On the question of manufacturing fire-resistant and fire-proof hoods of helicopter power plant engine nacholds from polymer composite materials

Part 1
Barannikov A.A., Veshkin E.A, Savitsky R.S., Slavin A.V.
Barannikov A.A., Veshkin E.A, Savitsky R.S., Slavin A.V. On the question of manufacturing fire-resistant and fire-proof hoods of helicopter power plant engine nacholds from polymer composite materials. Part 1 // Proceedings of VIAM. 2025. No. 8. DOI: 10.18577/2307-6046-2025-0-8-123-133. URL: https://viam-works.ru/en/journal/2025/8/11
Keywords
helicopter technology, polymer composite materials, carbon fiber, vacuum infusion, fire resistance, import substitution
Abstract

The article presents the results of the work over the past 10 years on the development of materials for use in the design of the engine nacelle of the power plant of a helicopter made of PCM. As part of import substitution, the issue of replacing the carbon reinforcing filler with a nominal surface density of 200 g/m2 of the Porcher brand (made in France) with a local analogue is considered. Domestic carbon fillers based on carbon fibers produced in China and the Russian Federation are studied. Studies of carbon fiber on the selected fabric are conducted based on the results of comparative tests. The material is shown to meet the specified requirements of the developer. The results confirm possible prospect of using the new carbon fiber in promising helicopters such as the Mi-171A3, Mi-38 or Ansat.

Reference list
  1. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  2. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  3. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7–8, pp. 54–58.
  4. Grashhenkov D.V., Chursova L.V. Strategy of development of composite and functional materials. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 231–242.
  5. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: June 14, 2025). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  6. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  7. Basharov E.A., Vagin A.Yu. Analysis of the use of composite materials in the design of helicopter airframes. Trudy MAI, 2017, no. 92, pp. 1–33.
  8. Technologies in helicopter engineering. Available at: https://aviatp.ru/files/aviaevents13-16/Helirussia-2013/1_Makareykin.pdf (accessed: June 14, 2025).
  9. Veshkin E.A., Postnov V.I., Postnova M.V., Barannikov A.A. Experience in the application of vacuum infusion technologies in the production of PCM structures. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2018, vol. 20, no. 4 (3), pp. 344–350.
  10. Merkulova Yu.I., Muhametov R.R., Dolgova E.V., Ahmadieva K.R. Polycyanurates binding for composites production by impregnation under pressure. Trudy VIAM, 2016, no. 11 (47), paper no. 05. Available at: http://www.viam-works.ru (accessed: June 14, 2025). DOI: 10.18577/2307-6046-2016-0-11-5-5.
  11. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Melt binding for perspective methods of production of PCM of new generation. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 260–265.
  12. Babin A.N. Binding for polymeric composite materials of new generation. Trudy VIAM, 2013, no. 4, paper no. 11. Available at: http://www.viam-works.ru (accessed: June 14, 2025).
  13. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), paper no. 03. Available at: https://www.journal.viam.ru (accessed: June 14, 2025). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  14. Antipov V.V., Samohvalov S.V., Nefedova Yu.N., Sidelnikov V.V., Somov A.V. Features of manufacturing complex contour parts from metal-polymer composite material. Trudy VIAM, 2023, no. 12 (130), paper no. 06. Available at: http://www.viam-works.ru (accessed: June 14, 2025). DOI: 10.18577/2307- 6046-2023-0-12-63-73.
  15. Antipov V.V., Somov A.V., Sidelnikov V.V., Nefedova Yu.N., Ogurtsov P.S., Soloviev V.A. Technological features of shaping fire-resistant light laminated material for helicopter engine hood manufacturing. Aviation materials and technologies, 2023, no. 3 (72), paper no. 07. Available at: http://www.journal.viam.ru (accessed: June 14, 2025). DOI: 10.18577/2713-0193-2023-0-3-90-100.
  16. Duyunova V.A., Kutyrev A.E., Serebrennikova N.Yu., Vdovin A.I., Somov A.V. Examination of the impact of aggressive environmental factors on the development of corrosion damage on samples of laminated glass-reinforced plastic of SIAL class. Aviation materials and technologies, 2021, no. 4 (65), paper no. 09. Available at: http://www.journal.viam.ru (accessed: June 14, 2025). DOI: 10.18577/2713-0193-2021-0-4-81-90.
  17. Development of design, technological processes, technological documentation and production of prototypes of the engine nacelle, cockpit canopy and structural elements of the Ka-226T helicopter airframe for the Indian Air Force. Available at: http://kai-composite.ru/index.php/raboty/11-works/26-ka226t (accessed: June 14, 2025).
  18. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  19. Practical Contact Angle Measurement (5). Custom-made models: from contact angle to surface free energy. Available at: https://warwick.ac.uk/fac/cross_fac/sciencecity/programmes/internal/themes/am2/booking/dropshapeanalyser/practical_contact_angle_measurement_5.pdf (accessed: June 14, 2025).