Structural factors determining applicability of the non-destructive X-ray diffraction method for assessing residual stress
Part 2
Medvedev P.N., Moiseeva N.S., Kochubey A.Ya., Juravleva P.L. Structural factors determining applicability of the non-destructive X-ray diffraction method for assessing residual stress. Part 2 // Proceedings of VIAM. 2025. No. 7. DOI: 10.18577/2307-6046-2025-0-7-130-140. URL: https://viam-works.ru/en/journal/2025/7/10
Keywords
surface residual stresses, metallography, phase composition, deformation
Abstract
The articlecompares the X-ray diffraction and metallographic methods for determining β- phase proportion in titanium alloys. The values of the β-phase proportion determined by the metallographic method are inflated against those determined by the X-ray method. These results show the necessity to improve these methods. The study of residual stresses has shown that when applying macrodeformation, the rate of the β-phase lattice deformation growth is higher than the same of the α-phase. The paper proposes to determine the Poisson’s ratio by the X-ray method using the accessoriez for modeling of bending or uniaxial tension tests.
Reference list
- Gorelik S.S. Recrystallization. Moscow: MISiS, 2005, 432 p.
- Gorelik S.S., Skakov Yu.A., Rastorguev L.N. X-ray and electron-optical analysis: textbook for universities. 4th ed., supple. and rev. Moscow: MISiS, 2002, 360 p.
- Umansky Ya.S., Skakov Yu.A., Ivanov A.N., Rastorguev L.N. Crystallography, X-ray and electron microscopy. Moscow: Metallurgiya, 1982, 632 p.
- EN 15305:2008. Non-destructive Testing. Test Method for Residual Stress analysis by X-ray Diffraction. BSI Standards Publication, 2009, 88 p.
- Medvedev P.N., Kashapov O.S., Reshetilo L.P. Study of surface layers of titanium alloy VT41 after mechanical treatment. Voprosy materialovedeniya, 2022, no. 3 (111), pp. 49–58.
- Medvedev P.N., Gulyaev A.I. Analysis of the spatial distribution of cracks in a heat-resistant nickel alloy manufactured using SLM technology. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 12–18. DOI: 10.18577/2071-9140-2020-0-1-12-18.
- Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
- Kablov E.N., Nochovnaya N.A., Shiryaev A.A., Davydova E.A. Investigation of structural and phase transformations in metastable β-titanium alloys and effect of cooling rate from homogenization temperature on structure and properties of VT47 alloy. Part 2. Trudy VIAM, 2020, no. 8 (90), paper no. 02. Available at: http://www.viam-works.ru (accessed: July 28, 2024). DOI: 10.18577/2307-6046-2020-0-8-11-19.
- Kalashnikov V.S., Reshetilo L.P., Chuchman O.V., Naprienko S.A. Strength and reliability of rods and rotor blade stamps made of heat-resistant industrial titanium alloys and modern pseudo-α-titanium alloy. Trudy VIAM, 2022, no. 2 (108), paper no. 02. Available at: http://www.viam-works.ru (accessed: July 28, 2024). DOI: 10.18577/2307-6046-2022-0-2-13-31.
- Oglodkov M.S., Kashapov O.S., Kalashnikov V.S., Kondratieva A.R. Comparative analysis of the characteristics of domestic alloys VT8, VT8M, VT8M-1, VT9 and Ti6242S alloy (USA) as applied to high-pressure compressor blades of aircraft gas turbine engines. Aviation materials and technologies, 2024, no. 3 (76), paper no. 04. Available at: http://www.journal.viam.ru (accessed: August 27, 2024). DOI: 10.18577/2713-0193-2024-0-3-35-50.
- Kashapov O.S., Pavlova T.V., Kalashnikov V.S., Zavodov A.V. Prerequisites for the development of new low-alloyed technological medium strength titanium alloy with operating temperature up to 400–450 °С, capable of strengthening. Aviation materials and technologies, 2024, no. 1 (74), paper no. 03. Available at: http://www.journal.viam.ru (accessed: August 28, 2024). DOI: 10.18577/2713-0193-2024-0-1-33-50.
- Kablov E.N., Putyrskiy S.V., Yakovlev A.L., Krokhina V.A., Naprienko S.A. Study of fatigue fracture resistance of stampings made of high-strength titanium alloy VT22M, manufactured with final deformation in the (α+β)- and β-regions. Titan, 2021, no. 1 (70), pp. 26–33.
- Peskova A.V., Sukhov D.I., Mazalov P.B. Examination of the formation of the titanium alloy VT6 structure obtained by additive manufacturing. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 38–44. DOI: 10.18577/2071-9140-2020-0-1-38-44.
- Kolpachev B.A., Elagin V.I., Livanov V.A. Metallurgy and heat treatment of non-ferrous metals and alloys: textbook for universities. 3rd ed., suppl. and rev. Moscow: MISiS, 2001, 416 p.
- Volkov N.V., Skrytny V.I., Filippov V.P., Yaltsev V.N. Physical materials science: textbook for universities in 8 vols. Moscow: NRNU MEPhI, 2012, vol. 3: Methods for studying the structural and phase state of materials, 800 p.