Comparative analysis of mechanical properties of the material of VT6 alloy disk forgings, manufactured by various methods and production conditions
Kashapov O.S., Pavlova T.V., Zaysev D.V., Chuchman O.V. Comparative analysis of mechanical properties of the material of VT6 alloy disk forgings, manufactured by various methods and production conditions // Proceedings of VIAM. 2026. No. 1. DOI: 10.18577/2307-6046-2026-0-1-51-66. URL: https://viam-works.ru/en/journal/2026/1/5
Keywords
Ti6-4, titanium alloys, VT6, VT6ch, microstructure, mechanical properties, thermomechanical treatment, heat treatment, compressor disks
Abstract
The article presents the mechanical properties of VT6 alloy disk forgings manufactured under various production conditions with different heat treatment modes. The research results presented in the main part of the article were obtained in the initial period of work on the introduction of VT6 alloy for engine parts and were confirmed later during the certification of disk forging weighing up to 100 kg. A comparison of the mechanical properties of stampings of the same type made of VT6 and VT3-1 alloys is given. The discussion pays special attention to the factors leading to a decrease in the viscosity characteristics of the material.
Reference list
- Pavlova T.V., Kashapov O.S., Chuchman O.V., Goncharova L.Yu. Comparative analysis of mechanical properties of the material of VT6 alloy forgings, manufactured by various methods and production conditions. Trudy VIAM, 2025, no. 5 (147), pp. 22–37. Available at: http://www.viam-works.ru (accessed: May 13, 2025). DOI: 10.18577/2307-6046-2025-0-5-25-37.
- Du S., Song Y., He Y. et al. Evolution of Microstructure and Mechanical Properties of Ti‒6Al‒4V Alloy under Heat Treatment and Multi-Axial Forging. Materials, 2024, vol. 17, pp. 1060–1079. DOI: 10.3390/ma17051060.
- Yan-Wei S., Ai-Hui L., Bang-Sheng L., Jing-Jie G. Relationship between Thickness of Lamellar α+β Phase and Mechanical Properties of Titanium Alloy. Advanced Materials Research, 2011, vol. 311–313, pp. 1916–1919. DOI: 10.4028/www.scientific.net/AMR.311-313.1916.
- Julien R., Velay V., Vidal V. et al. Characterization and modeling of forged Ti‒6Al‒4V Titanium alloy with microstructural considerations during quenching process. International Journal of Mechanical Sciences, 2018, vol. 142–143, pp. 456–467. DOI: 10.1016/j.ijmecsci.2018.05.023.
- Neminathan P.V., Yadav J.S., Reddy K.R. et al. Development of disc forgings in Ti‒6Al‒4V alloy for aero-engine application. Transactions of the Indian Institute of Metals, 2008, vol. 61, no. 5, pp. 363–370.
- Egorova Yu.B., Davydenko L.V. Influence of chemical composition and parameters of globular structure on the mechanical properties of rods made of titanium alloy VT6. Electrometallurgiya, 2025, no. 2, pp. 20–29. DOI: 10.31044/1684-5781-2025-0-2-20-29.
- Moiseyev V.N. Titanium Alloys: Russian Aircraft and Aerospace Applications. 1st ed. CRC Press, 2005, 216 p. DOI: 10.1201/9781420037678.
- Ji H., Zhanshuo P., Xiaomin H. et al. Dynamic recrystallization of Ti‒6Al‒4V titanium alloy based on cellular automata. Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering, 2023, vol. 237. DOI: 10.1177/09544089221125575.
- Seo S., Jung M., Park J. Microstructure control for enhancing the combination of strength and elongation in Ti‒6Al‒4V through heat treatment. Metals, 2024, vol. 14, p. 985. DOI: 10.3390/met14090985.
- Senkov O.N., Senkova S.V., Valencia J. et al. Effect of cooling rate on microstructure of Ti‒6Al‒4V forging. Materials Science and Technology, 2002, vol. 18, pp. 1470–1478. DOI: 10.1179/026708302225007808.
- Elmer J.W., Palmer T.A., Babu S.S. et al. In situ observations of lattice expansion and transformation rates of α and β phases in Ti–6Al–4V. Materials Science and Engineering A, 2005, vol. 391, pp. 104–113.
- Denisov Yu.P. Study of chemical microheterogeneity in two-phase titanium alloys using VT3-1 as an example: thesis abstract, Cand. Sc. (Tech.). Moscow, 1981, 25 p.
- Solonina O.P., Glazunov S.G. Modern heat-resistant titanium alloys and prospects for their application in engines. Moscow: Metallurgy, 1974, 448 p.
- Gorbovets M.A., Slavin A.V. Proof of material compliance with the requirements to part No. 33 of JARs. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 89–94. DOI: 10.18577/2071-9140-2018-0-3-89-94.
- Preliminary National Standard 658–2022. Aviation Materials. General and Special Qualification Procedure. Available at: https://gostassistent.ru/doc/0fbe057e-14bd-4e3f-b3bd-6b67c5efb163 (accessed: May 17, 2025).
- Berenson V.F., Shevchenko Yu.N., Kompaniets A.S. Passportization and certification of aviation materials – a guarantee of their quality. Aviation materials. Selected works of VIAM 1932–2002. Moscow: VIAM, 2002, pp. 409–412.
- Gorbovets M.A., Khodinev I.A., Karanov V.A., Yushin V.D. Influence of the type of loading on high-cycle fatigue of heat-resistant alloys. Trudy VIAM, 2019, no. 3 (75), pp. 96–104. Available at: http://www.viam-works.ru (accessed: May 12, 2025). DOI: 10.18577/2307-6046-2019-0-3-96-104.
- Callegari B., Marçola J.V., Aristizabal K. et al. Effect of microstructure on Ti3Al precipitation during ageing of Ti‒6Al‒4V alloy. MATEC Web of Conferences, 2020, vol. 321, pp. 1–7. DOI: 10.1051/matecconf/202032103013.
- Radecka A., Bagot P.A.J., Martin T.L. et al. The formation of ordered clusters in Ti‒7Al and Ti‒6Al‒4V. Acta Materialia, 2016, vol. 112, pp. 141–149. DOI: 10.1016/j.actamat.2016.03.080.
- Tubei V., Toda H., Hassanipour M. et al. 3D short fatigue crack closure behavior in Ti‒6Al‒4V alloy investigated using in-situ high resolution synchrotron X-ray tomography. Engineering Fracture Mechanics, 2021, vol. 249, art. 107755. DOI: 10.1016/j.engfracmech.2021.107755.
- Junet A., Messager A., Weck A. et al. Internal fatigue crack propagation in a Ti‒6Al‒4V alloy: an in situ study. International Journal of Fatigue, 2023, vol. 168, art. 107450. DOI: 10.1016/j.ijfatigue.2023.107450.
- Wang K., Wang F., Cui W. et al. Prediction of short fatigue crack growth of Ti‒6Al‒4V. Fatigue & Fracture of Engineering Materials & Structures, 2014, vol. 37, pp. 1075–1086. DOI: 10.1111/ffe.12177.
- Wei K., Ma Q., Wang G. et al. Exploration of the material transfer effect in local loading forming of ultra-large-size integrated component with multi-rib. International Journal of Advanced Manufacturing Technology, 2020, vol. 108, pp. 1413–1427. DOI: 10.1007/s00170-020-05517-1.
- Kuntz L., Pokorný P., Koněčná R. et al. Propagation of long fatigue cracks in Ti6Al4V alloy produced by direct metal laser sintering. Procedia Structural Integrity, 2019, vol. 17, pp. 222–229. DOI: 10.1016/j.prostr.2019.08.030.
- Ivanov B., Manokhin S.S., Kolobov Y.R. et al. Phase composition and microstructure of Ti‒6Al‒4V alloy after hydrogen-plastic working. Materials Physics and Mechanics, 2010, vol. 10, pp. 62–71.
- Gardner H., Radecka A., Rugg D. et al. Study of interaction of oxygen with the α2 phase in model alloy Ti-7 wt.% Al. Scripta Materialia, 2020, vol. 185, pp. 111–116. DOI: 10.1016/j.scriptamat.2020.03.048.
- Venkataraman A., Shade P., Adebisi R. et al. Structure and deformation pathways in Ti-7Al using atomistic simulations, experiments, and characterization. Metallurgical and Materials Transactions A, 2017, vol. 48A, pp. 2222–2235. DOI: 10.1007/s11661-017-4024-y.
- Chatterjee K., Venkataraman A., Garbaciak T. et al. Study of grain-level deformation and residual stresses in Ti-7Al under combined bending and tension using high energy diffraction microscopy (HEDM). International Journal of Solids and Structures, 2016, vol. 94–95, pp. 35–49. DOI: 10.1016/j.ijsolstr.2016.05.010.
- Worsnop F., Lim R., Bernier J. et al. The influence of alloying on slip intermittency and implications for dwell fatigue in titanium. Nature Communications, 2022, vol. 13, аrt. 5949. DOI: 10.1038/s41467-022-33437-z.
- Radecka A., Coakley J., Jones I. et al. Ordering and micromechanics of Ti-7Al. Materials Science and Engineering A, 2015, vol. 646, pp. 1–26. DOI: 10.1016/j.msea.2015.09.070.
- Xu Y., Worsnop F., Dye D., Dunne F. Slip intermittency and dwell fatigue in titanium alloys: discrete dislocation plasticity analysis: Preprint. 2023. Available at: https://www.researchgate.net/publication/372286366_Slip_intermittency_and_dwell_fatigue_in_titanium_alloys_a_discrete_dislocation_plasticity_analysis (accessed: May 18, 2025). DOI: 10.48550/arXiv.2307.05316.
- Yakovlev A.L., Arislanov A.A., Putyrsky S.V., Nochovnaya N.A. Study of mechanical properties and structure of large-sized semi-finished products made of VT6ch titanium alloy. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 12–18. DOI: 10.18577/2071-9140-2020-0-4-12-18.
- Krokhinа V.A., Arislanov A.A., Putyrskiy S.V. Investigation of the mechanical properties and structure of forgings made of VT6ch alloy after heat treatment with heating in the β-area. Trudy VIAM, 2024, no. 7 (137), pp. 24–33. Available at: http://www.viam-works.ru (accessed: May 13, 2025). DOI: 10.18577/2307-6046-2024-0-7-24-33.
- Sviridov A.V., Gribkov М.S. Features of repair of welded structures of large thicknesses from titanium alloy VT6ch. Trudy VIAM, 2021, no. 11 (105), pp. 34–43. Available at: http://www.viam-works.ru (accessed: May 13, 2025). DOI: 10.18577/2307-6046-2021-0-11-34-43.
- Berenson V.F., Shevchenko Yu.N., Kompaniets A.S. Passportization and certification of aviation materials – a guarantee of their quality. Aviation materials. Selected works of VIAM 1932–2002. Moscow: VIAM, 2002, pp. 907–916.
- Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
- Kablov E.N. Materials and Technologies of VIAM for Aviadvigatel. Permskie aviatsionnye dvigateli, 2014, no. 31, pp. 43–47.
- Kablov E.N. New Generation Materials. Zashchita i bezopasnost, 2014, no. 4, pp. 28–29.
- Kablov E.N., Grinevich A.V., Slavin A.V., Kabanov I.V., Gromov V.I., Ampilogov A.Yu., Yakovlev N.O., Polyakov A.N., Yakusheva N.A. Calculated Strength Characteristics of VKS-9M and 300M Steels. Zavodskaya laboratoriya. Diagnostika materialov, 2022, vol. 88, no. 3, pp. 51–60.
- State Standard 27.002–2015. Reliability in Engineering. Terms and Definitions. Moscow: Standartinform, 2016, pp. 9–11