarenko S.A., Lonskii S.L. Investigation of the resistance of thermoplastic polyurethane during thermooxidative and thermochemical treatment with diethylene glycole by gel permeation chromatography and microstructural analysis // Proceedings of VIAM. 2026. No. 1. DOI: 10.18577/2307-6046-2026-0-1-67-84. URL: https://viam-works.ru/en/journal/2026/1/6
Keywords
thermoplastic polyurethane, molecular mass distribution, number-average molecular mass, microstructural studies, microphase structure, long-time processing, thermooxi- dative treatment, thermochemical tr
Abstract
The stability of thermoplastic polyurethane samples during high temperature processing has been evaluated. Material degradation during thermooxidative processing in air at 200 °C is well explained by the possible presence of residual amounts of 1,4-butanediol and its participation in the processes taking place. For quantitative data processing, a model was proposed that is suitable to describe the kinetics of polymer degradation during its thermochemical processing at 150 °C (R2 = 0,9982); to assess its suitability at a higher processing temperature of 180 °C, more data is required.
Reference list
- Mazurin V.L. Polyurethane as a structural material of the 21st century. Nauchno-tekhnicheskie vedomosti Sankt-Peterburgskogo gosudarstvennogo politekhnicheskogo universiteta, 2013, no. 2 (171), pp. 165–170.
- Kuznetsov D.A. Segmented polyurethane-imide copolymers containing aromatic and aliphatic blocks: thesis, Cand. Sc. (Chem.). St. Petersburg, 2022, 124 p.
- Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
- Dedov A.V., Kolotilin D.V., Rybakov Yu.N. Permeability of thermoplastic polyurethanes for aviation kerosene storage tanks. Plasticheskie massy, 2021, no. 9–10, pp. 45–47.
- Zhdanov A.V. Analysis of modern technologies for the manufacture of pulsed-type individual housing construction. Biotechnosfera, 2011, no. 4 (16), pp. 35–37.
- Chaykun A.M., Sergeyev A.V., Pravada E.S. Elastomeric-fabric materials for products of special equipment (review). Trudy VIAM, 2023, no. 6 (124), pp. 25–37. Available at: http://www.viam-works.ru (accessed: April 21, 2025). DOI: 10.18577/2307-6046-2023-0-6-25-37.
- Kablov E.N. The Role of Fundamental Research in the Creation of Next-Generation Materials. Reports of the XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
- Kablov E.N. The Role of Chemistry in the Creation of Next-Generation Materials for Complex Technical Systems. Reports of the XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg, 2016, pp. 25–26.
- Gorbunova M.A., Anokhin D.V., Badamshina E.R. Modern Advances in the Production and Use of Thermoplastic Semicrystalline Polyurethanes with Shape Memory Effect. Vysokomolekulyarnye soedineniya. Ser.: B, 2020, vol. 62, no. 5, pp. 323–347.
- Lipatov Yu.S., Kercha Yu.Yu., Sergeeva L.M. Structure and Properties of Polyurethanes. Kyiv: Naukova Dumka, 1970, 279 p.
- Shilnikova N.V. Development of Technologies for Obtaining Composite Materials Based on Polyurethanes and Natural Cork: thesis, Cand. Sc. (Tech.). Kazan, 2002, 142 p.
- Nesterov S.V., Bakirova I.N., Samuilov Ya.D. Thermal and Thermo-oxidative Degradation of Polyurethanes: Mechanisms, Influencing Factors, and Basic Methods for Improving Thermal Stability. Review Based on Domestic and Foreign Publications. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2011, no. 14, pp. 10–23.
- Gallyamov A.A. Structure, properties, and application of polyurethane degradation products by di- and polyamines: thesis, Cand. Sc. (Tech.). Ekaterinburg, 2016, 163 p.
- Ponomarenko S.A., Shimkin A.A. Chromatographic methods of analysis: application possibilities in the aviation industry (review). Zavodskaya laboratoriya. Diagnostika materialov, 2017, no. 83 (4), pp. 5–13.
- Trathnigg B. Size-exclusion chromatography of polymers. Encyclopedia of Analytical Chemistry. Ed. R.A. Meyers. Chicheste: Wiley, 2000, pp. 8008–8034.
- Shimkin A.A., Ponomarenko S.A., Mukhametov R.R. Study of the curing process of diphthalonitrile binder. Zhurnal prikladnoy khimii, 2016, vol. 89, no. 2, pp. 256–264.
- Lem K.W., Haw J.R., Curran S. et al. Effect of Hard Segment Molecular Weight on Dilute Solution Properties of Ether Based Thermoplastic Polyurethanes. Nanoscience and Nanoengineering, 2013, no. 1 (3), pp. 123–133.
- Nguyen T.Q., Kausch H.H. GPC Data Interpretation in Mechanochemical Polymer Degradation. International Journal of polymer analysis and characterization, 1997, vol. 4 (5), pp. 447–470. DOI: 10.1080/10236669808009728.
- Novikov V.U., Kozitsky D.V., Deev I.S., Ivanova V.S., Kobets L.P. Multifractal analysis of the structure of polymethyl methacrylate studied by scanning electron microscopy. Plasticheskie massy, 2001, no. 1, pp. 7–9.
- Makushchenko I.S., Kozlov I.А., Smirnov D.N., Kurshev E.V., Lonskii S.L. Influence of corrosion inhibitors on the microstructure and vulcanization kinetics of polisulfide sealant. Trudy VIAM, 2024, no. 4 (134), pp. 123–132. Available at: http://www.viam-works.ru (accessed: April 21, 2025). DOI: 10.18577/2307-6046-2024-0-4-123-132.
- De Bruijn J.C.M., Meijer H.D.F. The design and application of a microfoil tensile test apparatus for monitoring the degree of ultraviolet degradation of polymers. Review of Scientific Instruments, 1991, no. 62, pp. 1620–1623.
- Kurshev E.V., Lonskii S.L., Mekalina I.V. Influence of long climatic aging on microstructure of surface of organic glass in semi-arid and subtropical climate. Trudy VIAM, 2022, no. 3 (109), pp. 15–26. Available at: http://www.viam-works.ru (accessed: April 21, 2025). DOI: 10.18577/2307-6046-2022-0-3-15-26.
- Deev I.S., Kuklin E.A. Features of the Formation of the Microphase Structure of Polymethyl Methacrylate Organic Glasses and Its Changes under Aging Conditions. Materialovedenie, 2014, no. 4, pp. 43–50.
- Deev I.S., Kobets L.P. Structure Formation in Filled Thermosetting Polymers. Kolloidnyy zhurnal, 1999, vol. 61, no. 5, pp. 650–660.
- Serdtselyubova A.S., Zverevich Yu.K., Kurshev E.V., Lonskiy S.L. Study of the Influence of Thermal Humidity Tests on the Microstructure of Fluoropolyurethane Coatings. Lakokrasochnye materialy i ikh primenenie, 2024, no. 7–8 (566), pp. 32–38.
- Thermoplastic polyurethane. Available at: https://www.vitur33.ru/publications/articles/articles_9.html (accessed: April 21, 2025).
- Yuan Y., Lin W., Xu L., Wang W. Recent Progress in Thermoplastic Polyurethane/MXene Nanocomposites: Preparation, Flame-Retardant Properties and Applications (review). Molecules, 2024, no. 29 (16). DOI: 10.3390/molecules29163880.
- Kablov E.N., Semenova L.V., Petrova G.N., Larionov S.A., Perfilova D.N. Polymer composite materials on a thermoplastic matrix. Izvestiya vysshikh uchebnykh zavedeniy. Ser.: Khimiya i khimicheskaya tekhnologiya, 2016, vol. 59, no. 10, pp. 61–71.
- Kablov E.N., Kondrashov S.V., Melnikov A.A., Schur P.A. Application of functional and adaptive materials obtained by 3D printing (review). Trudy VIAM, 2022, no. 2 (108), pp. 32–51. Available at: http://www.viam-works.ru (accessed: April 21, 2025). DOI: 10.18577/2307-6046-2022-0-2-32-51.
- A guide to thermoplastic polyurethanes (TPU). Available at: https://www.huntsman-pimcore.equisolve-dev.com/Documents/PU_Elastomers_Guide_to_TPU.pdf (accessed: April 21, 2025).
- Ponomarenko S.A., Kurshev E.V., Lonskii S.L. Investigation of degradation mechanisms of thermoplastic polyurethane by storage at long times in aviation kerosene TS-1 by gel permeation chromatography, optic and scanning electron microscopy, and FTIR spectroscopy. Trudy VIAM, 2025, no. 2 (144), pp. 47–64. Available at: http://www.viam-works.ru (accessed: April 21, 2025). DOI: 10.18577/2307-6046-2025-0-2-47-64.
- Lu L., Zhu Z., Wu Y. Depolymerization kinetics for thermoplastic polyurethane elastomer degradation in subcritical methanol. Polymer Degradation and Stability, 2017, vol. 140, pp. 126–135.
- Bardin A., Le Gac P.-Y., Gerontola S., Simon G. Hydrolytic kinetic model predicting embrittlement in thermoplastic elastomers. Polymer Degradation and Stability, 2020, vol. 171, аrt. 109902.
- State Standard R 57268.3–2016 (ISO 16014-3:2012). Polymer composites. Determination of average molecular weight and molecular weight distribution of polymers by size-exclusion chromatography. Part 3. Low-temperature method. Moscow: Standartinform, 2016, 18 p.